The mechanical behavior of cemented gangue backfill materials(CGBMs)is closely related to particle size distribution(PSD)of aggregates and properties of cementitious materials.Consequently,the true triaxial compressio...The mechanical behavior of cemented gangue backfill materials(CGBMs)is closely related to particle size distribution(PSD)of aggregates and properties of cementitious materials.Consequently,the true triaxial compression tests,CT scanning,SEM,and EDS tests were conducted on cemented gangue backfill samples(CGBSs)with various carbon nanotube concentrations(P_(CNT))that satisfied fractal theory for the PSD of aggregates.The mechanical properties,energy dissipations,and failure mechanisms of the CGBSs under true triaxial compression were systematically analyzed.The results indicate that appropriate carbon nanotubes(CNTs)effectively enhance the mechanical properties and energy dissipations of CGBSs through micropore filling and microcrack bridging,and the optimal effect appears at P_(CNT)of 0.08wt%.Taking PSD fractal dimension(D)of 2.500 as an example,compared to that of CGBS without CNT,the peak strength(σ_(p)),axial peak strain(ε_(1,p)),elastic strain energy(Ue),and dissipated energy(U_(d))increased by 12.76%,29.60%,19.05%,and90.39%,respectively.However,excessive CNTs can reduce the mechanical properties of CGBSs due to CNT agglomeration,manifesting a decrease inρ_(p),ε_(1,p),and the volumetric strain increment(Δε_(v))when P_(CNT)increases from 0.08wt%to 0.12wt%.Moreover,the addition of CNTs improved the integrity of CGBS after macroscopic failure,and crack extension in CGBSs appeared in two modes:detour and pass through the aggregates.Theσ_(p)and U_(d)firstly increase and then decrease with increasing D,and porosity shows the opposite trend.Theε_(1,p)andΔε_(v)are negatively correlated with D,and CGBS with D=2.150 has the maximum deformation parameters(ε_(1,p)=0.05079,Δε_(v)=0.01990)due to the frictional slip effect caused by coarse aggregates.With increasing D,the failure modes of CGBSs are sequentially manifested as oblique shear failure,"Y-shaped"shear failure,and conjugate shear failure.展开更多
Analyzing the fatigue damage characteristics of hot dry rock(HDR)affected by seawater thermal shock cycles is required for the efficient exploitation of HDR and the conservation of freshwater resources.Mechanical and ...Analyzing the fatigue damage characteristics of hot dry rock(HDR)affected by seawater thermal shock cycles is required for the efficient exploitation of HDR and the conservation of freshwater resources.Mechanical and acoustic emission(AE)monitoring tests were conducted during the triaxial compression of HDR at different confining pressures,temperatures,and numbers of seawater thermal shocks to investigate the seawater damage of HDR.The test results indicated an increase in the cumulative AE counts with increasing temperature and number of seawater thermal shocks,and a decrease in AE counts with increasing confining pressure.The effect of the number of seawater thermal shocks was significant.The AE counts were 276% higher at 15 than at 0 seawater thermal shocks.The b-value increased with the number of thermal shocks and stabilized after 5 shocks.Most of the damage was small fractures,which reduced the rock’s damage resistance.The AE time series under HDR triaxial compression exhibited multifractal features.High energy AE events dominated the damage mechanism of HDR,indicating shear damage to the HDR.Therefore,this study can provide a reference for seawater as a heat transfer fluid in the design of geothermal energy resource extraction.展开更多
Microbially induced calcium carbonate precipitation(MICP)technology can induce calcium carbonate crystals with cementation and stable performance in the process of microbial metabolism or enzymization through the regu...Microbially induced calcium carbonate precipitation(MICP)technology can induce calcium carbonate crystals with cementation and stable performance in the process of microbial metabolism or enzymization through the regulation of environmental factors MICP can be used as a cementing agent to cement cohesionless sand particles to form the materials with the characteristics of higher strength,better durability and environmental friendli-ness,as well as a good engineering application prospect.In this paper,the shear strength of sand column was tested by triaxial compression tests,and the strength index was obtained.In order to further study the micro-strength mechanism and the failure process,based on the discrete element method,a numerical model of MICP cemented sand column was established considering the factors of matrix soil particle gradation,particle mor-phology,content ratio of induced calcium carbonate,pore distribution characteristics,inter-particle cementation and so on.The failure process of MICP cemented sand column under load was analysed by numerical simulation,and the reliability of the numerical model was tested by combining with the stress intensity curve of samples under test conditions.The results indicate that compared with the actual triaxial tests of MICP cemented sand column,although there are deviations in stress and strain,cohesion and internal friction angle,the numerical simulation shows similar development law and intensity amplitude,and the same failure trend.The work in this paper verifies the reliability of the numerical model and provides a theoretical basis for the subsequent analysis of the factors influencing the geotechnical mechanical properties of biomineralized materials.展开更多
Rock-like specimens containing a joint with different inclination angles and roughness were prepared using 3D printing technology.Then,true triaxial compression loading experiments were conducted on those jointed spec...Rock-like specimens containing a joint with different inclination angles and roughness were prepared using 3D printing technology.Then,true triaxial compression loading experiments were conducted on those jointed specimens.The increase in roughness leads to an increase in the axial strength and peak strain.With the increasing inclination angle,the axial strength initially decreases from 30°to 60°and then increases from 60°to 90°.While the peak strain first rises from 30°to 45°and then declines from 45°to 90°.The variation in failure mode results from differences in lateral stress on the joints under different strike directions.Specimens with joint strike parallel to the intermediate principal stress predominantly showed matrix or matrix-joint mixed shear failure,whereas those parallel to the minimum principal stress exhibited matrix shear failure.The analysis results of acoustic emission signals indicate the crack number and shear crack percentage increase with the increasing roughness and first decrease(30°to 60°),then increase(60°to 90°)with the increasing inclination angle.The research results can provide some guidance for the design and support of underground engineering with jointed surrounding rock.展开更多
The backfill should keep stable in the primary stope when mining an adjacent secondary stope in subsequent open stoping mining methods,and the large-size mined-out area is usually backfilled by multiple backfilling be...The backfill should keep stable in the primary stope when mining an adjacent secondary stope in subsequent open stoping mining methods,and the large-size mined-out area is usually backfilled by multiple backfilling before the recovery of a secondary stope,resulting in a layered structure of backfill in stope.Therefore,it is significant to investigate the deformation responses and mechanical properties of stratified cemented tailings backfill(SCTB)with different layer structures to remain self-standing as an artificial pillar in the primary stope.The current work examined the effects of enhance layer position(1/3,1/2,and 2/3)and thickness ratio(0,0.1,0.2,and 0.3)on the mechanical properties,deformation,energy evolution,microstructures,and failure modes of SCTB.The results demonstrate that the incorporation of an enhance layer significantly strengthens the deformation and strength of SCTB.Under a confining pressure of 50 kPa,the peak deviatoric stress rises from 525.6 to 560.3,597.1,and 790.5 kPa as the thickness ratio of enhance layer is increased from 0 to 0.1,0.2,and 0.3,representing a significant increase of 6.6%,13.6%,and 50.4%.As the confining pressure increases,the slopes of the curves in the elastic stage become steep,and the plastic phase is extended accordingly.Additionally,the incorporation of the enhance layer significantly improves the energy storage linit of SCTB specimen.As the thickness ratio of the enhance layer increases from 0 to 0.1,0.2,and 0.3,the elastic energy rises from 0.54 to 0.67,0.84,and 1.00 MJ·m^(-3),representing a significant increase of 24.1%,55.6%,and 85.2%.The internal friction angles and cohesions of the SCTB specimens are higher than those of the CTB specimens,however,the cohesion is more susceptible to enhance layer position and thickness ratio than the internal friction angle.The failure style of the SCTB specimen changes from shear failure to splitting bulging failure and shear bulging failure with the presence of an enhance layer.The crack propagation path is significantly blocked by the enhance layer.The findings are of great significance to the application and stability of the SCTB in subsequent stoping backfilling mines.展开更多
Geological disasters will happen in cold regions because of the effects of freeze-thaw cycles on rocks or soils, so studying the effects of these cycles on the mechanical characteristics and permeability properties of...Geological disasters will happen in cold regions because of the effects of freeze-thaw cycles on rocks or soils, so studying the effects of these cycles on the mechanical characteristics and permeability properties of rocks is very important. In this study, red sandstone samples were frozen and thawed with o, 4, 8 and 12 cycles, each cycle including 12 h of freezing and 12 h of thawing. The P-wave velocities of these samples were measured, and the mechanical properties and evolution of the steady-state permeabilities were investigated in a series of uniaxial and triaxial compression tests. Experimental results show that, with the increasing of cyclic freeze-thaw times, the P-wave velocity of the red sandstone decreases. The number of freeze-thaw cycles has a significant influence on the uniaxial compressive strength, elastic modulus, cohesion, and angle of internal friction. The evolution of permeability of the rock samples after cycles of freeze-thaw in a complete stress-strain process under triaxial compression is closely related to the variation of the microstructure in the rock. There is a highly corresponding relationship between volumetric strain and permeability with axial strain in all stages of the stress-strain behaviour.展开更多
The mechanical behavior of plastic concrete used in the cut-off walls of earth dams has been studied. Triaxial compression tests on the specimens in various ages and mix designs under different confining pressures hav...The mechanical behavior of plastic concrete used in the cut-off walls of earth dams has been studied. Triaxial compression tests on the specimens in various ages and mix designs under different confining pressures have been done and the stress-strain behavior of such materials and their strength parameter changes have been experimentally investigated. It has been observed that increasing the confining pressures applied on the specimens causes the material behavior to be alike the more ductile materials and the compressive strength increases considerably as well. Moreover, a parametric study has been carded out to investigate the influence of essential parameters on the shear strength parameters of these materials. According to the research, increasing the coarse to fine aggregates ratio leads to the increase of compressive strength of the specimens as well as the increase of the cohesion and internal friction angle of the materials. Furthermore, the bentonite content decrease and the cement factor increase result in an increase of the cohesion parameter of plastic concretes and decrease of the internal friction angle of such materials.展开更多
Particle breakage continuously changes the grading of granular materials and has a significant effect on their mechanical behaviors.Revealing the evolution pattern of particle breakage is valuable for development and ...Particle breakage continuously changes the grading of granular materials and has a significant effect on their mechanical behaviors.Revealing the evolution pattern of particle breakage is valuable for development and validation of constitutive models for crushable materials.A series of parallel triaxial compression tests along the same loading paths but stopped at different axial strains were conducted on two coral sands with different particle sizes under drained and undrained conditions.The tested specimens were carefully sieved to investigate the intermediate accumulation of particle breakage during the loading process.The test results showed that under both drained and undrained conditions,particle breakage increases continuously with increasing axial strain but exhibits different accumulating patterns,and higher confining pressures lead to greater particle breakage.Based on the test results,the correlations between particle breakage and the stress state as well as the input energy were examined.The results demonstrated that either the stress state or input energy alone is inadequate for describing the intermediate process of particle breakage evolution.Then,based on experimental observation,a path-dependent model was proposed for particle breakage evolution,which was formulated in an incremental form and reasonably considers the effects of the past breakage history and current stress state on the breakage rate.The path-dependent model successfully reproduced the development of particle breakage during undrained triaxial compression using the parameters calibrated from the drained tests,preliminarily demonstrating its effectiveness for different stress paths.展开更多
To ensure safe and economical backfill mining,the mechanical response of the backfill–rock interaction system needs to be understood.The numerical investigation of the mechanical behavior of backfill–rock composite ...To ensure safe and economical backfill mining,the mechanical response of the backfill–rock interaction system needs to be understood.The numerical investigation of the mechanical behavior of backfill–rock composite structure(BRCS)under triaxial compression,which includes deformation,failure patterns,strength characteristics,and acoustic emission(AE)evolution,was proposed.The models used in the tests have one rough interface,two cement–iron tailings ratios(CTRs),four interface angles(IAs),and three confining pressures(CPs).Results showed that the deformation,strength characteristics,and failure patterns of BRCS under triaxial compression depend on IA,CP,and CTR.The stress–strain curves of BRCS under triaxial compression could be divided into five stages,namely,compaction,elasticity,yield,strain softening,and residual stress.The relevant AE counts have corresponding relationships with different stages.The triaxial compressive strengths of composites increase linearly with the increase of the CP.Furthermore,the CP stress strengthening effect occurs.When the IAs are45°and 60°,the failure areas of composites appear in the interface and backfill.When the IAs are 75°and 90°,the failure areas of composites appear in the backfill,interface,and rock.Moreover,the corresponding failure modes yield the combined shear failure.The research results provide the basis for further understanding of the stability of the BRCS.展开更多
To accurately predict coal burst hazards and estimate the failure of coal pillars in underground coal mining systems,it is of great significance to understand the mechanical behavior of coal-rock bimaterial composite ...To accurately predict coal burst hazards and estimate the failure of coal pillars in underground coal mining systems,it is of great significance to understand the mechanical behavior of coal-rock bimaterial composite structures.This paper presents experimental and numerical investigations on the response of rock-coal,coal-rock,and rock-coal-rock bimaterial composite structures under triaxial compression.The triaxial compression experiments are conducted under confining pressures in the range of 0-20 MPa.The resulting inside fracture networks are detected using X-ray-based computed tomography(CT).The experimentally observed data indicate that the mechanical parameters of the rock-coalrock composites are superior to those of the rock-coal and coal-rock combinations.After compression failure,the coal-rock combination specimens are analyzed via X-ray CT.The results display that the failure of the coal-rock composite bodies primarily takes place within the coal.Further,the bursting proneness is reduced by increasing confining pressure.Subsequently,the corresponding numerical simulations of the experiments are carried out by using the particle flow code.The numerical results reveal that coal is vulnerable with regard to energy storage and accumulation.展开更多
The mechanical behaviors of rocks affected by high temperature and stress are generally believed to be significant for the stability of certain projects involving rocks, such as nuclear waste storage and geothermal re...The mechanical behaviors of rocks affected by high temperature and stress are generally believed to be significant for the stability of certain projects involving rocks, such as nuclear waste storage and geothermal resource exploitation. In this paper, veined marble specimens were treated to high temperature treatment and then used in conventional triaxial compression tests to investigate the effect of temperature, confining pressure, and vein angle on strength and deformation behaviors. The results show that the strength and deformation parameters of the veined marble specimens changed with the temperature, presenting a critical temperature of 600 . The triaxial compression strength of a horizontal vein () is obviously larger than that of a vertical vein (). The triaxial compression strength, elasticity modulus, and secant modulus have an approximately linear relation to the confining pressure. Finally, Mohr-Coulomb and Hoek-Brown criteria were respectively used to analyze the effect of confining pressure on triaxial compression strength.展开更多
A series of triaxial compression tests for frozen clay were performed by KoDCGF (freezing with non-uniform temperature under loading after K0 consolidation) method and GFC (freezing with non-uniform temperature wit...A series of triaxial compression tests for frozen clay were performed by KoDCGF (freezing with non-uniform temperature under loading after K0 consolidation) method and GFC (freezing with non-uniform temperature without experiencing Ko consolidation) method at various confining pressures and thermal gradients. The experimental results indicate that the triaxial compression strength for frozen clay in KoDCGF test increases with the increase of confining pressure, but it decreases as the confining pressure increases further in GFC test. In other words, the compression strength for frozen clay with identical confining pressure decreases with the increase in thermal gradient both in KoDCGF test and GFC test. The strength of frozen clay in KoDCGF test is dependent of pore ice strength, soil particle strength and interaction between soil skeleton and pore ice. The decrease of water content and distance between soil particles leads to the decrease of pore size and the increase of contact area between particles in KoDCGF test, which further results in a higher compression strength than that in GFC test. The compression strength for frozen clay with thermal gradient can be descried by strength for frozen clay with a uniform temperature identical to the temperature at the height of specimen where the maximum tensile stress appears.展开更多
In deep geological disposal of high-level nuclear waste,one of the most important subjects is to estimate long-term stability and strength of host rock under high temperature conditions caused by radioactive decay of ...In deep geological disposal of high-level nuclear waste,one of the most important subjects is to estimate long-term stability and strength of host rock under high temperature conditions caused by radioactive decay of the waste.In this paper,some experimental researches on the thermo-mechanical characteristics of soft sedimentary rock have been presented.For this reason,a new temperature-controlled triaxial compression and creep test device,operated automatically by a computer-controlled system,whose control software has been developed by the authors,was developed to conduct the thermo-mechanical tests in different thermal loading paths,including an isothermal path.The new device is proved to be able to conduct typical thermo-mechanical element tests for soft rock.The test device and the related testing method were introduced in detail.Finally,some test results have been simulated with a thermo-elasto-viscoplastic model that was also developed by the authors.展开更多
The anisotropic mechanical behavior of rocks under high-stress and high-temperature coupled conditions is crucial for analyzing the stability of surrounding rocks in deep underground engineering.This paper is devoted ...The anisotropic mechanical behavior of rocks under high-stress and high-temperature coupled conditions is crucial for analyzing the stability of surrounding rocks in deep underground engineering.This paper is devoted to studying the anisotropic strength,deformation and failure behavior of gneiss granite from the deep boreholes of a railway tunnel that suffers from high tectonic stress and ground temperature in the eastern tectonic knot in the Tibet Plateau.High-temperature true triaxial compression tests are performed on the samples using a self-developed testing device with five different loading directions and three temperature values that are representative of the geological conditions of the deep underground tunnels in the region.Effect of temperature and loading direction on the strength,elastic modulus,Poisson’s ratio,and failure mode are analyzed.The method for quantitative identification of anisotropic failure is also proposed.The anisotropic mechanical behaviors of the gneiss granite are very sensitive to the changes in loading direction and temperature under true triaxial compression,and the high temperature seems to weaken the inherent anisotropy and stress-induced deformation anisotropy.The strength and deformation show obvious thermal degradation at 200℃due to the weakening of friction between failure surfaces and the transition of the failure pattern in rock grains.In the range of 25℃200℃,the failure is mainly governed by the loading direction due to the inherent anisotropy.This study is helpful to the in-depth understanding of the thermal-mechanical behavior of anisotropic rocks in deep underground projects.展开更多
Granular materials are omnipresent in industries and in nature. For small strains, elastic-plastic and hypoplastic constitutive relations are widely used in engineering practice, but they are not a significant reflect...Granular materials are omnipresent in industries and in nature. For small strains, elastic-plastic and hypoplastic constitutive relations are widely used in engineering practice, but they are not a significant reflection of the underlying physics. Under a unified thermodynamics framework explaining the physics of materials, granular solid hydrodynamics (GSH) was an ex- tension towards describing granular materials, not only solid-like, but also fluid-like behaviors. In this paper, the fundamentals of GSH are briefly treated and then simplified to analyze quasi- static deformations in triaxial compressions. The calculated stress-strain relations and volumetric strain are compared with experimental results. The influences of the major parameters in GSH, especially their cross coupling influences, are analyzed and their physical meanings are further clarified. After parameters were calibrated, the calculated stress values in the characteristic stress state are found to be within 22% of tested values. Meanwhile, the energy dissipation during triaxial compression is analyzed. The above results support and partially quantify GSH.展开更多
Crack initiation stress and crack damage stress are two critical indices for assessing the fracture strength of rock mass.However,understanding the stress characteristics of crack initiation and damage under triaxial ...Crack initiation stress and crack damage stress are two critical indices for assessing the fracture strength of rock mass.However,understanding the stress characteristics of crack initiation and damage under triaxial compression remains still immature.To address this problem,by acoustic monitoring,i.e.ultrasonic wave transmission and acoustic emission(AE),the integrated triaxial compression experiments were carried out on granitic specimens.The crack initiation and damage stresses were determined by wave velocity,wave amplitude and AE methods,respectively.The discrepancy of stresses for crack initiation and damage identified by these methods were examined.Results showed that the confinement affected the peak stress and corresponding strain,and these two parameters increased with increasing confining pressure.The ultrasonic wave velocity and wave amplitude first increased and then remained relatively stable,and finally decreased with increasing axial compressive stress.The number of AE events stayed at a relatively low extent until axial stress approached the peak;after that,the AE accumulative counts skyrocketed to the maximum.It also shows that for a given confinement,the stresses for crack initiation and damage identified by the wave amplitude method were the smallest,followed those by AE method and wave velocity method.Moreover,the stresses for crack initiation and crack damage identified by these methods increased generally with confining pressures.However,the rate of increment of these two crack stresses decreased with increasing confining pressure.In addition,the slight decrease in these two crack stresses ratios was noticed with increasing confining pressure.The findings are helpful to understand the crack stresses of deep rocks,in terms of support of deep underground engineering.展开更多
The initial micro-cracks affect the evolution characteristics of macroscopic deformation and failure of rock but are often ignored in theoretical calculation,numerical simulation,and mechanical experiments.In this stu...The initial micro-cracks affect the evolution characteristics of macroscopic deformation and failure of rock but are often ignored in theoretical calculation,numerical simulation,and mechanical experiments.In this study,we propose a quantitative analysis model to investigate the effects of initial micro-cracks on the evolution of marble deformation and failure.The relationship between the micro-crack propagation and the marble failure characteristics was comprehensively studied by combining theoretical analysis with a micro-computed tomography(micro-CT)scanning technique.We found that with the increase of confining pressure,the matrix elastic modulus of the marble first increased and then tended to be stable,while the micro-cracks increased exponentially.The sensitivity ranges of the marble sample matrix elastic modulus and micro-cracks to confining pressure were 0–30 MPa and 30–50 MPa,respectively.The porosity and Poisson’s ratio decreased exponentially.The increasing proportion of internal micro-cracks led to an increase in the sample non-uniformity.The samples presented mainly shear failure under triaxial compression,and the failure angle decreased linearly with the increase of confining pressure.The convergence direction of cracks decreased gradually.This quantitative analysis model could accurately portray the relationship between the overall macroscopic deformation and the deviatoric stress of the samples at the compaction and the linear elastic stages,thus deepening the understanding of the stress–strain behavior of rocks.展开更多
In practical engineering applications,rock mass are often found to be subjected to a triaxial stress state.Concurrently,defects like joints and fractures have a notable impact on the mechanical behavior of rock mass.S...In practical engineering applications,rock mass are often found to be subjected to a triaxial stress state.Concurrently,defects like joints and fractures have a notable impact on the mechanical behavior of rock mass.Such defects are identified as crucial contributors to the failure and instability of the surrounding rock,subsequently impacting the engineering stability.The study aimed to investigate the impact of fracture geometry and confining pressure on the deformation,failure characteristics,and strength of specimens using sand powder 3D printing technology and conventional triaxial compression tests.The results indicate that the number of fractures present considerably influences the peak strength,axial peak strain and elastic modulus of the specimens.Confining pressure is an important factor affecting the failure pattern of the specimen,under which the specimen is more prone to shear failure,but the initiation,expansion and penetration processes of secondary cracks in different fracture specimens are different.This study confirmed the feasibility of using sand powder 3D printing specimens as soft rock analogs for triaxial compression research.The insights from this research are deemed essential for a deeper understanding of the mechanical behavior of fractured surrounding rocks when under triaxial stress state.展开更多
Accurate estimation of the triaxial compression behavior of jointed coal is essential for coal mining.Few studies addressed the triaxial compression behavior of large-scale rock mass,especially with real joint geometr...Accurate estimation of the triaxial compression behavior of jointed coal is essential for coal mining.Few studies addressed the triaxial compression behavior of large-scale rock mass,especially with real joint geometry.We employed a numerical synthetic rock mass(SRM)method to study the triaxial compression behavior of jointed coal.Jointed-coal specimens were constructed based on in-situ joint measurements and microparameter calibration against laboratory experiments.A series of triaxial compression tests under different loading orientations and confining pressures were numerically performed to obtain joint and confining-pressure effects on the triaxial compression behavior and reveal the failure mechanism of jointed coal.Results suggest that the triaxial compression behavior of the jointed coal has strong joint and confining-pressure effects.Joints weaken the strength and elastic modulus,reduce the lateral deformation,and affect the geometries of the shear-rupture surface.An increase in the confining pressure causes the peak and residual strength increase significantly.With an increase in the confining pressure,the elastic modulus increases sharply at low confining pressure,the mechanical behavior transitions from brittleness to ductility,the failure mode transitions from shear-rupture surface to plastic flow,and the joint effect diminishes and even disappears.The jointed coal fails by means of a shear-rupture surface under triaxial compression loading with a confining pressure(which is not too high),and the geometries of the shear-rupture surface vary with the distribution of joints.展开更多
The strength of lightweight concrete under triaxial compressive stress is studied experimentally with the concrete triaxial apparatus designed by the authors, and is compared with that of normal concrete under the sam...The strength of lightweight concrete under triaxial compressive stress is studied experimentally with the concrete triaxial apparatus designed by the authors, and is compared with that of normal concrete under the same stress state. Ninety-five 100 mm cubes under twenty stress ratios are tested. As compared with normal concrete, it is found that not only the multiaxial compressive strength of lightweight concrete is small, but also the ratio of the multiaxial compressive strength to the uniaxial compressive strength is small. The influence of the intermediate principal stress on the multiaxial strength of lightweight concrete is discussed. The strength criteria which are expressed in the principal stresses and the octahedral stresses respectively are proposed.展开更多
基金financially supported by the National Natural Science Foundation of China(Nos.52174092,51904290,and 52374147)the Natural Science Foundation of Jiangsu Province,China(No.BK20220157)+2 种基金the Fundamental Research Funds for the Central Universities,China(No.2022YCPY0202)the National Key Research and Development Program of China(No.2023YFC3804204)the Major Program of Xinjiang Uygur Autonomous Region S cience and Technology(No.2023A01002)。
文摘The mechanical behavior of cemented gangue backfill materials(CGBMs)is closely related to particle size distribution(PSD)of aggregates and properties of cementitious materials.Consequently,the true triaxial compression tests,CT scanning,SEM,and EDS tests were conducted on cemented gangue backfill samples(CGBSs)with various carbon nanotube concentrations(P_(CNT))that satisfied fractal theory for the PSD of aggregates.The mechanical properties,energy dissipations,and failure mechanisms of the CGBSs under true triaxial compression were systematically analyzed.The results indicate that appropriate carbon nanotubes(CNTs)effectively enhance the mechanical properties and energy dissipations of CGBSs through micropore filling and microcrack bridging,and the optimal effect appears at P_(CNT)of 0.08wt%.Taking PSD fractal dimension(D)of 2.500 as an example,compared to that of CGBS without CNT,the peak strength(σ_(p)),axial peak strain(ε_(1,p)),elastic strain energy(Ue),and dissipated energy(U_(d))increased by 12.76%,29.60%,19.05%,and90.39%,respectively.However,excessive CNTs can reduce the mechanical properties of CGBSs due to CNT agglomeration,manifesting a decrease inρ_(p),ε_(1,p),and the volumetric strain increment(Δε_(v))when P_(CNT)increases from 0.08wt%to 0.12wt%.Moreover,the addition of CNTs improved the integrity of CGBS after macroscopic failure,and crack extension in CGBSs appeared in two modes:detour and pass through the aggregates.Theσ_(p)and U_(d)firstly increase and then decrease with increasing D,and porosity shows the opposite trend.Theε_(1,p)andΔε_(v)are negatively correlated with D,and CGBS with D=2.150 has the maximum deformation parameters(ε_(1,p)=0.05079,Δε_(v)=0.01990)due to the frictional slip effect caused by coarse aggregates.With increasing D,the failure modes of CGBSs are sequentially manifested as oblique shear failure,"Y-shaped"shear failure,and conjugate shear failure.
基金Projects(2024ZD1003903,2024ZD1003906)supported by the National Science and Technology Major ProjectProjects(U22A20166,52304097)supported by the National Natural Science Foundation of China+1 种基金Project(DUSE202301)supported by the Open Foundation of Key Laboratory of Deep Earth Science and Engineering(Sichuan University),Ministry of Education,ChinaProjects(2025A1515010049,2023A1515012654)supported by the Guangdong Basic and Applied Basic Research Foundation,China。
文摘Analyzing the fatigue damage characteristics of hot dry rock(HDR)affected by seawater thermal shock cycles is required for the efficient exploitation of HDR and the conservation of freshwater resources.Mechanical and acoustic emission(AE)monitoring tests were conducted during the triaxial compression of HDR at different confining pressures,temperatures,and numbers of seawater thermal shocks to investigate the seawater damage of HDR.The test results indicated an increase in the cumulative AE counts with increasing temperature and number of seawater thermal shocks,and a decrease in AE counts with increasing confining pressure.The effect of the number of seawater thermal shocks was significant.The AE counts were 276% higher at 15 than at 0 seawater thermal shocks.The b-value increased with the number of thermal shocks and stabilized after 5 shocks.Most of the damage was small fractures,which reduced the rock’s damage resistance.The AE time series under HDR triaxial compression exhibited multifractal features.High energy AE events dominated the damage mechanism of HDR,indicating shear damage to the HDR.Therefore,this study can provide a reference for seawater as a heat transfer fluid in the design of geothermal energy resource extraction.
基金sponsored by the National Natural Science Foundation of China(Grant No.12002173,12262027)Research start-up project of Inner Mongolia University of Technology(No.2200000924)key Lab.of University of Geological Hazards and Geotechnical Engineering Defense in Sandy and Drought Regions,Inner Mongolia Autonomous.
文摘Microbially induced calcium carbonate precipitation(MICP)technology can induce calcium carbonate crystals with cementation and stable performance in the process of microbial metabolism or enzymization through the regulation of environmental factors MICP can be used as a cementing agent to cement cohesionless sand particles to form the materials with the characteristics of higher strength,better durability and environmental friendli-ness,as well as a good engineering application prospect.In this paper,the shear strength of sand column was tested by triaxial compression tests,and the strength index was obtained.In order to further study the micro-strength mechanism and the failure process,based on the discrete element method,a numerical model of MICP cemented sand column was established considering the factors of matrix soil particle gradation,particle mor-phology,content ratio of induced calcium carbonate,pore distribution characteristics,inter-particle cementation and so on.The failure process of MICP cemented sand column under load was analysed by numerical simulation,and the reliability of the numerical model was tested by combining with the stress intensity curve of samples under test conditions.The results indicate that compared with the actual triaxial tests of MICP cemented sand column,although there are deviations in stress and strain,cohesion and internal friction angle,the numerical simulation shows similar development law and intensity amplitude,and the same failure trend.The work in this paper verifies the reliability of the numerical model and provides a theoretical basis for the subsequent analysis of the factors influencing the geotechnical mechanical properties of biomineralized materials.
基金Projects(52074259,52204132)supported by the National Natural Science Foundation of ChinaProject(104023002)supported by the Yunlong Lake Laboratory of Deep Underground Science and Engineering Project,China+2 种基金Project(BK20220157)supported by Natural Science Foundation of Jiangsu Province of ChinaProject(2023JJ40285)supported by Hunan Provincial Natural Science Foundation of ChinaProject(22B0469)supported by Scientific Research Foundation of Hunan Provincial Education Department,China。
文摘Rock-like specimens containing a joint with different inclination angles and roughness were prepared using 3D printing technology.Then,true triaxial compression loading experiments were conducted on those jointed specimens.The increase in roughness leads to an increase in the axial strength and peak strain.With the increasing inclination angle,the axial strength initially decreases from 30°to 60°and then increases from 60°to 90°.While the peak strain first rises from 30°to 45°and then declines from 45°to 90°.The variation in failure mode results from differences in lateral stress on the joints under different strike directions.Specimens with joint strike parallel to the intermediate principal stress predominantly showed matrix or matrix-joint mixed shear failure,whereas those parallel to the minimum principal stress exhibited matrix shear failure.The analysis results of acoustic emission signals indicate the crack number and shear crack percentage increase with the increasing roughness and first decrease(30°to 60°),then increase(60°to 90°)with the increasing inclination angle.The research results can provide some guidance for the design and support of underground engineering with jointed surrounding rock.
基金financially supported by the Fundamental Research Funds for the Central Universities,China(No.2023JCCXNY01)Guangxi Key Technologies R&D Program,China(No.2022AB31022).
文摘The backfill should keep stable in the primary stope when mining an adjacent secondary stope in subsequent open stoping mining methods,and the large-size mined-out area is usually backfilled by multiple backfilling before the recovery of a secondary stope,resulting in a layered structure of backfill in stope.Therefore,it is significant to investigate the deformation responses and mechanical properties of stratified cemented tailings backfill(SCTB)with different layer structures to remain self-standing as an artificial pillar in the primary stope.The current work examined the effects of enhance layer position(1/3,1/2,and 2/3)and thickness ratio(0,0.1,0.2,and 0.3)on the mechanical properties,deformation,energy evolution,microstructures,and failure modes of SCTB.The results demonstrate that the incorporation of an enhance layer significantly strengthens the deformation and strength of SCTB.Under a confining pressure of 50 kPa,the peak deviatoric stress rises from 525.6 to 560.3,597.1,and 790.5 kPa as the thickness ratio of enhance layer is increased from 0 to 0.1,0.2,and 0.3,representing a significant increase of 6.6%,13.6%,and 50.4%.As the confining pressure increases,the slopes of the curves in the elastic stage become steep,and the plastic phase is extended accordingly.Additionally,the incorporation of the enhance layer significantly improves the energy storage linit of SCTB specimen.As the thickness ratio of the enhance layer increases from 0 to 0.1,0.2,and 0.3,the elastic energy rises from 0.54 to 0.67,0.84,and 1.00 MJ·m^(-3),representing a significant increase of 24.1%,55.6%,and 85.2%.The internal friction angles and cohesions of the SCTB specimens are higher than those of the CTB specimens,however,the cohesion is more susceptible to enhance layer position and thickness ratio than the internal friction angle.The failure style of the SCTB specimen changes from shear failure to splitting bulging failure and shear bulging failure with the presence of an enhance layer.The crack propagation path is significantly blocked by the enhance layer.The findings are of great significance to the application and stability of the SCTB in subsequent stoping backfilling mines.
基金supported by the National Basic Research Program of China (973 Program) (Grant No. 2011CB013503)the National Natural Science Foundation of China (Grant No. 51374112)the Promotion Program for Young and Middle-aged Teacher in Science and Technology Research of Huaqiao University (ZQN-PY112)
文摘Geological disasters will happen in cold regions because of the effects of freeze-thaw cycles on rocks or soils, so studying the effects of these cycles on the mechanical characteristics and permeability properties of rocks is very important. In this study, red sandstone samples were frozen and thawed with o, 4, 8 and 12 cycles, each cycle including 12 h of freezing and 12 h of thawing. The P-wave velocities of these samples were measured, and the mechanical properties and evolution of the steady-state permeabilities were investigated in a series of uniaxial and triaxial compression tests. Experimental results show that, with the increasing of cyclic freeze-thaw times, the P-wave velocity of the red sandstone decreases. The number of freeze-thaw cycles has a significant influence on the uniaxial compressive strength, elastic modulus, cohesion, and angle of internal friction. The evolution of permeability of the rock samples after cycles of freeze-thaw in a complete stress-strain process under triaxial compression is closely related to the variation of the microstructure in the rock. There is a highly corresponding relationship between volumetric strain and permeability with axial strain in all stages of the stress-strain behaviour.
文摘The mechanical behavior of plastic concrete used in the cut-off walls of earth dams has been studied. Triaxial compression tests on the specimens in various ages and mix designs under different confining pressures have been done and the stress-strain behavior of such materials and their strength parameter changes have been experimentally investigated. It has been observed that increasing the confining pressures applied on the specimens causes the material behavior to be alike the more ductile materials and the compressive strength increases considerably as well. Moreover, a parametric study has been carded out to investigate the influence of essential parameters on the shear strength parameters of these materials. According to the research, increasing the coarse to fine aggregates ratio leads to the increase of compressive strength of the specimens as well as the increase of the cohesion and internal friction angle of the materials. Furthermore, the bentonite content decrease and the cement factor increase result in an increase of the cohesion parameter of plastic concretes and decrease of the internal friction angle of such materials.
基金This research was supported by the National Natural Science Foundation of China(Grant Nos.51679016 and 52079012).
文摘Particle breakage continuously changes the grading of granular materials and has a significant effect on their mechanical behaviors.Revealing the evolution pattern of particle breakage is valuable for development and validation of constitutive models for crushable materials.A series of parallel triaxial compression tests along the same loading paths but stopped at different axial strains were conducted on two coral sands with different particle sizes under drained and undrained conditions.The tested specimens were carefully sieved to investigate the intermediate accumulation of particle breakage during the loading process.The test results showed that under both drained and undrained conditions,particle breakage increases continuously with increasing axial strain but exhibits different accumulating patterns,and higher confining pressures lead to greater particle breakage.Based on the test results,the correlations between particle breakage and the stress state as well as the input energy were examined.The results demonstrated that either the stress state or input energy alone is inadequate for describing the intermediate process of particle breakage evolution.Then,based on experimental observation,a path-dependent model was proposed for particle breakage evolution,which was formulated in an incremental form and reasonably considers the effects of the past breakage history and current stress state on the breakage rate.The path-dependent model successfully reproduced the development of particle breakage during undrained triaxial compression using the parameters calibrated from the drained tests,preliminarily demonstrating its effectiveness for different stress paths.
基金financially supported by the National Natural Science Foundation of China(No.51774137)the Natural Science Foundation of Hebei Province,China(No.E2021209006)。
文摘To ensure safe and economical backfill mining,the mechanical response of the backfill–rock interaction system needs to be understood.The numerical investigation of the mechanical behavior of backfill–rock composite structure(BRCS)under triaxial compression,which includes deformation,failure patterns,strength characteristics,and acoustic emission(AE)evolution,was proposed.The models used in the tests have one rough interface,two cement–iron tailings ratios(CTRs),four interface angles(IAs),and three confining pressures(CPs).Results showed that the deformation,strength characteristics,and failure patterns of BRCS under triaxial compression depend on IA,CP,and CTR.The stress–strain curves of BRCS under triaxial compression could be divided into five stages,namely,compaction,elasticity,yield,strain softening,and residual stress.The relevant AE counts have corresponding relationships with different stages.The triaxial compressive strengths of composites increase linearly with the increase of the CP.Furthermore,the CP stress strengthening effect occurs.When the IAs are45°and 60°,the failure areas of composites appear in the interface and backfill.When the IAs are 75°and 90°,the failure areas of composites appear in the backfill,interface,and rock.Moreover,the corresponding failure modes yield the combined shear failure.The research results provide the basis for further understanding of the stability of the BRCS.
基金This study was financially supported by Beijing Outstanding Young Scientist Program(BJJWZYJH01201911413037)National Natural Science Foundation of China(41877257+3 种基金5162240452009131)Shaanxi Coal Group Key Project(2018SMHKJ-A-J-03)Yueqi outstanding scholar Award Program by CUMTB。
文摘To accurately predict coal burst hazards and estimate the failure of coal pillars in underground coal mining systems,it is of great significance to understand the mechanical behavior of coal-rock bimaterial composite structures.This paper presents experimental and numerical investigations on the response of rock-coal,coal-rock,and rock-coal-rock bimaterial composite structures under triaxial compression.The triaxial compression experiments are conducted under confining pressures in the range of 0-20 MPa.The resulting inside fracture networks are detected using X-ray-based computed tomography(CT).The experimentally observed data indicate that the mechanical parameters of the rock-coalrock composites are superior to those of the rock-coal and coal-rock combinations.After compression failure,the coal-rock combination specimens are analyzed via X-ray CT.The results display that the failure of the coal-rock composite bodies primarily takes place within the coal.Further,the bursting proneness is reduced by increasing confining pressure.Subsequently,the corresponding numerical simulations of the experiments are carried out by using the particle flow code.The numerical results reveal that coal is vulnerable with regard to energy storage and accumulation.
基金supported by the National Basic Research 973 Program of China (Grant 2013CB036003)the National Natural Science Foundation of China (Grants 51579239, 51323004, and 41572263)the China Postdoctoral Science Foundation (Grant 2016M590518)
文摘The mechanical behaviors of rocks affected by high temperature and stress are generally believed to be significant for the stability of certain projects involving rocks, such as nuclear waste storage and geothermal resource exploitation. In this paper, veined marble specimens were treated to high temperature treatment and then used in conventional triaxial compression tests to investigate the effect of temperature, confining pressure, and vein angle on strength and deformation behaviors. The results show that the strength and deformation parameters of the veined marble specimens changed with the temperature, presenting a critical temperature of 600 . The triaxial compression strength of a horizontal vein () is obviously larger than that of a vertical vein (). The triaxial compression strength, elasticity modulus, and secant modulus have an approximately linear relation to the confining pressure. Finally, Mohr-Coulomb and Hoek-Brown criteria were respectively used to analyze the effect of confining pressure on triaxial compression strength.
基金Project(50534040) supported by the National Natural Science Foundation of ChinaProject(20110491489) supported by China Postdoctoral Science FoundationProject(2011QNA03) supported by Fundamental Research Funds for the Central Universities of China
文摘A series of triaxial compression tests for frozen clay were performed by KoDCGF (freezing with non-uniform temperature under loading after K0 consolidation) method and GFC (freezing with non-uniform temperature without experiencing Ko consolidation) method at various confining pressures and thermal gradients. The experimental results indicate that the triaxial compression strength for frozen clay in KoDCGF test increases with the increase of confining pressure, but it decreases as the confining pressure increases further in GFC test. In other words, the compression strength for frozen clay with identical confining pressure decreases with the increase in thermal gradient both in KoDCGF test and GFC test. The strength of frozen clay in KoDCGF test is dependent of pore ice strength, soil particle strength and interaction between soil skeleton and pore ice. The decrease of water content and distance between soil particles leads to the decrease of pore size and the increase of contact area between particles in KoDCGF test, which further results in a higher compression strength than that in GFC test. The compression strength for frozen clay with thermal gradient can be descried by strength for frozen clay with a uniform temperature identical to the temperature at the height of specimen where the maximum tensile stress appears.
文摘In deep geological disposal of high-level nuclear waste,one of the most important subjects is to estimate long-term stability and strength of host rock under high temperature conditions caused by radioactive decay of the waste.In this paper,some experimental researches on the thermo-mechanical characteristics of soft sedimentary rock have been presented.For this reason,a new temperature-controlled triaxial compression and creep test device,operated automatically by a computer-controlled system,whose control software has been developed by the authors,was developed to conduct the thermo-mechanical tests in different thermal loading paths,including an isothermal path.The new device is proved to be able to conduct typical thermo-mechanical element tests for soft rock.The test device and the related testing method were introduced in detail.Finally,some test results have been simulated with a thermo-elasto-viscoplastic model that was also developed by the authors.
基金supported by Natural Science Foundation of China(Grant No.52278333)the Fundamental Research Funds for the Central Universities(Grant No.N2101021)The work is under the framework of the 111 Project(Grant No.B17009)and Sino-Franco Joint Research Laboratory on Multiphysics and Multiscale Rock Mechanics.
文摘The anisotropic mechanical behavior of rocks under high-stress and high-temperature coupled conditions is crucial for analyzing the stability of surrounding rocks in deep underground engineering.This paper is devoted to studying the anisotropic strength,deformation and failure behavior of gneiss granite from the deep boreholes of a railway tunnel that suffers from high tectonic stress and ground temperature in the eastern tectonic knot in the Tibet Plateau.High-temperature true triaxial compression tests are performed on the samples using a self-developed testing device with five different loading directions and three temperature values that are representative of the geological conditions of the deep underground tunnels in the region.Effect of temperature and loading direction on the strength,elastic modulus,Poisson’s ratio,and failure mode are analyzed.The method for quantitative identification of anisotropic failure is also proposed.The anisotropic mechanical behaviors of the gneiss granite are very sensitive to the changes in loading direction and temperature under true triaxial compression,and the high temperature seems to weaken the inherent anisotropy and stress-induced deformation anisotropy.The strength and deformation show obvious thermal degradation at 200℃due to the weakening of friction between failure surfaces and the transition of the failure pattern in rock grains.In the range of 25℃200℃,the failure is mainly governed by the loading direction due to the inherent anisotropy.This study is helpful to the in-depth understanding of the thermal-mechanical behavior of anisotropic rocks in deep underground projects.
基金support of the National Key Basic Research Program of China(No.2010CB731504)the National Natural Science Foundation of China(No.51239006)the research funding from the State Key Laboratoryof Hydroscience and Engineering,Tsinghua University(No.2013-KY-2)
文摘Granular materials are omnipresent in industries and in nature. For small strains, elastic-plastic and hypoplastic constitutive relations are widely used in engineering practice, but they are not a significant reflection of the underlying physics. Under a unified thermodynamics framework explaining the physics of materials, granular solid hydrodynamics (GSH) was an ex- tension towards describing granular materials, not only solid-like, but also fluid-like behaviors. In this paper, the fundamentals of GSH are briefly treated and then simplified to analyze quasi- static deformations in triaxial compressions. The calculated stress-strain relations and volumetric strain are compared with experimental results. The influences of the major parameters in GSH, especially their cross coupling influences, are analyzed and their physical meanings are further clarified. After parameters were calibrated, the calculated stress values in the characteristic stress state are found to be within 22% of tested values. Meanwhile, the energy dissipation during triaxial compression is analyzed. The above results support and partially quantify GSH.
基金funded by Shenzhen Basic Research Program,China(Grant No.JCYJ20220818095605012)the Program for Guangdong Introducing Innovative and Entrepreneurial Teams,China(Grant No.2019ZT08G315)the National Science Foundation of China(Grant No.52121003).
文摘Crack initiation stress and crack damage stress are two critical indices for assessing the fracture strength of rock mass.However,understanding the stress characteristics of crack initiation and damage under triaxial compression remains still immature.To address this problem,by acoustic monitoring,i.e.ultrasonic wave transmission and acoustic emission(AE),the integrated triaxial compression experiments were carried out on granitic specimens.The crack initiation and damage stresses were determined by wave velocity,wave amplitude and AE methods,respectively.The discrepancy of stresses for crack initiation and damage identified by these methods were examined.Results showed that the confinement affected the peak stress and corresponding strain,and these two parameters increased with increasing confining pressure.The ultrasonic wave velocity and wave amplitude first increased and then remained relatively stable,and finally decreased with increasing axial compressive stress.The number of AE events stayed at a relatively low extent until axial stress approached the peak;after that,the AE accumulative counts skyrocketed to the maximum.It also shows that for a given confinement,the stresses for crack initiation and damage identified by the wave amplitude method were the smallest,followed those by AE method and wave velocity method.Moreover,the stresses for crack initiation and crack damage identified by these methods increased generally with confining pressures.However,the rate of increment of these two crack stresses decreased with increasing confining pressure.In addition,the slight decrease in these two crack stresses ratios was noticed with increasing confining pressure.The findings are helpful to understand the crack stresses of deep rocks,in terms of support of deep underground engineering.
基金supported by the National Natural Science Foundation of China(Nos.12272119 and U1965101).
文摘The initial micro-cracks affect the evolution characteristics of macroscopic deformation and failure of rock but are often ignored in theoretical calculation,numerical simulation,and mechanical experiments.In this study,we propose a quantitative analysis model to investigate the effects of initial micro-cracks on the evolution of marble deformation and failure.The relationship between the micro-crack propagation and the marble failure characteristics was comprehensively studied by combining theoretical analysis with a micro-computed tomography(micro-CT)scanning technique.We found that with the increase of confining pressure,the matrix elastic modulus of the marble first increased and then tended to be stable,while the micro-cracks increased exponentially.The sensitivity ranges of the marble sample matrix elastic modulus and micro-cracks to confining pressure were 0–30 MPa and 30–50 MPa,respectively.The porosity and Poisson’s ratio decreased exponentially.The increasing proportion of internal micro-cracks led to an increase in the sample non-uniformity.The samples presented mainly shear failure under triaxial compression,and the failure angle decreased linearly with the increase of confining pressure.The convergence direction of cracks decreased gradually.This quantitative analysis model could accurately portray the relationship between the overall macroscopic deformation and the deviatoric stress of the samples at the compaction and the linear elastic stages,thus deepening the understanding of the stress–strain behavior of rocks.
基金Project(2021YFC2900600)supported by the Young Scientist Project of National Key Research and Development Program of ChinaProject(52074166)supported by the National Natural Science Foundation of China+1 种基金Projects(ZR2021YQ38,ZR2020QE121)supported by the Natural Science Foundation of Shandong Province,ChinaProject(2022KJ101)supported by the Science and Technology Support Plan for Youth Innovation of Colleges and Universities in Shandong Province,China。
文摘In practical engineering applications,rock mass are often found to be subjected to a triaxial stress state.Concurrently,defects like joints and fractures have a notable impact on the mechanical behavior of rock mass.Such defects are identified as crucial contributors to the failure and instability of the surrounding rock,subsequently impacting the engineering stability.The study aimed to investigate the impact of fracture geometry and confining pressure on the deformation,failure characteristics,and strength of specimens using sand powder 3D printing technology and conventional triaxial compression tests.The results indicate that the number of fractures present considerably influences the peak strength,axial peak strain and elastic modulus of the specimens.Confining pressure is an important factor affecting the failure pattern of the specimen,under which the specimen is more prone to shear failure,but the initiation,expansion and penetration processes of secondary cracks in different fracture specimens are different.This study confirmed the feasibility of using sand powder 3D printing specimens as soft rock analogs for triaxial compression research.The insights from this research are deemed essential for a deeper understanding of the mechanical behavior of fractured surrounding rocks when under triaxial stress state.
基金supported by the National Nature Science Foundation of China(51904153)funding of Tiandi Science&Technology Co Ltd(2022-2-TD-QN008,KJ2019-TDKCSYS-01).
文摘Accurate estimation of the triaxial compression behavior of jointed coal is essential for coal mining.Few studies addressed the triaxial compression behavior of large-scale rock mass,especially with real joint geometry.We employed a numerical synthetic rock mass(SRM)method to study the triaxial compression behavior of jointed coal.Jointed-coal specimens were constructed based on in-situ joint measurements and microparameter calibration against laboratory experiments.A series of triaxial compression tests under different loading orientations and confining pressures were numerically performed to obtain joint and confining-pressure effects on the triaxial compression behavior and reveal the failure mechanism of jointed coal.Results suggest that the triaxial compression behavior of the jointed coal has strong joint and confining-pressure effects.Joints weaken the strength and elastic modulus,reduce the lateral deformation,and affect the geometries of the shear-rupture surface.An increase in the confining pressure causes the peak and residual strength increase significantly.With an increase in the confining pressure,the elastic modulus increases sharply at low confining pressure,the mechanical behavior transitions from brittleness to ductility,the failure mode transitions from shear-rupture surface to plastic flow,and the joint effect diminishes and even disappears.The jointed coal fails by means of a shear-rupture surface under triaxial compression loading with a confining pressure(which is not too high),and the geometries of the shear-rupture surface vary with the distribution of joints.
文摘The strength of lightweight concrete under triaxial compressive stress is studied experimentally with the concrete triaxial apparatus designed by the authors, and is compared with that of normal concrete under the same stress state. Ninety-five 100 mm cubes under twenty stress ratios are tested. As compared with normal concrete, it is found that not only the multiaxial compressive strength of lightweight concrete is small, but also the ratio of the multiaxial compressive strength to the uniaxial compressive strength is small. The influence of the intermediate principal stress on the multiaxial strength of lightweight concrete is discussed. The strength criteria which are expressed in the principal stresses and the octahedral stresses respectively are proposed.