Discussion on the Defects of Carburizing Process and Preventive Measures
1
作者 DUAN Lei 《外文科技期刊数据库(文摘版)工程技术》 2021年第3期564-568,共5页
Under the background of the rapid development of the national economy, the domestic demand for medium and heavy machinery and equipment is also increasing, especially the demand for the key parts of machinery and equi... Under the background of the rapid development of the national economy, the domestic demand for medium and heavy machinery and equipment is also increasing, especially the demand for the key parts of machinery and equipment. Mechanical parts are required to have higher life, fatigue strength, impact fatigue strength, hardness and other indicators in engineering operation. Carburizing process is widely considered as a practical chemical heat treatment technology. However, there are still many problems in the carburizing process. Taking 20CrMnTi steel gear as an example, this paper briefly introduces the existing problems in carburizing technology and the optimization of key technologies. 展开更多
关键词 CARBURIZING process defect preventive measure
原文传递
Influence of Process Parameters and Sr Addition on the Microstructure and Casting Defects of LPDC A356 Alloy for Engine Blocks 被引量:13
2
作者 Giulio Timelli Daniele Caliari Jovid Rakhmonov 《Journal of Materials Science & Technology》 SCIE EI CAS CSCD 2016年第6期515-523,共9页
The effects of Sr addition and pressure increase on the microstructure and casting defects of a low-pressure die cast (LPDC) AISi7Mg0.3 alloy have been studied. Metallographic and image analysis techniques have been... The effects of Sr addition and pressure increase on the microstructure and casting defects of a low-pressure die cast (LPDC) AISi7Mg0.3 alloy have been studied. Metallographic and image analysis techniques have been used to quantitatively examine the microstructural changes and the amount of porosity occurring at different Sr levels and pressure parameters. The results indicate that an increase in the filling pressure induces lower heat dissipation of the liquid close to the die/core surfaces, with the formation of slightly greater dendrite arms and coarser eutectic Si particles. On the other hand, the increase in the Sr level leads to finer microstructural scale and eutectic Si. The analysed variables, within the experimental conditions, do not affect the morphology of eutectic Si particles. Higher applied pressure and Sr content generate castings with lower amount of porosiW. However, as the filling pressure increases the flow of metal inside the die cavity is more turbulent, leading to the formation of oxide films and cold shots. In the analysed range of experimental conditions, the design of experiment methodology and the analysis of variance have been used to develop statistical models that accurately predict the average size of secondary dendrite arm spacing and the amount of porosity in the low-pressure die cast AISiTMg0.3 alloy. 展开更多
关键词 Aluminium alloys Engine block Microstructure Casting defects Sr addition process parameters
原文传递
Improving the process forming limit considering forming defects in the transitional region in local loading forming of Ti-alloy rib-web components 被引量:4
3
作者 Pengfei GAO Xiaodi LI +2 位作者 He YANG Xiaoguang FAN Zhenni LEI 《Chinese Journal of Aeronautics》 SCIE EI CAS CSCD 2017年第3期1270-1280,共11页
The isothermal local loading forming technology provides a feasible way to form Ti-alloy large-scale rib-web components in aerospace and aviation fields.However,the local loading process forming limit is restricted by... The isothermal local loading forming technology provides a feasible way to form Ti-alloy large-scale rib-web components in aerospace and aviation fields.However,the local loading process forming limit is restricted by forming defects in the transitional region.In this work,the feasibility of controlling forming defects and improving the process forming limit by adjusting die parameters is explored through finite element(FE) simulation.It is found that the common cavum and folding defects in the transitional region are significantly influenced by the fillet radii of left rib and middle rib,respectively.The cavum and folding defects can be effectively controlled by increasing the fillet radii of left rib and middle rib,respectively.The process forming limits considering forming defects in the transitional region are determined by the stepwise searching method under various die parameters.Moreover,the relationship between the process forming limit and die parameters is developed through the response surface methodology(RSM).The developed RSM models suggest that increasing the fillet radii of left and middle ribs is effective to improve the process forming limit during local loading forming of rib-web components.The results will provide technical basis for the design of die parameters and the reduction amount,which is of great importance to control forming defects and improve the process forming limit in local loading forming of Ti-alloy large-scale rib-web components. 展开更多
关键词 defect Large-scale rib-web component Local loading forming process forming limit Transitional region
原文传递
Repair welding process of friction stir welding groove defect 被引量:10
4
作者 刘会杰 张会杰 《中国有色金属学会会刊:英文版》 CSCD 2009年第3期563-567,共5页
The groove defect formed in the friction stir welding dramatically deteriorates weld appearances and mechanical properties of the joints owing to its larger size and penetration. Therefore, the friction stir repair we... The groove defect formed in the friction stir welding dramatically deteriorates weld appearances and mechanical properties of the joints owing to its larger size and penetration. Therefore, the friction stir repair welding was utilized to remove such a groove defect, and the focus was placed on the mechanical properties and microstructural characteristics of the repair joints so as to obtain an optimum repair welding process. The experimental results indicate that the groove defect can be removed by friction stir repair welding, and the offset repair welding process is superior to the symmetrical repair welding process. In the symmetrical repair welding process, a large number of fine cavity defects and an obvious aggregation of hard-brittle phase Al2Cu occur, accordingly the mechanical properties of the repair joint are weakened, and the fracture feature of repair joint is partially brittle and partially plastic. A good-quality repair joint can be obtained by the offset repair welding process, and the repair joint is fractured near the interface between the weld nugget zone and thermal-mechanically affected zone. 展开更多
关键词 搅拌摩擦焊接 缺陷形成 补焊工艺 焊接修复 力学性能 修复过程 显微组织 关节
在线阅读 下载PDF
Processing Defect Analysis and Nondestructive Evaluation Technology for Si_3N_4 Bearing Ball 被引量:1
5
作者 杨铁滨 王黎钦 +1 位作者 古乐 郑德志 《Defence Technology(防务技术)》 SCIE EI CAS 2008年第3期218-224,共7页
Researches on the processing method of ceramic bearing ball,the formation and propagation of defects in the manufacturing and the nondestructive evaluation(NDE) are summarized in this paper.The key for successful proc... Researches on the processing method of ceramic bearing ball,the formation and propagation of defects in the manufacturing and the nondestructive evaluation(NDE) are summarized in this paper.The key for successful processing of high strength ceramic balls is to avoid producing related defects.Many investigations show that the material microstructures,defects as well as mechanical processing parameters influence the final surface quality significantly.Most of NDE technologies,such as radiation,ultrasonic,dye-penetration and laser scatter,have been studied for ceramic bearing ball surface inspection around the world.So far,the difficulties to develop the perfect NDE system for ceramic bearing balls,which are caused by the defect variety and surface unfolding,have not been overcome yet. 展开更多
关键词 滚动轴承 氮化硅瓷 物质材料 技术性能
在线阅读 下载PDF
Defects of (Tb_(0.3)Dy_(0.7))Fe_(1.95) Alloys with "One-Step" Directional Solidification Process
6
作者 李扩社 李红卫 +3 位作者 方以坤 于敦波 杨红川 徐建林 《Journal of Rare Earths》 SCIE EI CAS CSCD 2004年第S1期126-129,共4页
The main types of defect in the (Tb_(0.3)Dy_(0.7))Fe_(1.95) alloys with the 'one-step' directional solidification process were investigated. The effect of the dendrite, grain boundaries, twin boundaries, and R... The main types of defect in the (Tb_(0.3)Dy_(0.7))Fe_(1.95) alloys with the 'one-step' directional solidification process were investigated. The effect of the dendrite, grain boundaries, twin boundaries, and REFe_3 precipitates on the magnetostrictive response of the (Tb_(0.3)Dy_(0.7))Fe_(1.95) alloys was analyzed respectively. The experiment results demonstrate that the dendrite, twin boundaries, and REFe_3 precipitates can be avoided by modifying alloying ingredient, solidification parameters and annealing technique. The dendritic growth front often leads to dendrite sheet, rare earth-rich phase, and twin boundaries. The lower proportion of rare earth, or slow solidification rate, results in the occurrence of REFe_3 precipitatates. It is vital for diminishing the defects to control the undercooling of solid-liquid interface at (2.4~5.1)×10~4 K·s·cm^(-2) so that the crystal grows in cellular growth front. 展开更多
关键词 directional solidification 'one-step' process crystal defects TbDyFe MAGNETOSTRICTION rare earths
在线阅读 下载PDF
Successive defects asymmetric simple exclusion processes with particles of arbitrary size
7
作者 蔡九菊 肖松 +1 位作者 王若翚 刘飞 《Chinese Physics B》 SCIE EI CAS CSCD 2009年第12期5097-5102,共6页
This paper uses various mean-field approaches and the Monte Carlo simulation to calculate asymmetric simple exclusion processes with particles of arbitrary size in the successive defects system. In this system, the ho... This paper uses various mean-field approaches and the Monte Carlo simulation to calculate asymmetric simple exclusion processes with particles of arbitrary size in the successive defects system. In this system, the hopping probability p (p 〈 1) and the size d of particles are not constant, Through theoretical calculation and computer simulation, it obtains the exact theoretical results and finds that the theoretical results are in agreement with the computer simulation. These results are helpful in analysing the effect of traffic with different hopping probabilities p and sizes d of particle. 展开更多
关键词 successive defects asymmetric simple exclusion processes arbitrary size Monte Carlo simulation mean-field theory
原文传递
中镍无限冷硬球墨铸铁离心复合轧辊生产实践
8
作者 杨智强 初嘉樑 郭红星 《中国铸造装备与技术》 2026年第1期50-55,共6页
结合生产实践,全面介绍了中镍无限冷硬球墨铸铁离心复合轧辊的工艺特点、技术优势及生产应用效果。通过分析材料成分设计、离心铸造工艺、热处理技术及质量控制要点,阐述了该类型轧辊的生产关键技术。实践表明,采用离心复合铸造技术生... 结合生产实践,全面介绍了中镍无限冷硬球墨铸铁离心复合轧辊的工艺特点、技术优势及生产应用效果。通过分析材料成分设计、离心铸造工艺、热处理技术及质量控制要点,阐述了该类型轧辊的生产关键技术。实践表明,采用离心复合铸造技术生产的中镍无限冷硬球墨铸铁轧辊具有优异的耐磨性、抗热裂性和高强度,有效解决了传统轧辊易断裂、磨损快的问题,使用寿命显著提高,生产成本大幅降低,在棒材、线材及板带轧制领域具有广阔应用前景。 展开更多
关键词 中镍无限冷硬球墨铸铁 离心复合轧辊 生产工艺 缺陷控制 应用效果
在线阅读 下载PDF
AlSiCuSc合金涡轮蜗壳熔模铸造工艺与数值模拟研究
9
作者 郑宗文 张荣强 +2 位作者 付金龙 孟晓东 李俊涛 《铸造》 2026年第4期426-432,共7页
涡轮蜗壳作为涡轮增压器的关键承压部件,其内部质量直接决定了增压器的可靠性与寿命。熔模铸造是生产该类复杂薄壁件的常用方法,但在生产过程中易因工艺设计不当而产生缩孔、缩松及裂纹等铸造缺陷。本研究以某型号AlSiCuSc合金涡轮蜗壳... 涡轮蜗壳作为涡轮增压器的关键承压部件,其内部质量直接决定了增压器的可靠性与寿命。熔模铸造是生产该类复杂薄壁件的常用方法,但在生产过程中易因工艺设计不当而产生缩孔、缩松及裂纹等铸造缺陷。本研究以某型号AlSiCuSc合金涡轮蜗壳为对象,利用ProCAST软件对设计的三种工艺方案进行数值模拟,对比和分析铸件铸造缺陷产生的位置及原因,确定了最优的工艺方案并进行了试验验证。结果表明,模拟与试验结果保持一致,验证了模拟的可行性和准确性。本研究为涡轮蜗壳的高质量、高合格率熔模铸造生产提供了可靠的理论依据和工艺优化途径。 展开更多
关键词 涡轮蜗壳 熔模铸造 AlSiCuSc合金 数值模拟 PROCAST 铸造缺陷 工艺优化
在线阅读 下载PDF
图像处理技术在印染纺织品瑕疵检测中的应用
10
作者 邹星 毛开梅 《印染助剂》 2026年第2期55-59,共5页
图像处理技术在提升印染纺织品瑕疵检测精度与效率方面展现出显著优势,已经成为行业智能化转型的核心驱动力。系统阐述图像处理技术体系的核心环节:图像采集硬件架构的革新突破、预处理流程的优化方法以及特征提取范式的演进路径;详细... 图像处理技术在提升印染纺织品瑕疵检测精度与效率方面展现出显著优势,已经成为行业智能化转型的核心驱动力。系统阐述图像处理技术体系的核心环节:图像采集硬件架构的革新突破、预处理流程的优化方法以及特征提取范式的演进路径;详细解析传统算法、机器学习模型到深度学习框架的算法迭代逻辑;重点阐述其在色彩偏差诊断、花型错位识别及物理结构缺陷检测等印染特需场景的应用特性。揭示当前主要实施瓶颈集中于复杂花型干扰抑制与跨平台协议兼容性矛盾。 展开更多
关键词 图像处理 印染纺织品 瑕疵检测
在线阅读 下载PDF
基于多特征融合的集装箱船导轨缺陷检测算法
11
作者 李瑞 张贤宇 +2 位作者 尤尹 汪骥 张全有 《大连理工大学学报》 北大核心 2026年第1期86-93,共8页
针对传统集装箱船导轨缺陷检测方法完全依赖人工目视检查,存在效率低、工作量大等问题,提出一种基于多特征融合的集装箱船导轨缺陷检测算法.设计了数据自适应重采样处理方法,降低缺陷种类分布不均的影响.在骨干网络设置多梯度感受野聚... 针对传统集装箱船导轨缺陷检测方法完全依赖人工目视检查,存在效率低、工作量大等问题,提出一种基于多特征融合的集装箱船导轨缺陷检测算法.设计了数据自适应重采样处理方法,降低缺陷种类分布不均的影响.在骨干网络设置多梯度感受野聚合模块,聚合导轨不同程度破损特征和周围环境特征.根据上述方法,在残差分析模块后嵌入混合注意力机制,有效引导多尺度特征流关注重点特征信息.在网络的特征拼接处融合特征重组上采样算子,扩张流入特征的局部感受野,有效整合全局细微特征信息.在测试集上的验证以及与人工效率的比对表明:所提改进算法对导轨缺陷检测的均值平均精度可达到97.0%,相较原YOLOv5算法提升2.9个百分点,有效提升了集装箱船导轨缺陷检测精度. 展开更多
关键词 船舶建造工艺 集装箱船导轨缺陷 混合注意力机制 特征重组上采样算子
在线阅读 下载PDF
工艺调控对Ti-6.5Al-2Zr-1Mo-1V激光熔化沉积层的影响机制研究 被引量:1
12
作者 温钟淳 关峰 +4 位作者 李明 蒋文通 郑建超 谢洪志 赵栋 《热加工工艺》 北大核心 2026年第3期63-70,共8页
研究了工艺调控对激光熔化沉积Ti-6.5Al-2Zr-1Mo-1V(TA15)钛合金沉积层质量的影响机制,通过OM显微镜、有限元模拟对成形试样的几何样貌、搭接率、稀释率进行分析。结果表明:当送粉速率从500、600、700到800 g/h逐渐提高,试样层厚逐渐变... 研究了工艺调控对激光熔化沉积Ti-6.5Al-2Zr-1Mo-1V(TA15)钛合金沉积层质量的影响机制,通过OM显微镜、有限元模拟对成形试样的几何样貌、搭接率、稀释率进行分析。结果表明:当送粉速率从500、600、700到800 g/h逐渐提高,试样层厚逐渐变大,沉积道各处逐渐出现未熔粉末;有限元结果表明,激光功率P、扫描速度v对熔池温度作用明显,其中在提高激光功率时熔池“拖尾”大幅变化,熔宽变化趋势与实际一致,数值略大于测量值;多道搭接实验中,当轨迹间距由3.2 mm降低至2.4 mm时,道间塌陷发生平直化并逐渐变成突起;测量稀释率时发现,送粉速率主要通过影响层厚来改变稀释率,而P、v则是通过改变熔化深度而影响稀释率。通过总结沉积层几何形貌、搭接率、稀释率随参数的变化趋势,发现使用5000 W功率搭配1200 mm/min的扫描速度、500 g/h的送粉速率、2.8 mm的轨迹间距时,可以获得打印质量最为稳定的沉积层。 展开更多
关键词 激光熔化沉积 工艺参数 冶金缺陷 稀释率 有限元模拟
原文传递
基于改进Faster-R-CNN的起重设备轨道缺陷检测方法
13
作者 陈洪良 张燕超 +1 位作者 潘爱华 明阳 《起重运输机械》 2026年第6期75-80,共6页
文中针对起重设备轨道缺陷检测经验依赖性强、智能化程度低的特点,研究一种基于改进FasterR-CNN模型的起重设备轨道缺陷检测方法。所述方法利用起重设备轨道缺陷检测车对起重轨道的上表面、左右侧面进行视频图像采集,并将采集的视频文... 文中针对起重设备轨道缺陷检测经验依赖性强、智能化程度低的特点,研究一种基于改进FasterR-CNN模型的起重设备轨道缺陷检测方法。所述方法利用起重设备轨道缺陷检测车对起重轨道的上表面、左右侧面进行视频图像采集,并将采集的视频文件用视频拆解、透视校正、帧差检测等方法进行图像预处理;然后将图像数据导入经过改进的Faster R-CNN模型中进行缺陷数量、缺陷种类检测并确定缺陷位置,最终将完成检测标注的图像拼接成完整的轨道图像进行输出,使检测人员能直观看到当前轨道缺陷信息,便于其对轨道情况有清晰的认知,并对轨道检修保养等行为提供数据支撑。 展开更多
关键词 起重设备 轨道缺陷检测 Faster R-CNN 图像处理
在线阅读 下载PDF
重庆橙汁长周期加工原料品种筛选与加工关键技术研发进展
14
作者 周贤文 黄林华 +7 位作者 孔文斌 杨蕾 洪棋斌 张利 张凯 吴彦 陆奎荣 徐钥华 《中国南方果树》 北大核心 2026年第1期247-250,共4页
针对我国柑橘产业存在的加工周期短、装备使用率低、不宜鲜销果浪费严重、橙汁品质与效益不足等核心问题,以延长加工周期、实现全量利用、提质降本增效为目标,梳理了重庆近年来在橙汁长周期加工原料品种筛选与加工关键技术应用方面的进... 针对我国柑橘产业存在的加工周期短、装备使用率低、不宜鲜销果浪费严重、橙汁品质与效益不足等核心问题,以延长加工周期、实现全量利用、提质降本增效为目标,梳理了重庆近年来在橙汁长周期加工原料品种筛选与加工关键技术应用方面的进展。这些研究与应用集成柑橘DUS测试技术与区域测试、等外果利用加工与橙汁品质提升、柑橘原料加工品质数据库、无菌贮藏及保鲜灌装等技术,形成了品种选育—优质栽培—加工装备—品质保鲜全链条技术体系。该技术体系建立的柠檬(9月)+锦橙(11月至翌年4月)+血橙/晚锦橙(2—5月)+夏橙(4—7月)+脐橙(全年缺陷果)组合实现9月至翌年7月连续11个月原料供应,配套营养诊断技术使重庆三峡瘠薄山地柑橘园产量达1289kg/667m2,增幅达150.8%;缺陷果加工装备替代进口,脱苦率达60%以上,出汁率提高5%;汁胞制备技术提升产出率15%,NFC橙汁货架期延长至120d以上。该技术体系已在重庆派森百、森美等20余家龙头企业规模化应用,推动柑橘全量利用率提升至95%以上,培育年销售额超5亿元的品牌3个,产品远销日本、中国香港、中国澳门等10余个国家和地区,年新增产值30亿元,有效破解了我国橙汁加工依赖进口的困局,为产业高质量发展提供了核心技术支撑。 展开更多
关键词 柑橘 橙汁加工 品种选育 缺陷果利用 提质增效 DUS测试
原文传递
工艺参数对激光粉末床熔融K418B高温合金显微缺陷和组织的影响
15
作者 陈思远 杜大帆 +2 位作者 何林 熊良华 董安平 《航空材料学报》 北大核心 2026年第1期70-78,共9页
采用激光粉末床熔融(laser powder bed fusion,LPBF)技术制备K418B高温合金,利用光学显微镜、扫描电镜和硬度仪分析工艺参数激光功率(140~220 W)和扫描速度(600~1400 mm/s)对显微缺陷、致密度、微观组织及硬度的影响。结果表明,激光功... 采用激光粉末床熔融(laser powder bed fusion,LPBF)技术制备K418B高温合金,利用光学显微镜、扫描电镜和硬度仪分析工艺参数激光功率(140~220 W)和扫描速度(600~1400 mm/s)对显微缺陷、致密度、微观组织及硬度的影响。结果表明,激光功率和扫描速度均显著影响样品的相对密度与缺陷分布。低能量密度易产生不规则孔洞,高能量密度则易形成球形气孔与凝固裂纹;体积能量密度(volume energy density,VED)过低或过高都会降低致密度和性能。最佳工艺参数为激光功率180 W、扫描速度1400 mm/s,在该条件下样品致密度可达99.95%以上,表面缺陷少,仅有少量凝固裂纹,显微组织呈明显熔池边界和胞状结构,维氏硬度达366.8HV_(0.2)。微观组织观察显示,熔池边界处晶粒较粗大,内部可见细胞状柱状晶,局部连续跨越多个熔池,表现出快速凝固特征。硬度随VED先升后降,与孔隙含量及致密度变化一致。研究揭示热应力是裂纹产生的主要原因,为K418B合金LPBF成形的参数优化提供依据,对提升航空发动机关键部件制造质量具有工程应用价值。 展开更多
关键词 激光粉末床熔融 K418B 工艺参数 显微缺陷
在线阅读 下载PDF
基于AnyCasting的汽车蜗壳压铸件的铸造工艺优化
16
作者 陈昌明 王帅 +6 位作者 杜彬 张永伟 方略 陈曦 丁常青 周海滨 周志明 《特种铸造及有色合金》 北大核心 2026年第3期414-418,共5页
基于实际生产需求,采用AnyCasting软件对蜗壳压铸过程进行模拟仿真分析,通过建立三维有限元模型,对充型顺序、凝固顺序及缺陷概率等进行定量分析,评估其对铸件质量的影响。基于缺陷判据分析,对铸件关键区域的缺陷分布进行预测与验证,准... 基于实际生产需求,采用AnyCasting软件对蜗壳压铸过程进行模拟仿真分析,通过建立三维有限元模型,对充型顺序、凝固顺序及缺陷概率等进行定量分析,评估其对铸件质量的影响。基于缺陷判据分析,对铸件关键区域的缺陷分布进行预测与验证,准确定位了缩松、缩孔和卷气等铸造缺陷的高发区域。通过优化浇注系统设计,包括进浇方式布局改进及溢流槽设置等工艺措施,显著改善了铸件的凝固补缩条件,提升了铸件内部质量和服役可靠性。 展开更多
关键词 汽车蜗壳 压铸 缺陷分析 工艺优化
原文传递
基于高光谱成像的航空叶片缺陷检测
17
作者 魏永超 蔡双 +2 位作者 岳雨琛 刘芳 王应海 《激光杂志》 北大核心 2026年第1期69-76,共8页
针对航发叶片划痕、凹坑等缺陷难以准确检测与定量分析的问题,提出一种基于近红外高光谱成像技术的缺陷检测方法。通过空谱特征融合聚类算法,解决微小缺陷在单一光谱或空间维度难以检测的问题。结合ISODATA聚类与轮廓边界提取算法增强... 针对航发叶片划痕、凹坑等缺陷难以准确检测与定量分析的问题,提出一种基于近红外高光谱成像技术的缺陷检测方法。通过空谱特征融合聚类算法,解决微小缺陷在单一光谱或空间维度难以检测的问题。结合ISODATA聚类与轮廓边界提取算法增强缺陷特征并确定有效连通边界,进而提出一种基于形态学处理与标记控制的改进分水岭自适应分割算法,实现微小缺陷的精确分割与定量分析。实验结果表明,相较于现有方法,该算法在缺陷分割的完整性和连续性方面具有显著优势,缺陷的长、宽平均绝对误差均得到降低,平均百分比误差MPE分别达到4.14%和3.15%,验证了该方法的精确性与有效性。为多类型缺陷(划痕/凹坑)的同步定量分析提供解决方案,满足航空发动机高精度检测需求。 展开更多
关键词 缺陷检测 航空发动机叶片 近红外高光谱 图像处理 缺陷分割
原文传递
气密封装器件封盖空洞缺陷量化方法优化
18
作者 冉红雷 崔亚茹 +3 位作者 张鑫 褚昆 张欢 杨振宝 《半导体技术》 北大核心 2026年第3期298-304,共7页
针对玻封陶瓷类气密封装器件X射线检测中,封盖边角区域空洞缺陷计算失准、判定标准过严等问题,提出一套基于数字图像处理的综合改进方法。通过直方图均衡化、双边滤波与指数变换等自适应图像增强技术,对X射线检测图像进行预处理;在此基... 针对玻封陶瓷类气密封装器件X射线检测中,封盖边角区域空洞缺陷计算失准、判定标准过严等问题,提出一套基于数字图像处理的综合改进方法。通过直方图均衡化、双边滤波与指数变换等自适应图像增强技术,对X射线检测图像进行预处理;在此基础上,构建了边角区域缺陷的精确计算模型,并基于“最短泄漏路径”原则优化了缺陷量化方法,准确计算出GJB 548C—2021等标准中涉及的密封区域泄漏路径。验证结果表明,该方法使边角区域缺陷识别准确度提高了约50%,识别效率较传统人工方法提高了10倍以上。本研究为高可靠性气密封装器件的质量保障提供了可靠的量化依据,具有良好的工程应用价值。 展开更多
关键词 气密封装器件 封盖空洞缺陷 数字图像处理 缺陷量化 X射线检测 最短泄漏路径
原文传递
面向航空航天金属增材制造构件的焊接技术研究进展
19
作者 吴世凯 潘朋 +6 位作者 黄文琪 徐明 张建超 祁俊峰 邱晓杰 吴东方 邢飞 《航空制造技术》 北大核心 2026年第7期50-64,共15页
增材制造技术因其高设计自由度、优异的尺寸精度和简化的制造流程,在航空航天复杂金属构件制造中具有广阔的应用前景。然而,空间尺寸受限、制造成本高昂及长时间成形的工艺不确定性等因素限制了大型构件的直接增材成形,采用模块化设计... 增材制造技术因其高设计自由度、优异的尺寸精度和简化的制造流程,在航空航天复杂金属构件制造中具有广阔的应用前景。然而,空间尺寸受限、制造成本高昂及长时间成形的工艺不确定性等因素限制了大型构件的直接增材成形,采用模块化设计与分批制造结合焊接技术能够有效缓解这些问题,成为该领域当前的研究热点。本文系统阐述了金属结构增材制造特有的微观组织特征及其焊接难点,并从合金成分优化、焊接方法创新及辅助技术应用等方面总结了这些难点问题的解决策略;详细介绍了增材制造结构常用焊接方法的原理与工艺特点;重点梳理了增材制造铝合金、钛合金、铁基及镍基合金的焊接性及面向航空航天增材制造构件焊接的工程应用进展;最后,展望了人工智能在焊接制造领域中的潜在应用。 展开更多
关键词 增材制造金属材料 焊接工艺 焊接缺陷 微观组织 接头性能
在线阅读 下载PDF
基于深度学习的低温沉积食品3D打印缺陷识别
20
作者 童强 马黄平 +4 位作者 杨俊豪 毕野 肖帅磊 董秀萍 孟庆国 《食品工业科技》 北大核心 2026年第5期339-347,共9页
低温沉积(LDM)食品3D打印过程中易受到挤出温度、速度、物料流变性能等多因素耦合影响,导致堵料、过量挤出、干涉等多种缺陷,影响打印质量。为实现对缺陷的高效识别,本文搭建了基于工业相机的视觉监测平台,并构建了多类别喷嘴挤出缺陷... 低温沉积(LDM)食品3D打印过程中易受到挤出温度、速度、物料流变性能等多因素耦合影响,导致堵料、过量挤出、干涉等多种缺陷,影响打印质量。为实现对缺陷的高效识别,本文搭建了基于工业相机的视觉监测平台,并构建了多类别喷嘴挤出缺陷图像数据集。针对缺陷尺寸小、类间差异不显著等问题,提出了一种融合ResNet与Swin Transformer的双通道多尺度特征提取网络,并引入多尺度注意力融合模块以提升识别精度。实验结果表明,所提模型能有效识别各类挤出缺陷,对堵料、过量、颗粒状和干涉类别的预测精度分别为98.20%、97.89%、94.90%和97.86%,正常挤出为97.63%;单张图像平均检测时间为0.2 s。整体准确率为97.53%,宏召回率为97.62%,较ResNet34分别提升4.11和4.00个百分点,展现出优异的识别性能与实时性,可为食品3D打印质量控制提供可靠数据支撑。 展开更多
关键词 食品3D打印 深度学习 过程检测 低温沉积 缺陷识别
在线阅读 下载PDF