期刊文献+

Mn^(3+)/Mn^(2+)间接电氧化法分解辉钼矿 被引量:8

Indirect Electro-oxidation of Molybdenite by Mn^(3+)/Mn^(2+)
在线阅读 下载PDF
导出
摘要 采用Mn3+/Mn2+间接电氧化法湿法分解辉钼矿。在强酸介质中,媒介Mn3+/Mn2+氧化能力很强,能将MoS2氧化分解为MoO3和硫酸,且锰离子可以循环利用。探讨了Mn3+/Mn2+间接电氧化法的工艺条件,结果表明:在H2SO4浓度为7mol/L,MnSO4浓度为0.5mol/L,电解电量为20A·h·g-1,电极间距15mm,阳极电流密度为800A·m-2,矿浆液固比为40,温度为55℃的条件下,钼的浸出率为88.5%。此外,对氧化浸出过程采用了超声波外场强化,Mo浸出率可以提高到92.3%。 Indirect electro-oxidation of molybdenite concentrates by Mn^(3+)/Mn^(2+) was studied. Because of the strong oxidation capability of Mn^(3+)/Mn^(2+) redox couple in acid condition, MoS_2 was decomposed to MoO_3 and H_2SO_4, while Mn ion could be recycled in the redox system. The results show that under suitable conditions H_2SO_4 concentration 7 mol/L, MnSO_4 concentration (0.5 mol/L,) electrolytic quantity of electricity 20 A·h·g^(-1), electrode spacing 15 mm, anode current density 800 A/m^2, rate of liquid to solid 40, and 55 ℃, the Mo leaching ratio can reach (88.5%.) Using ultrasonic increases the Mo leaching ratio to 92.3%.
出处 《中南大学学报(自然科学版)》 EI CAS CSCD 北大核心 2004年第5期797-801,共5页 Journal of Central South University:Science and Technology
关键词 间接电氧化 辉钼矿 Mn^3+/Mn^2+ 超声波 浸出 indirect electro-oxidation molybdenite Mn^(3+)/Mn^(2+) ultrasonic leaching
  • 相关文献

参考文献4

二级参考文献31

  • 1胡万里,周定,秦天雄,崔丽娟.间接电氧化制苯甲醛的研究[J].哈尔滨工业大学学报,1994,26(1):59-62. 被引量:13
  • 2张国衡,刘淑兰,齐欣.Mn(Ⅲ)/Mn(Ⅱ)体系电极过程的研究[J].天津大学学报,1989,22(4):65-72. 被引量:8
  • 3王文英,刘伟,丁克强,顾登平.间接电氧化法合成苯甲醛[J].现代化工,1996,16(6):33-35. 被引量:21
  • 4孙治荣,周定.硫酸锰的非均相电解氧化[J].化学世界,1996,37(10):517-519. 被引量:5
  • 5马保平.我国钼矿山生产现状调查分析[J].中国钼业,1998,22(5).
  • 6郑可利 赵崇涛 等.以苯为原料电化学氧化制备对苯酯的研究[J].化学世界,1992,6:256-259.
  • 7[智利]亚历山大·苏图洛夫 胡家璜(译).国际钼数据库[M].陕西:西安交通大学出版社,1989..
  • 8[智利]亚历山大·苏图洛夫 庄著学(译).钼与铼[M].陕西:西安交通大学出版社,1989..
  • 9[苏]M.A.雷斯 周进华(译).铁合金冶炼[M].北京:冶金工业出版社,1981..
  • 10吴海赢.国际钼市场回顾与展望[J].中国钼业,1998,22(2):52-54.

共引文献33

同被引文献81

引证文献8

二级引证文献45

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部