Correction:Enhanced Hydrogen Embrittlement Resistance in a Vanadium-Alloyed 42CrNiMoV Steel for High-Strength Wind Turbine Bolts
1
作者 Jiang Liu Fengping Zhao +2 位作者 Wen Shi Han Dong Xiaofei Guo 《Acta Metallurgica Sinica(English Letters)》 2025年第12期2316-2317,共2页
In the sentence beginning'and more irreversible hydrogentrapping sites….'in this article,the value'0.38×1025 cm-3'should have read'0.68×1020 cm-3'.These corrections do not alter the ... In the sentence beginning'and more irreversible hydrogentrapping sites….'in this article,the value'0.38×1025 cm-3'should have read'0.68×1020 cm-3'.These corrections do not alter the primary conclusion that the irreversible hydrogen trap density in 42CrNiMoV steel is nearly twice that of 40CrNiMo steel. 展开更多
关键词 wind turbine bolts hydrogen trap density irreversible hydrogen trapping sites hydrogen embrittlement irreversible hydrogentrapping irreversible hydrogen trap vanadium alloyed crnimov steel