Hot Load Deformation of Light-weight Insulating Fireclay Bricks
1
作者 HAN Bo, LI Yushan 《China's Refractories》 CAS 2012年第4期13-16,共4页
The hot load deformation tests of four kinds of insulating fireclay bricks were carried out using a high temperature creep furnace from Sinosteel Luoyang hlstitute of Refractories Reseorch Co. , Ltd. The testing load ... The hot load deformation tests of four kinds of insulating fireclay bricks were carried out using a high temperature creep furnace from Sinosteel Luoyang hlstitute of Refractories Reseorch Co. , Ltd. The testing load was fixed at 0. 069 MPa and the total testing time was with- in 6 h including the holding time of 1.5 h. The hot load defi〉rmation process of insulating fireclay bricks can be divided into three steps : ( 1 ) expansion step from room temperature to RUL Tmax;( 2 ) quick shrinkage step be- tween. RUL T and Ttest; 3 ) relatively slow shrinkage step during holding process. The deformation rate at the beginning of holding process (D0h) should be controlled withi, +0. 1%. The hot load deformation testing tem- perature of insulating fireclay bricks was optimized as the value of RUL T plus 220℃. 展开更多
关键词 insulating fireclay bricks hot load deformation refiactoriness under load CREEP
在线阅读 下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部