期刊文献+
共找到1篇文章
< 1 >
每页显示 20 50 100
Fluidized magnetization roasting of refractory siderite-containing iron ore via preoxidation-low-temperature reduction 被引量:1
1
作者 Haoyan Sun Zheng Zou +1 位作者 Meiju Zhang Dong Yan 《International Journal of Minerals,Metallurgy and Materials》 SCIE EI CAS CSCD 2023年第6期1057-1066,共10页
Magnetization roasting is one of the most effective way of utilizing low-grade refractory iron ore.However,the reduction roasting of siderite(FeCO3)generates weakly magnetic wüstite,thus reducing iron recovery vi... Magnetization roasting is one of the most effective way of utilizing low-grade refractory iron ore.However,the reduction roasting of siderite(FeCO3)generates weakly magnetic wüstite,thus reducing iron recovery via weak magnetic separation.We systematically studied and proposed the fluidized preoxidation-low-temperature reduction magnetization roasting process for siderite.We found that the maghemite generated during the air oxidation roasting of siderite would be further reduced into wüstite at 500 and 550℃due to the unstable intermediate product magnetite(Fe_(3)O_(4)).Stable magnetite can be obtained through maghemite reduction only at low temperature.The optimal fluidized magnetization roasting parameters included preoxidation at 610℃for 2.5 min,followed by reduction at 450℃for 5 min.For roasted ore,weak magnetic separation yielded an iron ore concentrate grade of 62.0wt%and an iron recovery rate of 88.36%.Compared with that of conventional direct reduction magnetization roasting,the iron recovery rate of weak magnetic separation had greatly improved by 34.33%.The proposed fluidized preoxidation-low-temperature reduction magnetization roasting process can realize the efficient magnetization roasting utilization of low-grade refractory siderite-containing iron ore without wüstite generation and is unlimited by the proportion of siderite and hematite in iron ore. 展开更多
关键词 magnetization roasting fluidization SIDERITE preoxdization low-temperature reduction
在线阅读 下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部