Stress-strain behavior of plastic concrete using monotonic triaxial compression tests 被引量:14
1
作者 Y.Pashang Pisheh S.M.Mir Mohammad Hosseini 《Journal of Central South University》 SCIE EI CAS 2012年第4期1125-1131,共7页
The mechanical behavior of plastic concrete used in the cut-off walls of earth dams has been studied. Triaxial compression tests on the specimens in various ages and mix designs under different confining pressures hav... The mechanical behavior of plastic concrete used in the cut-off walls of earth dams has been studied. Triaxial compression tests on the specimens in various ages and mix designs under different confining pressures have been done and the stress-strain behavior of such materials and their strength parameter changes have been experimentally investigated. It has been observed that increasing the confining pressures applied on the specimens causes the material behavior to be alike the more ductile materials and the compressive strength increases considerably as well. Moreover, a parametric study has been carded out to investigate the influence of essential parameters on the shear strength parameters of these materials. According to the research, increasing the coarse to fine aggregates ratio leads to the increase of compressive strength of the specimens as well as the increase of the cohesion and internal friction angle of the materials. Furthermore, the bentonite content decrease and the cement factor increase result in an increase of the cohesion parameter of plastic concretes and decrease of the internal friction angle of such materials. 展开更多
关键词 plastic concrete stress-strain behavior triaxial compression test STRENGTH elastic modulus
在线阅读 下载PDF
Effects of aggregate size distribution and carbon nanotubes on the mechanical properties of cemented gangue backfill samples under true triaxial compression
2
作者 Qian Yin Fan Wen +7 位作者 Zhigang Tao Hai Pu Tianci Deng Yaoyao Meng Qingbin Meng Hongwen Jing Bo Meng Jiangyu Wu 《International Journal of Minerals,Metallurgy and Materials》 SCIE EI CAS 2025年第2期311-324,共14页
The mechanical behavior of cemented gangue backfill materials(CGBMs)is closely related to particle size distribution(PSD)of aggregates and properties of cementitious materials.Consequently,the true triaxial compressio... The mechanical behavior of cemented gangue backfill materials(CGBMs)is closely related to particle size distribution(PSD)of aggregates and properties of cementitious materials.Consequently,the true triaxial compression tests,CT scanning,SEM,and EDS tests were conducted on cemented gangue backfill samples(CGBSs)with various carbon nanotube concentrations(P_(CNT))that satisfied fractal theory for the PSD of aggregates.The mechanical properties,energy dissipations,and failure mechanisms of the CGBSs under true triaxial compression were systematically analyzed.The results indicate that appropriate carbon nanotubes(CNTs)effectively enhance the mechanical properties and energy dissipations of CGBSs through micropore filling and microcrack bridging,and the optimal effect appears at P_(CNT)of 0.08wt%.Taking PSD fractal dimension(D)of 2.500 as an example,compared to that of CGBS without CNT,the peak strength(σ_(p)),axial peak strain(ε_(1,p)),elastic strain energy(Ue),and dissipated energy(U_(d))increased by 12.76%,29.60%,19.05%,and90.39%,respectively.However,excessive CNTs can reduce the mechanical properties of CGBSs due to CNT agglomeration,manifesting a decrease inρ_(p),ε_(1,p),and the volumetric strain increment(Δε_(v))when P_(CNT)increases from 0.08wt%to 0.12wt%.Moreover,the addition of CNTs improved the integrity of CGBS after macroscopic failure,and crack extension in CGBSs appeared in two modes:detour and pass through the aggregates.Theσ_(p)and U_(d)firstly increase and then decrease with increasing D,and porosity shows the opposite trend.Theε_(1,p)andΔε_(v)are negatively correlated with D,and CGBS with D=2.150 has the maximum deformation parameters(ε_(1,p)=0.05079,Δε_(v)=0.01990)due to the frictional slip effect caused by coarse aggregates.With increasing D,the failure modes of CGBSs are sequentially manifested as oblique shear failure,"Y-shaped"shear failure,and conjugate shear failure. 展开更多
关键词 cemented gangue backfill materials particle size distribution true triaxial compression test carbon nanotubes mechanical properties failure modes
在线阅读 下载PDF
Temperature-controlled triaxial compression/creep test device for thermodynamic properties of soft sedimentary rock and corresponding theoretical prediction 被引量:2
3
作者 Sheng Zhang Hirotomo Nakano +2 位作者 Yonglin Xiong Tomohiro Nishimura Feng Zhang 《Journal of Rock Mechanics and Geotechnical Engineering》 SCIE 2010年第3期255-261,共7页
In deep geological disposal of high-level nuclear waste,one of the most important subjects is to estimate long-term stability and strength of host rock under high temperature conditions caused by radioactive decay of ... In deep geological disposal of high-level nuclear waste,one of the most important subjects is to estimate long-term stability and strength of host rock under high temperature conditions caused by radioactive decay of the waste.In this paper,some experimental researches on the thermo-mechanical characteristics of soft sedimentary rock have been presented.For this reason,a new temperature-controlled triaxial compression and creep test device,operated automatically by a computer-controlled system,whose control software has been developed by the authors,was developed to conduct the thermo-mechanical tests in different thermal loading paths,including an isothermal path.The new device is proved to be able to conduct typical thermo-mechanical element tests for soft rock.The test device and the related testing method were introduced in detail.Finally,some test results have been simulated with a thermo-elasto-viscoplastic model that was also developed by the authors. 展开更多
关键词 temperature control soft sedimentary rock thermal triaxial compression test thermal triaxial creep test
在线阅读 下载PDF
Mechanical response and failure mechanism of inclined rough jointed rock under true triaxial compression loading
4
作者 LIU Han-xiang JING Hong-wen +3 位作者 YUAN Yong YIN Qian WEN Fan LI Bo 《Journal of Central South University》 2025年第10期4012-4034,共23页
Rock-like specimens containing a joint with different inclination angles and roughness were prepared using 3D printing technology.Then,true triaxial compression loading experiments were conducted on those jointed spec... Rock-like specimens containing a joint with different inclination angles and roughness were prepared using 3D printing technology.Then,true triaxial compression loading experiments were conducted on those jointed specimens.The increase in roughness leads to an increase in the axial strength and peak strain.With the increasing inclination angle,the axial strength initially decreases from 30°to 60°and then increases from 60°to 90°.While the peak strain first rises from 30°to 45°and then declines from 45°to 90°.The variation in failure mode results from differences in lateral stress on the joints under different strike directions.Specimens with joint strike parallel to the intermediate principal stress predominantly showed matrix or matrix-joint mixed shear failure,whereas those parallel to the minimum principal stress exhibited matrix shear failure.The analysis results of acoustic emission signals indicate the crack number and shear crack percentage increase with the increasing roughness and first decrease(30°to 60°),then increase(60°to 90°)with the increasing inclination angle.The research results can provide some guidance for the design and support of underground engineering with jointed surrounding rock. 展开更多
关键词 jointed rock true triaxial compression test mechanical response failure mechanism
在线阅读 下载PDF
Mechanical properties, deformation response, energy evolution and failure pattern of stratified cemented tailings backfill under triaxial compression
5
作者 Wenbin Xu Yalun Zhang +1 位作者 Kangqi Zhao Tong Sun 《International Journal of Minerals,Metallurgy and Materials》 2025年第10期2391-2405,共15页
The backfill should keep stable in the primary stope when mining an adjacent secondary stope in subsequent open stoping mining methods,and the large-size mined-out area is usually backfilled by multiple backfilling be... The backfill should keep stable in the primary stope when mining an adjacent secondary stope in subsequent open stoping mining methods,and the large-size mined-out area is usually backfilled by multiple backfilling before the recovery of a secondary stope,resulting in a layered structure of backfill in stope.Therefore,it is significant to investigate the deformation responses and mechanical properties of stratified cemented tailings backfill(SCTB)with different layer structures to remain self-standing as an artificial pillar in the primary stope.The current work examined the effects of enhance layer position(1/3,1/2,and 2/3)and thickness ratio(0,0.1,0.2,and 0.3)on the mechanical properties,deformation,energy evolution,microstructures,and failure modes of SCTB.The results demonstrate that the incorporation of an enhance layer significantly strengthens the deformation and strength of SCTB.Under a confining pressure of 50 kPa,the peak deviatoric stress rises from 525.6 to 560.3,597.1,and 790.5 kPa as the thickness ratio of enhance layer is increased from 0 to 0.1,0.2,and 0.3,representing a significant increase of 6.6%,13.6%,and 50.4%.As the confining pressure increases,the slopes of the curves in the elastic stage become steep,and the plastic phase is extended accordingly.Additionally,the incorporation of the enhance layer significantly improves the energy storage linit of SCTB specimen.As the thickness ratio of the enhance layer increases from 0 to 0.1,0.2,and 0.3,the elastic energy rises from 0.54 to 0.67,0.84,and 1.00 MJ·m^(-3),representing a significant increase of 24.1%,55.6%,and 85.2%.The internal friction angles and cohesions of the SCTB specimens are higher than those of the CTB specimens,however,the cohesion is more susceptible to enhance layer position and thickness ratio than the internal friction angle.The failure style of the SCTB specimen changes from shear failure to splitting bulging failure and shear bulging failure with the presence of an enhance layer.The crack propagation path is significantly blocked by the enhance layer.The findings are of great significance to the application and stability of the SCTB in subsequent stoping backfilling mines. 展开更多
关键词 stratified cemented tailings backfill enhance layer triaxial compressive tests mechanical properties energy evolution
在线阅读 下载PDF
Triaxial creep tests of weak sandstone from fracture zone of high dam foundation 被引量:13
6
作者 张玉 徐卫亚 +1 位作者 顾锦健 王伟 《Journal of Central South University》 SCIE EI CAS 2013年第9期2528-2536,共9页
The lithology of fracture zone which was developed at the dam foundation of a hydropower station is weak sandstone with poor integrity and pore cementation contact.Its creep properties have a significant impact on the... The lithology of fracture zone which was developed at the dam foundation of a hydropower station is weak sandstone with poor integrity and pore cementation contact.Its creep properties have a significant impact on the deformation and stability of the dam.Based on the characteristics of loose organizational structure,high moisture content and poor mechanical properties,the triaxial compression tests and creep tests were carried out,respectively.The results show significant non-linear,low strength and no obvious strength peaks.Both axial and lateral strains are achieved more than 3%when the tests are failed.The weak sandstone has a significant creep property,but only transient and steady state appear under low stress.Increased stress causes creep intensified and lateral strain gradually exceeds axial strain.In the failure stage,it has characteristics of large axial plastic deformation,obvious volumetric ductility dilation and large steady creep rate.The accelerated creep appears shortly after transient loading under confining of pressures 1.0 MPa and 1.5 MPa.Therefore,an improved Burgers creep model considering the non-linear characteristics of weak sandstone is built based on hyperbolic equation and the creep parameters are identified.This model can well describe the creep properties of weak sandstone. 展开更多
关键词 hydropower station weak sandstone creep properties triaxial compression tests triaxial creep tests improved Burgers creep model
在线阅读 下载PDF
Triaxial compression strength for artificial frozen clay with thermal gradient 被引量:2
7
作者 赵晓东 周国庆 陈国舟 《Journal of Central South University》 SCIE EI CAS 2013年第1期218-225,共8页
A series of triaxial compression tests for frozen clay were performed by KoDCGF (freezing with non-uniform temperature under loading after K0 consolidation) method and GFC (freezing with non-uniform temperature wit... A series of triaxial compression tests for frozen clay were performed by KoDCGF (freezing with non-uniform temperature under loading after K0 consolidation) method and GFC (freezing with non-uniform temperature without experiencing Ko consolidation) method at various confining pressures and thermal gradients. The experimental results indicate that the triaxial compression strength for frozen clay in KoDCGF test increases with the increase of confining pressure, but it decreases as the confining pressure increases further in GFC test. In other words, the compression strength for frozen clay with identical confining pressure decreases with the increase in thermal gradient both in KoDCGF test and GFC test. The strength of frozen clay in KoDCGF test is dependent of pore ice strength, soil particle strength and interaction between soil skeleton and pore ice. The decrease of water content and distance between soil particles leads to the decrease of pore size and the increase of contact area between particles in KoDCGF test, which further results in a higher compression strength than that in GFC test. The compression strength for frozen clay with thermal gradient can be descried by strength for frozen clay with a uniform temperature identical to the temperature at the height of specimen where the maximum tensile stress appears. 展开更多
关键词 artificial frozen clay triaxial compression test thermal gradient STRENGTH
在线阅读 下载PDF
Three dimensional discrete element modelling of the conventional compression behavior of gas hydrate bearing coal
8
作者 Xia Gao Nannan Wang +4 位作者 Baoyong Zhang Qiqi Lin Qiang Wu Wei Meng Xia Liu 《International Journal of Coal Science & Technology》 EI CAS CSCD 2024年第1期61-77,共17页
To analyze the relationship between macro and meso parameters of the gas hydrate bearing coal(GHBC)and to calibrate the meso-parameters,the numerical tests were conducted to simulate the laboratory triaxial compressio... To analyze the relationship between macro and meso parameters of the gas hydrate bearing coal(GHBC)and to calibrate the meso-parameters,the numerical tests were conducted to simulate the laboratory triaxial compression tests by PFC3D,with the parallel bond model employed as the particle contact constitutive model.First,twenty simulation tests were conducted to quantify the relationship between the macro–meso parameters.Then,nine orthogonal simulation tests were performed using four meso-mechanical parameters in a three-level to evaluate the sensitivity of the meso-mechanical parameters.Furthermore,the calibration method of the meso-parameters were then proposed.Finally,the contact force chain,the contact force and the contact number were examined to investigate the saturation effect on the meso-mechanical behavior of GHBC.The results show that:(1)The elastic modulus linearly increases with the bonding stiffness ratio and the friction coefficient while exponentially increasing with the normal bonding strength and the bonding radius coefficient.The failure strength increases exponentially with the increase of the friction coefficient,the normal bonding strength and the bonding radius coefficient,and remains constant with the increase of bond stiffness ratio;(2)The friction coefficient and the bond radius coefficient are most sensitive to the elastic modulus and the failure strength;(3)The number of the force chains,the contact force,and the bond strength between particles will increase with the increase of the hydrate saturation,which leads to the larger failure strength. 展开更多
关键词 Gas hydrate bearing coal Discrete element method triaxial compression test Macro-meso mechanical propertie
在线阅读 下载PDF
Thermomechanical failure analysis of sandstone subjected to high ground temperature
9
作者 Yan Zhang Chunchi Ma +4 位作者 Minglang Zou Tianbin Li Peng Zeng Yuemao Zhao Hongzhuo Fan 《Journal of Rock Mechanics and Geotechnical Engineering》 2025年第6期3524-3545,共22页
The temperature effect of rock failure has primarily focused on high temperature and large temperature gradients.However,the temperature range of engineered rocks in high ground temperature tunnel is generally within ... The temperature effect of rock failure has primarily focused on high temperature and large temperature gradients.However,the temperature range of engineered rocks in high ground temperature tunnel is generally within 100℃.For this,this study conducts real-time thermomechanical coupling tests with small temperature gradient within the engineering temperature.We analyzed rock mechanical parameter,rock failure characteristics,and acoustic emission(AE)and energy characteristics.The results indicate that the strength,peak strain,elastic modulus,and peak energy storage of sandstone decrease with increasing temperature.The peak AE count of sandstone in triaxial test at high temperature decreases with increasing temperature.The RA(Rising time/Amplitude)and AF(Average frequency)parameters associated with the AE signals indicate that the shear and tensile cracks are produced almost simultaneously throughout the rock failure process with increasing temperature.The PFC(particle flow code)simulation results show that the crack number of PBM(parallel bond model)specimen at high σ_(3) is significantly higher than that at low σ_(3) and the cracks number difference under high and low σ_(3) also rises as the temperature increases.Finally,the strength attenuation characteristics are explained by the competition and coupling action of temperature and σ_(3).This paper provides theoretical insights into rock failure mechanisms under thermomechanical coupling related to underground engineering. 展开更多
关键词 Temperature effect Thermomechanical coupling triaxial compression test Acoustic emission Energy characteristic Engineering temperature
在线阅读 下载PDF
Tri-axial compressive behavior of high-water material for deep underground spaces
10
作者 Honglin Liu Yang Xia +3 位作者 Jianbiao Bai Zhongzong Cao Zizheng Zhang Hongchao Zhao 《Deep Underground Science and Engineering》 2025年第3期482-497,共16页
Attributed to its superior water-to-solid ratio and quick setting time,the highwater material is widely adopted in underground spaces as a cost-effective and environmentally friendly backfill material.To elucidate the... Attributed to its superior water-to-solid ratio and quick setting time,the highwater material is widely adopted in underground spaces as a cost-effective and environmentally friendly backfill material.To elucidate the bleeding mechanism of high-water material under the high confining pressure,a total of 57 tubular specimens were prepared and tested,critical parameters of which included the water-to-solid ratio,curing time,and lateral confinement pressure.Test results showed that no obvious cracks were observed from the surface of confined highwater material,which is different from that of unconfined high-water material,which featured shear cracks.Moreover,the volume of these confined high-water materials under compaction exhibited a continuous shrinkage associated with the water bleeding.The threshold values of the water bleeding are significantly affected by the water-to-solid ratio,followed by the confining pressure and curing time.When other parameters are constant,the higher confinement is requested for these specimens with a small water-to-solid ratio.Meanwhile,the mass of bleeding water increased with the lateral confinement,showing a quick increase at the initial stage.During the bleeding process,the free water stored in the pores was compacted,the evidence of which is the transformation of the hydration products(calcium aluminate hydrate)from its natural fibrous structure into the rod-shaped or dense agglomerate structures.These research outcomes provide an in-depth insight into the fundamental mechanics of the high-water material under the high lateral confinement when it is used for underground spaces. 展开更多
关键词 bleeding mechanism free water high-water material laboratory tests lateral confinement triaxial compression test
原文传递
Characterization of unsaturated coarse-grained railway embankment fill:Water retention and dilatancy
11
作者 Yuanjie Xiao Wenqi Li +4 位作者 Liuxin Chen Xiaoming Wang Yunbo Li Pan Tan Jiapei Du 《Journal of Rock Mechanics and Geotechnical Engineering》 2025年第5期3125-3145,共21页
This study investigated the hydraulic and mechanical behaviors of unsaturated coarse-grained railway embankment fill materials(CREFMs)using a novel unsaturated large-scale triaxial apparatus equipped with the axis tra... This study investigated the hydraulic and mechanical behaviors of unsaturated coarse-grained railway embankment fill materials(CREFMs)using a novel unsaturated large-scale triaxial apparatus equipped with the axis translation technique(ATT).Comprehensive soil-water retention and constant-suction triaxial compression tests were conducted to evaluate the effects of initial void ratio,matric suction,and confining pressure on the properties of CREFMs.Key findings reveal a primary suction range of 0 e100 kPa characterized by hysteresis,which intensifies with decreasing density.Notably,the air entry value and residual suction are influenced by void ratio,with higher void ratios leading to decreased air entry values and residual suctions,underscoring the critical role of void ratio in hydraulic behavior.Additionally,the critical state line(CSL)in the bi-logarithmic space of void ratio and mean effective stress shifts towards higher void ratios with increasing matric suction,significantly affecting dilatancy and critical states.Furthermore,the study demonstrated that the mobilized friction angle and modulus properties depend on confining pressure and matric suction.A novel modified dilatancy equation was proposed,which enhances the predictability of CREFMs'responses under variable loading,particularly at high stress ratios defined by the deviatoric stress over the mean effective stress.This research advances the understanding of CREFMs'performance,especially under fluctuating environmental conditions that alter suction levels. 展开更多
关键词 Coarse-grained railway embankment fill materials(CREFMs) Soil-water retention curve(SWRC) Constant-suction triaxial compression test Critical state Dilatancy equation Unsaturated soil
在线阅读 下载PDF
Mechanical differences of laminations and crack propagation mechanism of continental shale
12
作者 Yong-Ting Duan Cheng-Cheng Zhu +3 位作者 Pathegama Gamage Ranjith Bai-Cun Yang Tian-Qiao Mao Yu Li 《Petroleum Science》 2025年第4期1653-1669,共17页
Clarify the mechanical properties of different laminations and the fracture mechanism of continental shale under in-situ stress can provide theoretical basis for more comprehensive evaluation of the fracability of con... Clarify the mechanical properties of different laminations and the fracture mechanism of continental shale under in-situ stress can provide theoretical basis for more comprehensive evaluation of the fracability of continental shale oil reservoir.The Chang 72continental shale was used to investigate the mechanical properties of laminations and the effect of natural structure on the crack propagation of the shale.The XRD and thin section tests show that the laminations contain two types:bright sandy lamination with void structure and dark muddy lamination with layer structure.The real-time CT uniaxial compression tests were conducted to investigate the differences of mechanical properties between the muddy lamination and sandy lamination.It found that the uniaxial compression strength and elastic modulus of the sandy lamination are higher,forming a simple crack with large opening,and the Poisson's ratio of the muddy lamination is large,forming obvious lateral deformation and more secondary cracks.On this basis,the cuboid-shaped continental shale specimens were tested under true triaxial compression conditions to study the effect of laminations and interface cracks on crack propagation combining AE and CT techniques.It found that nascent cracks connected laminations and interface cracks to form fracture network under appropriate loading condition,tensile cracks developed in sandy lamination and shear cracks occurred in muddy lamination because of deformation dissonance and brittleness index differences,and more secondary cracks formed in muddy lamination with smaller fracture toughness.Moreover,the combination relationships between nascent and natural cracks mainly conclude direct penetration and deflection,which is affected by the filling degree and morphology of interface cracks and the relationship of lamination types.These conclusions show that laminar continental shale is conducive to forming complex fracture network,which can provide a theoretical basis for the proposal of indicators and methods for fracability evaluation. 展开更多
关键词 Continental shale oil Mechanical properties of different lamination types True triaxial compression test Structure control mechanism Fracability evaluation
原文传递
Coupling effects of confiningpressure and strain rate on rock compressive strength
13
作者 Yongan Ma Chong Yu +3 位作者 Haibo Li Zun Cheng Yaqun Liu Jiajun Wu 《Journal of Rock Mechanics and Geotechnical Engineering》 2025年第11期6881-6899,共19页
This study systematically investigated the coupling effects of confiningpressure and strain rate on the dynamic strength of granite through dynamic triaxial compression tests.A dynamic strength criterion was developed... This study systematically investigated the coupling effects of confiningpressure and strain rate on the dynamic strength of granite through dynamic triaxial compression tests.A dynamic strength criterion was developed to incorporate these coupling effects for further analysis.Moreover,the research thoroughly revealed the underlying mechanism by which these coupling effects influencethe rock strength.The results revealed that both confiningpressure and strain rate significantly enhanced the dynamic strength of rock;however,a mutual inhibition effect emerged under their coupling.Specifically,as the confiningpressure increased,the strengthening effect of strain rate gradually diminished.Conversely,increasing the strain rate weakened the strengthening effect of confiningpressure.The proposed strength criterion successfully predicted rock strength under various confiningpressures(0-225 MPa)and strain rates(10^(-6)-600 s^(-1)).It achieved an average prediction error of only 8.3%,which represents a 65%improvement in accuracy compared to models that consider confiningpressure and strain rate effects independently.At the micro-mechanism level,increasing confiningpressure and strain rate promoted crack propagation in a transgranular(TG)mode,thereby enhancing the overall rock strength.However,under the coupling effects,the interference and interaction of TG cracks weakened the overall strengthening effect.This indicated that the competitive interaction between confiningpressure and strain rate during crack propagation constitutes the intrinsic mechanism underlying their mutual inhibitory effect on rock strength.This study provides a more accurate theoretical basis for understanding the dynamic responses of rocks and contributes valuable insights for disaster prevention and control in deep rock engineering projects. 展开更多
关键词 Confiningpressure-strain rate interaction Dynamic compressive strength Dynamic strength criterion Dynamic triaxial compression test Crack propagation
在线阅读 下载PDF
An investigation into the effects of lime on compressive and shear strength characteristics of fiber-reinforced clays 被引量:9
14
作者 Mahmood Reza Abdi Abbas Ghalandarzadeh Leila Shafiei Chafi 《Journal of Rock Mechanics and Geotechnical Engineering》 SCIE CSCD 2021年第4期885-898,共14页
To meet the ever-increasing construction demands around the world during recent years,reinforcement and stabilization methods have been widely used by geotechnical engineers to improve the performances and behavior of... To meet the ever-increasing construction demands around the world during recent years,reinforcement and stabilization methods have been widely used by geotechnical engineers to improve the performances and behavior of fine-grained soils.Although lime stabilization increases the compressive strength of soils,it reduces the soil ductility at the same time.Recent research shows that random fiber inclusion modifies the brittleness of soils.In the current research,the effects of lime and polypropylene(PP)fiber additions on such characteristics as compressive and shear strengths,failure strain,secant modulus of elasticity(E50)and shear strength parameters of mixtures were investigated.Kaolinite was treated with 1%,3% and 5% lime by dry weight of soil and reinforced with 0.1% monovalent PP fibers with the length of 6 mm.Samples were prepared at optimum conditions and cured at 35℃ for 1 d,7 d and 28 d at 90% relative humidity and subsequently subjected to uniaxial and triaxial compression tests(UCT and TCT)under cell pressures of 25 kPa,50 kPa and 100 kPa.Results showed that inclusion of random PP fibers to clay-lime mixtures increases both compressive and shear strengths as well as the ductility.Lime content and curing period were found to be the most influential factors.Scanning electron microscopy(SEM)analysis showed that lime addition and the formation of cementitious compounds bind soil particles and increase soil/fiber interactions at interface,leading to enhanced shear strength.The more ductile the stabilized and reinforced composition,the less the cracks in roads and waste landfill covers. 展开更多
关键词 KAOLINITE LIME Polypropylene(PP) Fiber-reinforced clay triaxial compression test(TCT) Uniaxial compression test(UCT) Scanning electron microscopy(SEM)
在线阅读 下载PDF
Effect of gravel on rock failure in glutenite reservoirs under different confining pressures 被引量:3
15
作者 Jian-Tong Liu Jian-Bo Wang +5 位作者 Hong-Kui Ge Wei Zhou Bei-Bei Chen Xiao-Di Li Xian-Jie Xue Sen-Lin Luo 《Petroleum Science》 SCIE EI CSCD 2023年第5期3022-3036,共15页
Due to the existence of gravel,glutenite is heterogeneous and different from fine-grained rocks such as sandstone and shale in structure.To fully understand the effect of gravel on failure mode in glutenite,we perform... Due to the existence of gravel,glutenite is heterogeneous and different from fine-grained rocks such as sandstone and shale in structure.To fully understand the effect of gravel on failure mode in glutenite,we performed triaxial compression tests on different glutenites.The results indicate that failure modes of glutenite are complex due to the existence of gravel.Under different confining pressures,three failure modes were observed.The first failure mode,a tensile failure under uniaxial compression,produces multiple tortuous longitudinal cracks.In this failure mode,the interaction between gravels provides the lateral tensile stress for rock splitting.The second failure mode occurs under low and medium confining pressure and produces a crack band composed of micro-cracks around gravels.This failure mode conforms to the Mohr-Coulomb criterion and is generated by shear failure.In this failure mode,shear dilatancy and shear compaction may occur under different confining pressures to produce different crack band types.In the second failure mode,gravel-induced stress concentration produces masses of initial micro-cracks for shear cracking,and gravels deflect the fracture surfaces.As a result,the fracture is characterized by crack bands that are far broader than in fine-grained rocks.The third failure mode requires high confining pressure and produces disconnected cracks around gravels without apparent crack bands.In this failure mode,the gravel rarely breaks,indicating that the formation of these fractures is related to the deformation of the matrix.The third failure mode requires lower confining pressure in glutenite with weak cement and matrix support.Generally,unlike fine-grained rocks,the failure mode of glutenite is not only controlled by confining pressure but also by the gravel.The failure of glutenite is characterized by producing cracks around gravels.These cracks are produced by different mechanisms and distributed in different manners under different confining pressures to form different fracture patterns.Therefore,understanding the rock microstructure and formation stress state is essential in guiding glutenite reservoir development. 展开更多
关键词 GLUTENITE HETEROGENEITY Failure mode triaxial compression test Shear dilatancy Shear compaction
原文传递
A Strain Rate Dependent Constitutive Model for the Lower Silurian Longmaxi Formation Shale in the Fuling Gas Field of the Sichuan Basin,China 被引量:3
16
作者 HOU Zhenkun LI Xianwen +4 位作者 ZHANG Yanming LIANG Huqing GUO Ying CHENG Hanlie GAO Ruchao 《Acta Geologica Sinica(English Edition)》 SCIE CAS CSCD 2019年第4期972-981,共10页
Shale,as a kind of brittle rock,often exhibits different nonlinear stress-strain behavior,failure and timedependent behavior under different strain rates.To capture these features,this work conducted triaxial compress... Shale,as a kind of brittle rock,often exhibits different nonlinear stress-strain behavior,failure and timedependent behavior under different strain rates.To capture these features,this work conducted triaxial compression tests under axial strain rates ranging from 5×10-6 s-1 to 1×10-3 s-1.The results show that both elastic modulus and peak strength have a positive correlation relationship with strain rates.These strain rate-dependent mechanical behaviors of shale are originated from damage growth,which is described by a damage parameter.When axial strain is the same,the damage parameter is positively correlated with strain rate.When strain rate is the same,with an increase of axial strain,the damage parameter decreases firstly from an initial value(about 0.1 to 0.2),soon reaches its minimum(about 0.1),and then increases to an asymptotic value of 0.8.Based on the experimental results,taking yield stress as the cut-off point and considering damage variable evolution,a new measure of micro-mechanical strength is proposed.Based on the Lemaitre’s equivalent strain assumption and the new measure of micro-mechanical strength,a statistical strain-rate dependent damage constitutive model for shale that couples physically meaningful model parameters was established.Numerical back-calculations of these triaxial compression tests results demonstrate the ability of the model to reproduce the primary features of the strain rate dependent mechanical behavior of shale. 展开更多
关键词 strain rates triaxial compression tests damage variable constitutive model Longmaxi Formation shale
在线阅读 下载PDF
Mechanical Properties of Soil-Rock Mixture Filling in Fault Zone Based on Mesostructure 被引量:2
17
作者 Mei Tao Qingwen Ren +2 位作者 Hanbing Bian Maosen Cao Yun Jia 《Computer Modeling in Engineering & Sciences》 SCIE EI 2022年第8期681-705,共25页
Soil-rock mixture(SRM)filling in fault zone is an inhomogeneous geomaterial,which is composed of soil and rock block.It controls the deformation and stability of the abutment and dam foundation,and threatens the long-... Soil-rock mixture(SRM)filling in fault zone is an inhomogeneous geomaterial,which is composed of soil and rock block.It controls the deformation and stability of the abutment and dam foundation,and threatens the long-term safety of high arch dams.To study the macroscopic and mesoscopic mechanical properties of SRM,the development of a viable mesoscopic numerical simulation method with a mesoscopic model generation technology,and a reasonable parametric model is crucially desired to overcome the limitations of experimental conditions,specimen dimensions,and experiment fund.To this end,this study presents a mesoscopic numerical method for simulating the mechanical behavior of SRM by proposing mesoscopic model generation technology based on its mesostructure features,and a rock parameter model considering size effect.The validity and rationality of the presented mesoscopic numerical method is experimentally verified by the triaxial compression tests with different rock block contents(RBC).The results indicate that the rock block can increase the strength of SRM,and it is proved that the random generation technique and the rock parameter model considering size effect are validated.Furthermore,there are multiple failure surfaces for inhomogeneous geomaterial of SRM,and the angle of the failure zone is no longer 45◦.The yielding zones of the specimen are more likely to occur in thin sections of soil matrix isolated by blocks with the failure path avoiding the rock block.The proposed numerical method is effective to investigate the meso-damage mechanism of SRM. 展开更多
关键词 Soil-rock mixture(SRM) triaxial compression tests random generation technique MESOSTRUCTURE rock parameter model size effect finite element method
在线阅读 下载PDF
Stress-strain relationship of unsaturated cohesive soil 被引量:2
18
作者 梅国雄 陈启明 姜朋明 《Journal of Central South University》 SCIE EI CAS 2010年第3期653-657,共5页
A moisture-content based constitutive model was proposed based on the hyperbolic model as an attempt to move towards the implementation of unsaturated soil mechanics into routine geotechnical engineering practice. The... A moisture-content based constitutive model was proposed based on the hyperbolic model as an attempt to move towards the implementation of unsaturated soil mechanics into routine geotechnical engineering practice. The stress-strain behavior of in-situ soil at a depth of 5 m was investigated by conducting undrained triaxial compression tests using the remolded soil samples. The test results show that the stress-strain relationship of unsaturated cohesive soil is still hyperbolic. The values of parameters a and b given in the model decrease with increasing the confining pressure for soil samples with the same moisture content and increase with increasing the moisture content for soil samples under the same confining pressure. The relationships between parameters a, b and moisture content were studied for confining pressures of 100, 150, 200 and 250 kPa. The comparison between the measured and predicted stress-strain curves for an additional group of soil samples, having a moisture content of 25.4%, shows that the proposed moisture content-dependent hyperbolic model provides a good prediction of stress-strain behavior of unsaturated cohesive soil. 展开更多
关键词 unsaturated cohesive soil moisture content triaxial compression test stress-strain relationship
在线阅读 下载PDF
振动拉压扭剪三轴仪及其试验研究 被引量:10
19
作者 姚仰平 谢定义 《西安建筑科技大学学报(自然科学版)》 CSCD 1996年第2期129-133,共5页
简要介绍了国内首创的振动拉压扭剪三轴仪的主要特征,给出了饱和标准砂的部分动力试验结果,并对其作了必要的分析研究。
关键词 振动三轴仪 动三轴试验 砂土液化
在线阅读 下载PDF
Shear Strength Behavior of Two Landfill Clay Liners 被引量:1
20
作者 Jian Wenxing Engineering Faculty, China University of Geosciences, Wuhan 430074 Masashi Kamon Toru Inui Department of Global Environmental Engineering, Graduate School of Engineering, Kyoto University,Kyoto, 606 8501, Japan Takeshi Katsumi Department of Civil Engineering, Ritsumeikan University, Kusatsu, Shiga, 525 8577, Japan 《Journal of China University of Geosciences》 SCIE CSCD 2002年第3期260-265,共5页
Direct shear tests were conducted to obtain both the shear strength ofcompacted clay liners (CCLs) specimens and the interface shear strength between compacted clay linerand base soil. These experiments were conducted... Direct shear tests were conducted to obtain both the shear strength ofcompacted clay liners (CCLs) specimens and the interface shear strength between compacted clay linerand base soil. These experiments were conducted under the conditions of five different watercontents. The experimental results show that shear strength of both CCLs and CCLs/base interfacedecreases with the increase in the water content of CCLs and base soil. In addition, the considerateconcentration of NaCl in leachate has no deteriorating effect on the shear strength of liners.Triaxial shear tests were also conducted on clay liner specimens to obtain total and effective shearstrength under a fast compression. The shear strength parameters with total stress are φ=18. 5°and c=30 kPa for clay-bentonite, and φ=48. 5° and c=90 kPa for sand-bentonite and those witheffective stress are φ'= 27. 2° and c'=25 kPa for clay-bentonite, and φ'=35° and c'=100 kPa forsand-bentonite, respectively. These results indicate that the compacted clay-bentonite shows normalconsolidation, but that the compacted sand-bentonite exhibits over-consolidation. 展开更多
关键词 shear strength behavior direct shear test CU triaxial compression test compacted clay liner LANDFILL