Research efforts on electromagnetic interference(EMI)shielding materials have begun to converge on green and sustainable biomass materials.These materials offer numerous advantages such as being lightweight,porous,and...Research efforts on electromagnetic interference(EMI)shielding materials have begun to converge on green and sustainable biomass materials.These materials offer numerous advantages such as being lightweight,porous,and hierarchical.Due to their porous nature,interfacial compatibility,and electrical conductivity,biomass materials hold significant potential as EMI shielding materials.Despite concerted efforts on the EMI shielding of biomass materials have been reported,this research area is still relatively new compared to traditional EMI shielding materials.In particular,a more comprehensive study and summary of the factors influencing biomass EMI shielding materials including the pore structure adjustment,preparation process,and micro-control would be valuable.The preparation methods and characteristics of wood,bamboo,cellulose and lignin in EMI shielding field are critically discussed in this paper,and similar biomass EMI materials are summarized and analyzed.The composite methods and fillers of various biomass materials were reviewed.this paper also highlights the mechanism of EMI shielding as well as existing prospects and challenges for development trends in this field.展开更多
The lamellar layer of intermetallic compounds(IMCs)was adversely affected the performance of welding-brazing joints in Al/steel dissimilar metals.In this study,a short fiber-like surface morphology was fabricated on t...The lamellar layer of intermetallic compounds(IMCs)was adversely affected the performance of welding-brazing joints in Al/steel dissimilar metals.In this study,a short fiber-like surface morphology was fabricated on the butt surface of Q235 steel via laser.The interaction behavior between the short fibers and the molten pool was captured using a high-speed camera.Laser-arc hybrid welding-brazing was then employed to join Al(6061-T6)to the steel.This process successfully created a short fiber-like interface structure at the joint.The relationship between microstructure and mechanical properties was investigated,compared with Al/bare steel(ABS)joint.The research results indicated that the IMCs layer consisted of FeAl_(3)and Fe_(2)Al_(5).The interface strength of the Al/short fiber-like surface structural steel(ASFSSS)joint reached 153.2 MPa,an 82.2%increase compared to the ABS joint,which reached 84.1 MPa.When the ASFSSS joints without the reinforcement were bent to 58.2°and 25.2°in the longitudinal and transverse direction,respectively,they remained intact.However,cracks were discovered when the bending angle of the ABS reached 39.1°and 0°in the two directions.Numerical simulation revealed that the short fiber-like interface structure significantly reduced residual stress and improved the stress distribution in the weld,thereby enhancing the strength and toughness of Al/steel dissimilar joints.The crack propagation path in the ASFSSS joint was deflected into the weld when it encountered short fibers,and the fracture morphology presented the characteristic of ductile-brittle mixed fracture.展开更多
The infinite-layer nickelates,proposed as analogs to superconducting cuprates,provide a promising platform for exploring the mechanisms of unconventional superconductivity.However,the superconductivity has been exclus...The infinite-layer nickelates,proposed as analogs to superconducting cuprates,provide a promising platform for exploring the mechanisms of unconventional superconductivity.However,the superconductivity has been exclusively observed in thin films under atmospheric pressure,underscoring the critical role of the heterointerface.展开更多
Currently,carbon materials derived from biomass are widely sought after as electromagnetic absorbing(EMWA)materials owing to the unique structure,as well as the wide range of natural acquisition pathways,economic viab...Currently,carbon materials derived from biomass are widely sought after as electromagnetic absorbing(EMWA)materials owing to the unique structure,as well as the wide range of natural acquisition pathways,economic viability,and simple processing.However,due to the high dielectric properties,mismatched impedance and single attenuation mechanism,they cannot achieve efficient EMWA performance.Herein,the biomass carbon/Co/porous carbon magnetic composites with a layered gradient structure were fabricated by in-situ deposition of ZIF-67 on the lotus leaf base and then pyrolysis at high temperature.By adjusting the pyrolysis temperature,the sample obtained at 650℃ achieved a minimum reflection value(RLmin)of-34.2dB at a matching thickness of 2.6mm,and a maximum effective absorption bandwidth(EAB)of 7.12GHz.The results indicate that this magnetic composite with a multi-sized layered gradient porous structure has a good electron transport network,a large number of heterogeneous interfaces,and dipole polarization centers,which are conducive to multiple reflection and scattering of microwaves,conduction loss,interface loss,magnetic loss,and impedance matching of materials.Therefore,this work provided a reference for optimizing the EMWA performance of carbon materials and designing a layered gradient porous magnetic composite with multi-sized structure.展开更多
Optimizing electrolytes is non-trivial and yet promising strategies to simultaneously address dendrite growth and parasitic reactions for aqueous zinc-ion batteries.Herein,we present a low-cost zwitterionic additive,1...Optimizing electrolytes is non-trivial and yet promising strategies to simultaneously address dendrite growth and parasitic reactions for aqueous zinc-ion batteries.Herein,we present a low-cost zwitterionic additive,1-butylsulfonic-3-methylimidazolium(BSM),to enhance conventional ZnSO_(4)electrolytes.Combining experimental characterization and theoretical calculations,the results reveal that the zincophilic sulfonate groups in BSM partially substitute coordinated H_(2)O molecules in the Zn^(2+)hydration shell,thereby optimizing solvation dynamics.Meanwhile,the imidazole groups are preferentially adsorbed onto the zinc anode surface,forming an adaptive layer that guides uniform Zn^(2+)deposition along the(002)crystal orientation,suppresses parasitic reaction,and mitigates dendrite growth.Consequently,the Zn||Zn symmetric cells with BSM electrolyte achieve an exceptional plating/stripping lifespan of 4000 h at 1 mA cm^(-2)(1 mA h cm^(-2))and over 1600 h under elevated current density(5 mA cm^(-2),5 mA h cm^(-2)).Moreover,the Zn||Cu asymmetric cell demonstrates a long cycle life exceeding 1100 cycles while it maintains an average Coulombic efficiency(CE)of above 99.5%.Impressively,the assembled Zn||NH_(4)V_(4)O_(10)(NVO)full cell with BSM modified ZnSO_(4)electrolyte retains 77.6%capacity retention after 1000 cycles at 5 A g^(-1).Thus,this work establishes a dual-regulatory mechanism through zwitterionic additives to enable dendrite-free anodes and ultra-stable aqueous metal batteries.展开更多
The stability of the“surrounding rock-backfill”com posite system is crucial for the safety of mining stopes.This study systematically investigates the effects of steel slag(SS)content and interface angle on the stre...The stability of the“surrounding rock-backfill”com posite system is crucial for the safety of mining stopes.This study systematically investigates the effects of steel slag(SS)content and interface angle on the strength and failure characteristics of rock and SS-cemented paste backfill composite specimens(RBCS)through uniaxial compression strength tests(UCS),acoustic emission systems(AE),and 3 D digital image correlation monitoring technology(3 D-DIC).The intrinsic mechanism by which SS content influences the strength of SS-CPB was revealed through an analysis of its hydration reaction degree and microstructural characteristics under varying SS content.Moreover,a theoretical strength model incorporating different interface angles was developed to explore the impact of interface inclination on failure modes and mechanical strength.The main conclusions are as follows:The incorporation of SS enhances the plastic characteristics of RBCS and reduces its brittleness,with the increase of SS content,the stress-strain curve of RBCS in the“staircase-like”stag e becomes smoother;When the interface angle is 45°,the RBCS stress-strain curve exhibits a bimodal feature,and the failure mode changes from Y-shaped fractures to interface and axial splitting;The addition of SS results in a reduction of hydration products such as Ca(OH)_(2) in the backfill cementing system and an increase in harmful pores,which weakens the bonding performance and strength of RBCS,and the SS content should not exceed 45%;As the interface angle increases,the strength of RBCS decreases,and the critical interface slip angle decreases first and then increases with the increase in the E S/E R ratio.This study provides technical references for the large-scale application of SS in mine backfill.展开更多
Flexible pressure sensors have excellent prospects in applications of human-machine interfaces,artificial intelligence and human health monitoring due to their bendable and lightweight characteristics compared to rigi...Flexible pressure sensors have excellent prospects in applications of human-machine interfaces,artificial intelligence and human health monitoring due to their bendable and lightweight characteristics compared to rigid pressure sensors.However,arising from the limited compressibility of soft materials and the hardening of microstructures at the device interface,there is always a trade-off between high sensitivity and broad sensing range for most flexible pressure sensors,which results in a gradual saturation response and limits their practical applications.Herein,inspired by the distinct pressure perception function of crocodile receptors,a highly sensitive and wide-range flexible pressure sensor with multiscale microdomes and interlocked architecture is developed via a facile PS-decorated molding method.Combined with interlocked architecture,the multiscale dome-shaped structured interface enhances the compressibility of the material through structural complementarity,increases the contact area between functional materials,which compensates for the stiffness induced by the deformation of dense microscale columns.This effectively mitigates structural hardening across a wide pressure range,leading to the overall high performance of the sensor.As a result,the obtained sensor exhibits a low detection limit of 5 Pa,a high sensitivity of 6.14 kPa^(-1),a wide measurement range up to 231 kPa,short response/recovery time of 56 ms/69 ms,outstanding stability over 10,000 cycles.Considering these excellent properties,the sensor shows promising potential in health monitoring,human-computer interaction,wearable electronics.This study presents a strategy for the fabrication of flexible pressure sensors exhibiting high sensitivity and a wide pressure response range.展开更多
Buried interface passivation is crucial for high-efficiency,stable perovskite solar cells(PSCs).Herein,we design a three-layer passivation structure toward the buried interface of inverted PSCs,consisting of NiO_(x),p...Buried interface passivation is crucial for high-efficiency,stable perovskite solar cells(PSCs).Herein,we design a three-layer passivation structure toward the buried interface of inverted PSCs,consisting of NiO_(x),poly(V-p-TPD)and PFN-Br(V-p-TPD,N,N'-di-p-tolyl-N,-N'-bis(4-vinylphenyl)-[1,1'-biphenyl]-4,4'-diamine;PFN-Br,poly[(9,9-bis(3'-((N,N-dimethyl)-N-ethylammonium)-propyl)-2,7-fluorene)-alt-2,7-(9,9-dioctylfluorene)]dibromide).Typically,in situ poly(V-p-TPD)layer on the NiO_(x) surface was obtained by a simple thermal crosslinking process.This poly(V-p-TPD)/NiO_(x) bilayer structure is beneficial for hole extraction and high-quality perovskite films with larger grain sizes and less lattice distortion.On this basis,the PFN-Br is further introduced as a surface modification layer,which can not only optimize the energy level alignment with the perovskite but also passivate defects and suppress carrier recombination at the perovskite bottom interface.Finally,inverted PSCs based on(FA_(0.95)Cs_(0.05))PbI_(3) present 25.5%efficiency with a low V_(OC)deficit.Besides,the devices could maintain 91.15%of the initial efficiency after being stored at 85℃for 1080 h,indicating excellent thermal stability.This work highlights the potential of a three-layered passivation structure based on crosslinking polymer HTLs for highly efficient and stable PSCs.展开更多
The nitrate reduction via electrochemical catalysis offers an environmentally friendly method for sustainable ammonia production and wastewater remediation.However,conventional Co-based catalysts suffer from a major l...The nitrate reduction via electrochemical catalysis offers an environmentally friendly method for sustainable ammonia production and wastewater remediation.However,conventional Co-based catalysts suffer from a major limitation:their nitrate(NO_(3)^(-))adsorption capacity remains weak.This drawback severely restricts their catalytic efficiency.To overcome this limitation,we synthesized a triphasic interface material(Cu/Co/CoO@C)via rapid joule heating and elucidated its performance-enhancing mechanisms.The exceptional catalytic performance originates from the phase interface-induced multiscale structural regulation.At the microscopic scale,electronic structure modulation through interfacial charge redistribution between Cu and Co/CoO significantly reduces intermediate adsorption energies.Co 3d and O 2p orbitals coupling generates a localized polarized electric field,enhancing NO_(3)^(-)activation.At the macroscopic scale,defect-rich structures improve mass transfer and expose abundant active sites.With the Cu/Co/CoO@C,the yield of NH_(3) is achieved to 2.03 mmol h^(-1)cm^(-2)(-0.4 V vs.RHE,Faradaic efficiency(FE)98.4%).The assembled Zn-NO_(3)^(-)battery delivered a maximum power density of 52.09 mW cm^(-2)and a NH_(3) production rate of 297.5μmol h^(-1)cm^(-2)(FE 95.4%).Based on these results,this work offers new insights into multiphase interface design.展开更多
Efficient thermal management is critical to the reliability and performance of nanoscale electronic and photonic devices,particularly those incorporating multilayer structures.In this study,non-equilibrium molecular d...Efficient thermal management is critical to the reliability and performance of nanoscale electronic and photonic devices,particularly those incorporating multilayer structures.In this study,non-equilibrium molecular dynamics simulations were conducted to systematically investigate the effects of temperature,penetration depth,and Si layer thickness on the interfacial thermal resistance(ITR)in nanometer-scale Mo/Si multilayers,widely employed in extreme ultraviolet lithography.The results indicate that:(i)temperature variations exert a negligible influence on the ITR of amorphous Mo/Si interfaces,which remains stable across the range of 200-900 K;(ii)increasing penetration depth enhances the overlap of phonon density of states,thereby significantly reducing ITR;(iii)the ITR decreases with increasing Si thickness up to4.2 nm due to quasi-ballistic phonon transport,but rises again as phonon scattering becomes more pronounced at larger thicknesses.This study provides quantitative insights into heat transfer mechanisms at amorphous interfaces and also offers a feasible strategy for tailoring interfacial thermal transport through structural design.展开更多
High silicon content Al-Si composites with a composition of Al-40 wt% Si were fabricated via a highenergy ball milling method. The microstructure evolution of Al-40 wt% Si milled powders and sintered composites has be...High silicon content Al-Si composites with a composition of Al-40 wt% Si were fabricated via a highenergy ball milling method. The microstructure evolution of Al-40 wt% Si milled powders and sintered composites has been thoroughly studied by scanning electron microscopy, X-ray diffraction, energydispersive spectrometry and high-resolution transmission electron microscopy. The mechanism of ball milling Al-40 wt% Si powders has been disclosed in detail: fracture mechanism dominating in the early stages, followed by the agglomeration mechanism, finally reaching the balance between the fragments and the agglomerates. It has been found that the average particle sizes of mixed Al-Si powders can be refined to the nanoscale, and the crystallite sizes of Al and Si have been reduced to 10nm and 62nm upon milling for 2h–50h, respectively. The finally formed Al-Si interfaces after ball milling for 50h are wellcohesive. A dense and homogenous Al-40 wt% Si composite have been achieved by solid-state sintering at550?C. The results thus provide an effective support for producing bulk nanostructured Al-Si composites.展开更多
Heterogeneous-structured Cu samples composed of coarse-grained(CG) and ultrafine-grained(UFG) domains with a transitional interface were fabricated by friction stir processing, in order to investigate the effect of in...Heterogeneous-structured Cu samples composed of coarse-grained(CG) and ultrafine-grained(UFG) domains with a transitional interface were fabricated by friction stir processing, in order to investigate the effect of interface constraint on the yielding and fracture behaviors. Tensile test revealed that the synergetic strengthening induced by elastic/plastic interaction between incompatible domains increases with increasing the area of constraint interface. The strain distribution near interface and the fracture morphology were characterized using digital image correlation technique and scanning electron microscopy, respectively. Fracture dimples preferentially formed at the interface, possibly due to extremely high triaxial stress and strain accumulation near the interface. Surprisingly, the CG domain was fractured by pure shear instead of the expected voids growth caused by tensile stress.展开更多
The turbulence structures near a sheared air-water interface were experimentally investigated with the hydrogen bubble visualization technique. Surface shear was imposed by an airflow over the water flow which was kep...The turbulence structures near a sheared air-water interface were experimentally investigated with the hydrogen bubble visualization technique. Surface shear was imposed by an airflow over the water flow which was kept free from surface waves. Results show that the wind shear has the main influence on coherent structures under air-water interfaces. Low- and high- speed streaks form in the region close to the interface as a result of the imposed shear stress. When a certain airflow velocity is reached, “turbulent spots” appear randomly at low-speed streaks with some characteristics of hairpin vortices. At even higher shear rates, the flow near the interface is dominated primarily by intermittent bursting events. The coherent structures observed near sheared air-water interfaces show qualitative similarities with those occurring in near-wall turbulence. However, a few distinctive phenomena were also observed, including the fluctuating thickness of the instantaneous boundary layer and vertical vortices in bursting processes, which appear to be associated with the characteristics of air-water interfaces.展开更多
Vacuum diffusion bonding of a TiAl based alloy (TAD) to a titanium alloy (TC2) was carried out at 1 273 K for 15~120 min under a pressure of 25 MPa . The kinds of the reaction products and the interface s...Vacuum diffusion bonding of a TiAl based alloy (TAD) to a titanium alloy (TC2) was carried out at 1 273 K for 15~120 min under a pressure of 25 MPa . The kinds of the reaction products and the interface structures of the joints were investigated by SEM, EPMA and XRD. Based on this, a formation mechanism of the interface structure was elucidated. Experimental and analytical results show that two reaction layers have formed during the diffusion bonding of TAD to TC2. One is Al rich α(Ti)layer adjacent to TC2,and the other is (Ti 3Al+TiAl)layer adjacent to TAD,thus the interface structure of the TAD/TC2 joints is TAD/(Ti 3Al+TiAl)/α(Ti)/TC2.This interface structure forms according to a three stage mechanism,namely(a)the occurrence of a single phase α(Ti)layer;(b)the occurrence of a duplex phase(Ti 3Al+TiAl)layer;and(c)the growth of the α(Ti)and (Ti 3Al+TiAl)layers.展开更多
Cold-drawn pearlitic steel wire is irreplaceably used in industry owing to its outstanding mechanical property which is dominated by the cementite/ferrite(Fe_(3)C/Fe) interfaces in the material. However, the fine stru...Cold-drawn pearlitic steel wire is irreplaceably used in industry owing to its outstanding mechanical property which is dominated by the cementite/ferrite(Fe_(3)C/Fe) interfaces in the material. However, the fine structures of the Fe3C/Fe interfaces in the deformed wires are less known to date. In this work, transmission electron microscopic investigation was performed on the atomic structures of the interfaces with the Isaichev orientation relationship(OR) in the wires with progressive deformation strains. In addition to the effect of the dislocation/interface interactions, this work revealed that the deformation-induced partial decomposition of cementite plays an important role in the interface reconstruction during deformation. The interfacial carbon vacancies generated by cementite decomposition and particularly, the amorphization of cementite layers in the sample with ε > 1 could effectively annihilated the interfacial dislocations and consequently relaxed the interfacial stress. The correlations between the interface structure changes and the mechanical properties of the wires were discussed.展开更多
A novel single-step method is proposed for the analysis of dynamic response of visco-elastic structures containing non-smooth contactable interfaces. In the method, a two-level algorithm is employed for dealing with a...A novel single-step method is proposed for the analysis of dynamic response of visco-elastic structures containing non-smooth contactable interfaces. In the method, a two-level algorithm is employed for dealing with a nonlinear boundary condition caused by the dynamic contact of interfaces. At the first level, an explicit method is adopted to calculate nodal displacements of global viscoelastic system without considering the effect of dynamic contact of interfaces and at the second level, by introducing contact conditions of interfaces, a group of equations of lower order is derived to calculate dynamic contact normal and shear forces on the interfaces. The method is convenient and efficient for the analysis of problems of dynamic contact. The accuracy of the method is of the second order and the numerical stability condition is wider than that of other explicit methods.展开更多
In modern chemical engineering processes, solid interface involvement is the most important component of process intensification techniques, such as nanoporous membrane separation and heterogeneous catalysis. The fund...In modern chemical engineering processes, solid interface involvement is the most important component of process intensification techniques, such as nanoporous membrane separation and heterogeneous catalysis. The fundamental mechanism underlying interfacial transport remains incompletely understood given the complexity of heterogeneous interfacial molecular interactions and the high nonideality of the fluid involved. Thus, understanding the effects of interface-induced fluid microstructures on flow resistance is the first step in further understanding interfacial transport. Molecular simulation has become an indispensable method for the investigation of fluid microstructure and flow resistance. Here, we reviewed the recent research progress of our group and the latest relevant works to elucidate the contribution of interface-induced fluid microstructures to flow resistance.We specifically focused on water, ionic aqueous solutions, and alcohol–water mixtures given the ubiquity of these fluid systems in modern chemical engineering processes. We discussed the effects of the interfaceinduced hydrogen bond networks of water molecules, the ionic hydration of ionic aqueous solutions, and the spatial distributions of alcohol and alcohol–water mixtures on flow resistance on the basis of the distinctive characteristics of different fluid systems.展开更多
A radial basis function collocation method based on the nonlocal elastic continuum theory is developed to compute the band structures of nanoscale multilayered phononic crystals. The effects of nonlocal imperfect inte...A radial basis function collocation method based on the nonlocal elastic continuum theory is developed to compute the band structures of nanoscale multilayered phononic crystals. The effects of nonlocal imperfect interfaces on band structures of transverse waves propagating obliquely or vertically in the system are studied. The correctness of the present method is verified by comparing the numerical results with those obtained by applying the transfer matrix method in the case of nonlocal perfect interface. Furthermore, the influences of the nanoscale size, the impedance ratio and the incident angle on the cut-off frequency and band structures are investigated and discussed in detail. Numerical results show that the nonlocal interface imperfections have significant effects on the band structures in the macroscopic and microscopic scale.展开更多
Most reported electromagnetic wave absorption(EWA)materials show significant effective absorption in a certain frequency range,but their performances deteriorate dramatically as the frequency changes.As the range of w...Most reported electromagnetic wave absorption(EWA)materials show significant effective absorption in a certain frequency range,but their performances deteriorate dramatically as the frequency changes.As the range of working frequencies for electronic devices is gradually widening,it is of great interest to explore frequency-insensitive EWA materials that can achieve efficient absorption in every waveband by simply changing the absorption thickness.To this end,a multi-scale absorber(Fe/Fe_(3) C@NC)is rationally synthesized by chemical foaming and in-situ growth strategy.By controlling the growth of carbon nan-otubes,the Fe/Fe_(3) C@NC-2 exhibits a well-constructed 3D multi-scale architecture.Thanks to dipole po-larization,interface polarization and magnetic-dielectric energy conversion,the Fe/Fe_(3) C@NC-2 overcomes the frequency dispersion behavior and keeps a stable dielectric attenuation capability across the entire frequency range.Consequently,it delivers a superb full-band absorption of-50.1,-59.83,-55.87 and-51.91 dB in the S,C,X and Ku bands,respectively.The maximum radar cross-sectional reduction reaches 35.44 dB m^(-2) when the incidentθis 20°,testifying its impressive performance.Surprisingly,this EWA material also shows a remarkable resistance to oxidation and corrosion derived from the tightly coated carbon layers.This work provides new insight into the design of multi-band and stable EWA materials for practical application.展开更多
Due to the incompatibility of the interlaminar deformations,the interface debonding or cracking usually happens in a layered magnetoelectric(ME)structure under an applied load.In this paper,the transient responses of ...Due to the incompatibility of the interlaminar deformations,the interface debonding or cracking usually happens in a layered magnetoelectric(ME)structure under an applied load.In this paper,the transient responses of the anti-plane interface cracks in piezoelectric(PE)-piezomagnetic(PM)sandwich structures are studied by the standard methods of the integral transform and singular integral equation.Discussion on the numerical examples indicates that the PE-PM-PE structure under electric impact is more likely to fracture than the PM-PE-PM structure under a magnetic impact.The dynamic stress intensity factors(DSIFs)are more sensitive to the variation of the active layer thickness.The effects of the material constants on the DSIFs are dependent on the roles played by PE and PM media during the deformation process.展开更多
基金National Natural Science Foundation of China(32201491)Young Elite Scientists Sponsorship Program by CAST(2023QNRC001)The authors extend their appreciation to the Deanship of Scientific Research at Northern Border University,Arar,KSA for funding this research work through the project number“NBU-FPEJ-2024-1101-02”.
文摘Research efforts on electromagnetic interference(EMI)shielding materials have begun to converge on green and sustainable biomass materials.These materials offer numerous advantages such as being lightweight,porous,and hierarchical.Due to their porous nature,interfacial compatibility,and electrical conductivity,biomass materials hold significant potential as EMI shielding materials.Despite concerted efforts on the EMI shielding of biomass materials have been reported,this research area is still relatively new compared to traditional EMI shielding materials.In particular,a more comprehensive study and summary of the factors influencing biomass EMI shielding materials including the pore structure adjustment,preparation process,and micro-control would be valuable.The preparation methods and characteristics of wood,bamboo,cellulose and lignin in EMI shielding field are critically discussed in this paper,and similar biomass EMI materials are summarized and analyzed.The composite methods and fillers of various biomass materials were reviewed.this paper also highlights the mechanism of EMI shielding as well as existing prospects and challenges for development trends in this field.
基金supported by the National Natural Science Foundation of China(No.52275306)the Beijing Municipal Natural Science Foundation(No.3232021).
文摘The lamellar layer of intermetallic compounds(IMCs)was adversely affected the performance of welding-brazing joints in Al/steel dissimilar metals.In this study,a short fiber-like surface morphology was fabricated on the butt surface of Q235 steel via laser.The interaction behavior between the short fibers and the molten pool was captured using a high-speed camera.Laser-arc hybrid welding-brazing was then employed to join Al(6061-T6)to the steel.This process successfully created a short fiber-like interface structure at the joint.The relationship between microstructure and mechanical properties was investigated,compared with Al/bare steel(ABS)joint.The research results indicated that the IMCs layer consisted of FeAl_(3)and Fe_(2)Al_(5).The interface strength of the Al/short fiber-like surface structural steel(ASFSSS)joint reached 153.2 MPa,an 82.2%increase compared to the ABS joint,which reached 84.1 MPa.When the ASFSSS joints without the reinforcement were bent to 58.2°and 25.2°in the longitudinal and transverse direction,respectively,they remained intact.However,cracks were discovered when the bending angle of the ABS reached 39.1°and 0°in the two directions.Numerical simulation revealed that the short fiber-like interface structure significantly reduced residual stress and improved the stress distribution in the weld,thereby enhancing the strength and toughness of Al/steel dissimilar joints.The crack propagation path in the ASFSSS joint was deflected into the weld when it encountered short fibers,and the fracture morphology presented the characteristic of ductile-brittle mixed fracture.
基金supported by the National Natural Science Foundation of China[52125307(to P.G.),12404192(to R.C.S),12274061(to L.Q.)]Key Research and Development Program from the Ministry of Science and Technology(2023YFA1406301)the support from the New Cornerstone Science Foundation through the XPLORER PRIZE。
文摘The infinite-layer nickelates,proposed as analogs to superconducting cuprates,provide a promising platform for exploring the mechanisms of unconventional superconductivity.However,the superconductivity has been exclusively observed in thin films under atmospheric pressure,underscoring the critical role of the heterointerface.
基金supported by the National Natural Science Foundation of China(Nos.21667019,22066017,and 52173267)the Aviation Science Foundation of China(No.2017ZF56020).
文摘Currently,carbon materials derived from biomass are widely sought after as electromagnetic absorbing(EMWA)materials owing to the unique structure,as well as the wide range of natural acquisition pathways,economic viability,and simple processing.However,due to the high dielectric properties,mismatched impedance and single attenuation mechanism,they cannot achieve efficient EMWA performance.Herein,the biomass carbon/Co/porous carbon magnetic composites with a layered gradient structure were fabricated by in-situ deposition of ZIF-67 on the lotus leaf base and then pyrolysis at high temperature.By adjusting the pyrolysis temperature,the sample obtained at 650℃ achieved a minimum reflection value(RLmin)of-34.2dB at a matching thickness of 2.6mm,and a maximum effective absorption bandwidth(EAB)of 7.12GHz.The results indicate that this magnetic composite with a multi-sized layered gradient porous structure has a good electron transport network,a large number of heterogeneous interfaces,and dipole polarization centers,which are conducive to multiple reflection and scattering of microwaves,conduction loss,interface loss,magnetic loss,and impedance matching of materials.Therefore,this work provided a reference for optimizing the EMWA performance of carbon materials and designing a layered gradient porous magnetic composite with multi-sized structure.
基金financially supported by the National Natural Science Foundation of China(No.21703152,21801136,52025013,and 22121005)the National Key R&D Program of China(2021YFB4000200)the Natural Science Foundation of Tianjin(No.19JCQNJC02000)。
文摘Optimizing electrolytes is non-trivial and yet promising strategies to simultaneously address dendrite growth and parasitic reactions for aqueous zinc-ion batteries.Herein,we present a low-cost zwitterionic additive,1-butylsulfonic-3-methylimidazolium(BSM),to enhance conventional ZnSO_(4)electrolytes.Combining experimental characterization and theoretical calculations,the results reveal that the zincophilic sulfonate groups in BSM partially substitute coordinated H_(2)O molecules in the Zn^(2+)hydration shell,thereby optimizing solvation dynamics.Meanwhile,the imidazole groups are preferentially adsorbed onto the zinc anode surface,forming an adaptive layer that guides uniform Zn^(2+)deposition along the(002)crystal orientation,suppresses parasitic reaction,and mitigates dendrite growth.Consequently,the Zn||Zn symmetric cells with BSM electrolyte achieve an exceptional plating/stripping lifespan of 4000 h at 1 mA cm^(-2)(1 mA h cm^(-2))and over 1600 h under elevated current density(5 mA cm^(-2),5 mA h cm^(-2)).Moreover,the Zn||Cu asymmetric cell demonstrates a long cycle life exceeding 1100 cycles while it maintains an average Coulombic efficiency(CE)of above 99.5%.Impressively,the assembled Zn||NH_(4)V_(4)O_(10)(NVO)full cell with BSM modified ZnSO_(4)electrolyte retains 77.6%capacity retention after 1000 cycles at 5 A g^(-1).Thus,this work establishes a dual-regulatory mechanism through zwitterionic additives to enable dendrite-free anodes and ultra-stable aqueous metal batteries.
基金Project(52308316)supported by the National Natural Science Foundation of China,Project(BBJ2024088)supported by the Fundamental Research Funds for the Central Universities(PhD.Top Innovative Talents Fund of CUMTB),China。
文摘The stability of the“surrounding rock-backfill”com posite system is crucial for the safety of mining stopes.This study systematically investigates the effects of steel slag(SS)content and interface angle on the strength and failure characteristics of rock and SS-cemented paste backfill composite specimens(RBCS)through uniaxial compression strength tests(UCS),acoustic emission systems(AE),and 3 D digital image correlation monitoring technology(3 D-DIC).The intrinsic mechanism by which SS content influences the strength of SS-CPB was revealed through an analysis of its hydration reaction degree and microstructural characteristics under varying SS content.Moreover,a theoretical strength model incorporating different interface angles was developed to explore the impact of interface inclination on failure modes and mechanical strength.The main conclusions are as follows:The incorporation of SS enhances the plastic characteristics of RBCS and reduces its brittleness,with the increase of SS content,the stress-strain curve of RBCS in the“staircase-like”stag e becomes smoother;When the interface angle is 45°,the RBCS stress-strain curve exhibits a bimodal feature,and the failure mode changes from Y-shaped fractures to interface and axial splitting;The addition of SS results in a reduction of hydration products such as Ca(OH)_(2) in the backfill cementing system and an increase in harmful pores,which weakens the bonding performance and strength of RBCS,and the SS content should not exceed 45%;As the interface angle increases,the strength of RBCS decreases,and the critical interface slip angle decreases first and then increases with the increase in the E S/E R ratio.This study provides technical references for the large-scale application of SS in mine backfill.
基金supported by the National Natural Science Foundation of China(No.52175269)the Innovative Research Groups of the National Natural Science Foundation of China(No.52021003)+2 种基金Natural Science Foundation of Jilin Province of China(No.20210101052JC)Science and Technology Research Project of Education Department of Jilin Province(JJKH20231146KJ,JJKH20241262KJ)China Postdoctoral Science Foundation(2024M751086).
文摘Flexible pressure sensors have excellent prospects in applications of human-machine interfaces,artificial intelligence and human health monitoring due to their bendable and lightweight characteristics compared to rigid pressure sensors.However,arising from the limited compressibility of soft materials and the hardening of microstructures at the device interface,there is always a trade-off between high sensitivity and broad sensing range for most flexible pressure sensors,which results in a gradual saturation response and limits their practical applications.Herein,inspired by the distinct pressure perception function of crocodile receptors,a highly sensitive and wide-range flexible pressure sensor with multiscale microdomes and interlocked architecture is developed via a facile PS-decorated molding method.Combined with interlocked architecture,the multiscale dome-shaped structured interface enhances the compressibility of the material through structural complementarity,increases the contact area between functional materials,which compensates for the stiffness induced by the deformation of dense microscale columns.This effectively mitigates structural hardening across a wide pressure range,leading to the overall high performance of the sensor.As a result,the obtained sensor exhibits a low detection limit of 5 Pa,a high sensitivity of 6.14 kPa^(-1),a wide measurement range up to 231 kPa,short response/recovery time of 56 ms/69 ms,outstanding stability over 10,000 cycles.Considering these excellent properties,the sensor shows promising potential in health monitoring,human-computer interaction,wearable electronics.This study presents a strategy for the fabrication of flexible pressure sensors exhibiting high sensitivity and a wide pressure response range.
基金financial support from the Ministry of Science and Technology of China(2021YFB3800103)Natural Science Foundation of China(U24A6003,52361145847,52172260,52227803,52222212)Chinese Academy of Sciences-Commonwealth Scientific and Industrial Research Organization(CAS-CSIRO)Joint Project(112111KYSB20210017)。
文摘Buried interface passivation is crucial for high-efficiency,stable perovskite solar cells(PSCs).Herein,we design a three-layer passivation structure toward the buried interface of inverted PSCs,consisting of NiO_(x),poly(V-p-TPD)and PFN-Br(V-p-TPD,N,N'-di-p-tolyl-N,-N'-bis(4-vinylphenyl)-[1,1'-biphenyl]-4,4'-diamine;PFN-Br,poly[(9,9-bis(3'-((N,N-dimethyl)-N-ethylammonium)-propyl)-2,7-fluorene)-alt-2,7-(9,9-dioctylfluorene)]dibromide).Typically,in situ poly(V-p-TPD)layer on the NiO_(x) surface was obtained by a simple thermal crosslinking process.This poly(V-p-TPD)/NiO_(x) bilayer structure is beneficial for hole extraction and high-quality perovskite films with larger grain sizes and less lattice distortion.On this basis,the PFN-Br is further introduced as a surface modification layer,which can not only optimize the energy level alignment with the perovskite but also passivate defects and suppress carrier recombination at the perovskite bottom interface.Finally,inverted PSCs based on(FA_(0.95)Cs_(0.05))PbI_(3) present 25.5%efficiency with a low V_(OC)deficit.Besides,the devices could maintain 91.15%of the initial efficiency after being stored at 85℃for 1080 h,indicating excellent thermal stability.This work highlights the potential of a three-layered passivation structure based on crosslinking polymer HTLs for highly efficient and stable PSCs.
基金financial support provided by the National Natural Science Foundation of Yunnan Province(202301AS070040,202301AU070209)the Major Science and Technology Projects of Yunnan Province(202302AB080019-3)+3 种基金the Scientific Research Fund Project of Yunnan Provincial Department of Education(2023J0033)the Laboratory of Solid-State Ions for Green Energy of Yunnan Universitythe Analysis and Measurements Center of Yunnan University for the sample testing servicethe Electron Microscope Center of Yunnan University for the support of this work。
文摘The nitrate reduction via electrochemical catalysis offers an environmentally friendly method for sustainable ammonia production and wastewater remediation.However,conventional Co-based catalysts suffer from a major limitation:their nitrate(NO_(3)^(-))adsorption capacity remains weak.This drawback severely restricts their catalytic efficiency.To overcome this limitation,we synthesized a triphasic interface material(Cu/Co/CoO@C)via rapid joule heating and elucidated its performance-enhancing mechanisms.The exceptional catalytic performance originates from the phase interface-induced multiscale structural regulation.At the microscopic scale,electronic structure modulation through interfacial charge redistribution between Cu and Co/CoO significantly reduces intermediate adsorption energies.Co 3d and O 2p orbitals coupling generates a localized polarized electric field,enhancing NO_(3)^(-)activation.At the macroscopic scale,defect-rich structures improve mass transfer and expose abundant active sites.With the Cu/Co/CoO@C,the yield of NH_(3) is achieved to 2.03 mmol h^(-1)cm^(-2)(-0.4 V vs.RHE,Faradaic efficiency(FE)98.4%).The assembled Zn-NO_(3)^(-)battery delivered a maximum power density of 52.09 mW cm^(-2)and a NH_(3) production rate of 297.5μmol h^(-1)cm^(-2)(FE 95.4%).Based on these results,this work offers new insights into multiphase interface design.
基金supported by the National Natural Science Foundation of China(Grant No.52206092)the National Key R&D Program of China(Grant No.2024YFF0508900)+1 种基金the Big Data Computing Center of Southeast Universitythe Center for Fundamental and Interdisciplinary Sciences of Southeast University。
文摘Efficient thermal management is critical to the reliability and performance of nanoscale electronic and photonic devices,particularly those incorporating multilayer structures.In this study,non-equilibrium molecular dynamics simulations were conducted to systematically investigate the effects of temperature,penetration depth,and Si layer thickness on the interfacial thermal resistance(ITR)in nanometer-scale Mo/Si multilayers,widely employed in extreme ultraviolet lithography.The results indicate that:(i)temperature variations exert a negligible influence on the ITR of amorphous Mo/Si interfaces,which remains stable across the range of 200-900 K;(ii)increasing penetration depth enhances the overlap of phonon density of states,thereby significantly reducing ITR;(iii)the ITR decreases with increasing Si thickness up to4.2 nm due to quasi-ballistic phonon transport,but rises again as phonon scattering becomes more pronounced at larger thicknesses.This study provides quantitative insights into heat transfer mechanisms at amorphous interfaces and also offers a feasible strategy for tailoring interfacial thermal transport through structural design.
基金financially supported by the National Natural Science Foundation of China (No.51571148)the National Key Research and Development Program of China (No.2017YFE0302600 and No.2017YFB0701801)the Thousand Talents Program for Distinguished Young Scholars of China
文摘High silicon content Al-Si composites with a composition of Al-40 wt% Si were fabricated via a highenergy ball milling method. The microstructure evolution of Al-40 wt% Si milled powders and sintered composites has been thoroughly studied by scanning electron microscopy, X-ray diffraction, energydispersive spectrometry and high-resolution transmission electron microscopy. The mechanism of ball milling Al-40 wt% Si powders has been disclosed in detail: fracture mechanism dominating in the early stages, followed by the agglomeration mechanism, finally reaching the balance between the fragments and the agglomerates. It has been found that the average particle sizes of mixed Al-Si powders can be refined to the nanoscale, and the crystallite sizes of Al and Si have been reduced to 10nm and 62nm upon milling for 2h–50h, respectively. The finally formed Al-Si interfaces after ball milling for 50h are wellcohesive. A dense and homogenous Al-40 wt% Si composite have been achieved by solid-state sintering at550?C. The results thus provide an effective support for producing bulk nanostructured Al-Si composites.
基金Projects(11672195,51301092) supported by the National Natural Science Foundation of ChinaProject(2016JQ0047) supported by Sichuan Youth Science and Technology Foundation,China
文摘Heterogeneous-structured Cu samples composed of coarse-grained(CG) and ultrafine-grained(UFG) domains with a transitional interface were fabricated by friction stir processing, in order to investigate the effect of interface constraint on the yielding and fracture behaviors. Tensile test revealed that the synergetic strengthening induced by elastic/plastic interaction between incompatible domains increases with increasing the area of constraint interface. The strain distribution near interface and the fracture morphology were characterized using digital image correlation technique and scanning electron microscopy, respectively. Fracture dimples preferentially formed at the interface, possibly due to extremely high triaxial stress and strain accumulation near the interface. Surprisingly, the CG domain was fractured by pure shear instead of the expected voids growth caused by tensile stress.
基金The project supported by the National Natural Science Foundation of China (Grant No.19672070)
文摘The turbulence structures near a sheared air-water interface were experimentally investigated with the hydrogen bubble visualization technique. Surface shear was imposed by an airflow over the water flow which was kept free from surface waves. Results show that the wind shear has the main influence on coherent structures under air-water interfaces. Low- and high- speed streaks form in the region close to the interface as a result of the imposed shear stress. When a certain airflow velocity is reached, “turbulent spots” appear randomly at low-speed streaks with some characteristics of hairpin vortices. At even higher shear rates, the flow near the interface is dominated primarily by intermittent bursting events. The coherent structures observed near sheared air-water interfaces show qualitative similarities with those occurring in near-wall turbulence. However, a few distinctive phenomena were also observed, including the fluctuating thickness of the instantaneous boundary layer and vertical vortices in bursting processes, which appear to be associated with the characteristics of air-water interfaces.
文摘Vacuum diffusion bonding of a TiAl based alloy (TAD) to a titanium alloy (TC2) was carried out at 1 273 K for 15~120 min under a pressure of 25 MPa . The kinds of the reaction products and the interface structures of the joints were investigated by SEM, EPMA and XRD. Based on this, a formation mechanism of the interface structure was elucidated. Experimental and analytical results show that two reaction layers have formed during the diffusion bonding of TAD to TC2. One is Al rich α(Ti)layer adjacent to TC2,and the other is (Ti 3Al+TiAl)layer adjacent to TAD,thus the interface structure of the TAD/TC2 joints is TAD/(Ti 3Al+TiAl)/α(Ti)/TC2.This interface structure forms according to a three stage mechanism,namely(a)the occurrence of a single phase α(Ti)layer;(b)the occurrence of a duplex phase(Ti 3Al+TiAl)layer;and(c)the growth of the α(Ti)and (Ti 3Al+TiAl)layers.
基金financially supported by the National Natural Science Foundation of China (No. 51501195)the Fund of SYNL。
文摘Cold-drawn pearlitic steel wire is irreplaceably used in industry owing to its outstanding mechanical property which is dominated by the cementite/ferrite(Fe_(3)C/Fe) interfaces in the material. However, the fine structures of the Fe3C/Fe interfaces in the deformed wires are less known to date. In this work, transmission electron microscopic investigation was performed on the atomic structures of the interfaces with the Isaichev orientation relationship(OR) in the wires with progressive deformation strains. In addition to the effect of the dislocation/interface interactions, this work revealed that the deformation-induced partial decomposition of cementite plays an important role in the interface reconstruction during deformation. The interfacial carbon vacancies generated by cementite decomposition and particularly, the amorphization of cementite layers in the sample with ε > 1 could effectively annihilated the interfacial dislocations and consequently relaxed the interfacial stress. The correlations between the interface structure changes and the mechanical properties of the wires were discussed.
基金The project supported by the National Natural Science Foundation of China(59578032)the Key Project of the Ninth Five-Year Plan(96221030202)
文摘A novel single-step method is proposed for the analysis of dynamic response of visco-elastic structures containing non-smooth contactable interfaces. In the method, a two-level algorithm is employed for dealing with a nonlinear boundary condition caused by the dynamic contact of interfaces. At the first level, an explicit method is adopted to calculate nodal displacements of global viscoelastic system without considering the effect of dynamic contact of interfaces and at the second level, by introducing contact conditions of interfaces, a group of equations of lower order is derived to calculate dynamic contact normal and shear forces on the interfaces. The method is convenient and efficient for the analysis of problems of dynamic contact. The accuracy of the method is of the second order and the numerical stability condition is wider than that of other explicit methods.
基金Supported by the National Natural Science Foundation of China(21878144,21576130,21490584 and 21838004)Project of Jiangsu Natural Science Foundation of China(BK20171464)+2 种基金Qing Lan ProjectJiangsu Overseas Visiting Scholar Program for University Prominent Young&Middle-aged Teachers and Presidentsthe Project of Priority Academic Program Development of Jiangsu Higher Education Institutions(PAPD)
文摘In modern chemical engineering processes, solid interface involvement is the most important component of process intensification techniques, such as nanoporous membrane separation and heterogeneous catalysis. The fundamental mechanism underlying interfacial transport remains incompletely understood given the complexity of heterogeneous interfacial molecular interactions and the high nonideality of the fluid involved. Thus, understanding the effects of interface-induced fluid microstructures on flow resistance is the first step in further understanding interfacial transport. Molecular simulation has become an indispensable method for the investigation of fluid microstructure and flow resistance. Here, we reviewed the recent research progress of our group and the latest relevant works to elucidate the contribution of interface-induced fluid microstructures to flow resistance.We specifically focused on water, ionic aqueous solutions, and alcohol–water mixtures given the ubiquity of these fluid systems in modern chemical engineering processes. We discussed the effects of the interfaceinduced hydrogen bond networks of water molecules, the ionic hydration of ionic aqueous solutions, and the spatial distributions of alcohol and alcohol–water mixtures on flow resistance on the basis of the distinctive characteristics of different fluid systems.
基金supports by the National Natural Science Foundation of China (Grants 11002026, 11372039)the Beijing Natural Science Foundation (Grant 3133039)the Scientific Research Foundation for the Returned (Grant 20121832001)
文摘A radial basis function collocation method based on the nonlocal elastic continuum theory is developed to compute the band structures of nanoscale multilayered phononic crystals. The effects of nonlocal imperfect interfaces on band structures of transverse waves propagating obliquely or vertically in the system are studied. The correctness of the present method is verified by comparing the numerical results with those obtained by applying the transfer matrix method in the case of nonlocal perfect interface. Furthermore, the influences of the nanoscale size, the impedance ratio and the incident angle on the cut-off frequency and band structures are investigated and discussed in detail. Numerical results show that the nonlocal interface imperfections have significant effects on the band structures in the macroscopic and microscopic scale.
基金financially supported by the National Natu-ral Science Foundation of China(Grant Nos.22178384,22238012 and 52002363)the Science Foundation of China University of Petroleum,Beijing(Grant No.ZX20220079)the Aeronautical Science Foundation of China(Grant No.2020Z054025002).
文摘Most reported electromagnetic wave absorption(EWA)materials show significant effective absorption in a certain frequency range,but their performances deteriorate dramatically as the frequency changes.As the range of working frequencies for electronic devices is gradually widening,it is of great interest to explore frequency-insensitive EWA materials that can achieve efficient absorption in every waveband by simply changing the absorption thickness.To this end,a multi-scale absorber(Fe/Fe_(3) C@NC)is rationally synthesized by chemical foaming and in-situ growth strategy.By controlling the growth of carbon nan-otubes,the Fe/Fe_(3) C@NC-2 exhibits a well-constructed 3D multi-scale architecture.Thanks to dipole po-larization,interface polarization and magnetic-dielectric energy conversion,the Fe/Fe_(3) C@NC-2 overcomes the frequency dispersion behavior and keeps a stable dielectric attenuation capability across the entire frequency range.Consequently,it delivers a superb full-band absorption of-50.1,-59.83,-55.87 and-51.91 dB in the S,C,X and Ku bands,respectively.The maximum radar cross-sectional reduction reaches 35.44 dB m^(-2) when the incidentθis 20°,testifying its impressive performance.Surprisingly,this EWA material also shows a remarkable resistance to oxidation and corrosion derived from the tightly coated carbon layers.This work provides new insight into the design of multi-band and stable EWA materials for practical application.
基金Project supported by the National Natural Science Foundation of China(Nos.11272222,11502108,and 11611530686)the Natural Science Foundation for Distinguished Young Scholars of Jiangsu Province of China(No.BK20140037)
文摘Due to the incompatibility of the interlaminar deformations,the interface debonding or cracking usually happens in a layered magnetoelectric(ME)structure under an applied load.In this paper,the transient responses of the anti-plane interface cracks in piezoelectric(PE)-piezomagnetic(PM)sandwich structures are studied by the standard methods of the integral transform and singular integral equation.Discussion on the numerical examples indicates that the PE-PM-PE structure under electric impact is more likely to fracture than the PM-PE-PM structure under a magnetic impact.The dynamic stress intensity factors(DSIFs)are more sensitive to the variation of the active layer thickness.The effects of the material constants on the DSIFs are dependent on the roles played by PE and PM media during the deformation process.