摘要 采用均匀沉淀法,用尿素为水解剂,60~90℃,0.005mol·L^(-1)≤C(La^(3+))≤0.025mol·L^(-1),0.27mol·L^(-1)≤C(urca)≤0.81mol·L^(-1),用La(NO_3)_3溶液备了La(Ⅲ)的超微粒化合物,所得沉淀为LaOHCO_3,具有与CaCO_3超微粒相似的结晶形态,粒径≤0.02μm.将此超微粒前驱体置于高温沪中,1200℃烧1h后,得到La_2O_3超微粒,粒径≤0.04μm. By means of the homogeneous precipitation and with urea as the hydrolytic agent (at 60-90 C . 0. OOSmol L-'< [La3+] initial <0. 025 mol L->, 0. 27 mol L-'< [urea] initial <0. 81 mol L-', the La ( H ) ultrafine particle compound from La(NO3)3 solution was prepared. The precipitates obtained are LaOHCO3, whose size is less than 0. 02 Mm in diam and whose crystal pattern is similar to that of CaCOs ultrafine particales. The La2O3 ultrafine particles with the size of less than 0. 04 |am in diam. Can be obtained by means of calcining the ultrafine particle precursors at 1200 C in the high-temperature stove for an hour.
出处 《西南师范大学学报(自然科学版)》 CAS CSCD 1993年第3期320-325,共6页 Journal of Southwest China Normal University(Natural Science Edition)
基金 国家自然科学基金资助项目
关键词 尿素 均匀沉淀法 超微粒 氧化镧 urea homogeneous precipitation ullrafines of lanthanum preparation
  • 相关文献

参考文献2

二级参考文献1

共引文献11

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部