Photocatalytic purification of dye-containing wastewater using a novel embedded hybrid TiO2–slag catalyst heterojunction nanocomposite coupled with statistical models: A sustainable and techno-economic approach
1
作者 Kingsley Safo Norbert Onen Rubangakene +1 位作者 Hussien Noby Ahmed H.El-Shazly 《Water Science and Engineering》 2025年第2期151-164,共14页
The steel industry produces many byproducts, requiring extensive land for storage and causing significant environmental contamination. Industrial effluents discharged into water bodies negatively impact both aquatic e... The steel industry produces many byproducts, requiring extensive land for storage and causing significant environmental contamination. Industrial effluents discharged into water bodies negatively impact both aquatic ecosystems and human health. To solve this problem, this study synthesized a composite of titanium dioxide (TiO2) and steel slag nanocomposites (SSNC) at a 1:2 mass ratio to create a robust photocatalyst for the treatment of synthetic wastewater. The efficacy of this catalyst in degrading various dye pollutants, including methylene blue (MB), was tested under simulated solar light conditions. Comprehensive analyses were conducted to assess the physical and chemical characteristics, crystalline structure, energy gap, and point of zero charge of the composite. The TiO2-SSNC composite catalyst exhibited excellent stability, with a point of zero charge at 8.342 and an energy gap of 2.4 eV. The degradation process conformed to pseudo-first-order kinetics. Optimization of operational parameters was achieved through the response surface methodology. Reusability tests demonstrated that the TiO2-SSNC composite catalyst effectively degraded up to 93.41% of MB in the suspended mode and 92.03% in the coated mode after five cycles. Additionally, the degradation efficiencies for various dyes were significant, highlighting the potential of the composite for broad applications in industrial wastewater treatment. This study also explored the degradation mechanisms and identified byproducts, establishing a pathway for contaminant breakdown. The cost-benefit analysis revealed a total cost of 0.842 8 USD per cubic meter for each treatment activity, indicating low operational and production costs. These findings underscore the promise of the TiO2-SSNC composite as a cost-effective and efficient alternative for wastewater purification. 展开更多
关键词 tio2 Photocatalysis Steel slag Response surface methodology Dye degradation Transformation products
在线阅读 下载PDF
基于溶胶-凝胶TiO2的棉织物多功能整理
2
作者 周稚荃 李颖 +3 位作者 马青松 张学坤 任琪 王妮 《上海纺织科技》 2024年第11期49-51,59,共4页
以钛酸四丁酯为前驱体,通过溶胶-凝胶法制备二氧化钛(TiO2)溶胶,以棉织物为基体,经二浸二轧后分别通过焙烘和汽蒸的热固化方式将二氧化钛溶胶整理于织物表面得到功能改性棉织物。通过扫描电子显微镜(SEM)、扫描仪、Datacolor型测色配色... 以钛酸四丁酯为前驱体,通过溶胶-凝胶法制备二氧化钛(TiO2)溶胶,以棉织物为基体,经二浸二轧后分别通过焙烘和汽蒸的热固化方式将二氧化钛溶胶整理于织物表面得到功能改性棉织物。通过扫描电子显微镜(SEM)、扫描仪、Datacolor型测色配色仪、紫外线防护系数测试仪、导热系数测试仪、接触角测量仪等对整理前后织物的表面形貌、灰度差、遮蔽率、防紫外性能、隔热性能和静态水接触角进行测试。结果表明,整理后棉织物表面形成二氧化钛薄膜,织物具有较好的抗紫外性能,同时视觉遮蔽性能有所改善,还兼具较好的隔热性能和疏水性能。 展开更多
关键词 棉织物 溶胶-凝胶 tio2 视觉遮蔽性能 抗紫外性能
原文传递
多孔碳基TiO2纳米复合微粒制备及其降解罗丹明B的研究
3
作者 赵鹏 齐晓彤 +2 位作者 王海帆 王佳爽 贾正锋 《中文科技期刊数据库(全文版)自然科学》 2024年第5期163-170,共8页
以杨絮纤维和硼酸钙(CaB)为模板,以聚多巴胺(PDA)为联结剂及模板制备二氧化钛(TiO2)纳米复合微粒(Catkin/CaB/PDA/TiO2 )。在惰性气氛(Ar)下烧结、腐蚀制备多孔碳基TiO2纳米复合微粒。利用扫描电子显微镜(SEM)、透射电子显微镜(TEM)、X... 以杨絮纤维和硼酸钙(CaB)为模板,以聚多巴胺(PDA)为联结剂及模板制备二氧化钛(TiO2)纳米复合微粒(Catkin/CaB/PDA/TiO2 )。在惰性气氛(Ar)下烧结、腐蚀制备多孔碳基TiO2纳米复合微粒。利用扫描电子显微镜(SEM)、透射电子显微镜(TEM)、X射线衍射(XRD)、同步热分析(TGA)考察样品结构。利用 Belsorp-max物理吸附仪研究样品比表面积。利用紫外可见分光光度计和光致发光光谱(PL)测定样品光降解效率和荧光强度。研究所制备纳米微粒对罗丹明B(RhB)的催化降解性能,发现TiO2的含量、烧结温度、聚多巴胺、硼酸盐等对RhB光降解能力均有影响。所制备复合微粒在40 min内对RhB的降解率可达94.92%。烧结促使杨絮纤维和PDA碳化,所形成的管状碳材料和多孔结构为光生电子向碳化飞絮富集并与活性物种发生氧化还原反应和TiO2纳米粒子的附着和分散提供了保障进一步促进光解效果提升。 展开更多
关键词 杨絮 tio2 多孔碳 光催化 RHB
在线阅读 下载PDF
Photocatalytic Decoloration of Methyl Orange by TiO2 in Slurry
4
作者 M’Bra Ignace Christian Konan Affoué Tindo Sylvie +4 位作者 Gnagne Essoh Jean Eudes Yves Yacouba Zoungranan Touré Late Arsène Ekou Lynda Ekou Tchirioua 《American Journal of Analytical Chemistry》 CAS 2024年第11期347-356,共10页
The problem of water depollution is gaining importance, especially as regulatory standards concerning drinking water are increasingly strict. The different industries (textile industries) generate chemically stable po... The problem of water depollution is gaining importance, especially as regulatory standards concerning drinking water are increasingly strict. The different industries (textile industries) generate chemically stable pollutants such as methyl orange which make their degradation difficult. It is therefore necessary to find new, more effective techniques for the treatment of these discharges. Among the different solutions proposed to deal with this problem, we find advanced oxidation processes (POAs) which are clean and promising technologies in the field of wastewater depollution. In this regard, heterogeneous photocatalysis was used in an aqueous suspension of titanium oxide (TiO2) using a ultraviolet (UV) lamp as artificial radiation. The objective of this work is to study the influence of some operating parameters such as: the catalyst mass, the initial pollutant concentration, the volume of the solution and the pH of the solution, were examined. The results obtained showed that this photocatalyst made it possible to degrade 99.85% of the initial concentration of methyl orange (10 ppm), after 240 min of irradiation with an optimal mass of 0.50 g of TiO2 for a volume of 200 mL of methyl orange solution at pH = 3.0. 展开更多
关键词 DEPOLLUTION Methyl Orange tio2 SLURRY
在线阅读 下载PDF
TiO2纳米管的制备及其光电性能研究
5
作者 李荡 张杨 《山东化工》 CAS 2024年第1期48-50,54,共4页
采用水热法成功地制备了厚度为1 nm,直径为15 nm的TiO_(2)纳米管。利用差热-热重分析、X射线衍射、透射电镜及紫外-可见漫反射光谱对产物的结构进行了表征,并通过TiO_(2)纳米管对甲基橙的降解效果对其光催化活性进行评价。结果表明:制备... 采用水热法成功地制备了厚度为1 nm,直径为15 nm的TiO_(2)纳米管。利用差热-热重分析、X射线衍射、透射电镜及紫外-可见漫反射光谱对产物的结构进行了表征,并通过TiO_(2)纳米管对甲基橙的降解效果对其光催化活性进行评价。结果表明:制备的TiO_(2)纳米管有锐钛矿和金红石两种晶型,反应时间对样品的组织结构和光催化活性有较大影响,金红石相比例随着反应时间的增长而减少。反应时间为12 h时,TiO_(2)纳米管具有更佳的晶型比例及形貌结构,光催化性能最好。通过对TiO_(2)纳米管的形成机理研究发现:TiO_(2)前驱体先在强碱的作用下形成片状结构的碱金属钛盐,然后,该片状结构在表面静电作用和弹性形变等多因素诱导下转变成更稳定的纳米管状结构。 展开更多
关键词 水热法 tio2纳米管 光催化活性 形成机理
在线阅读 下载PDF
New Flexible Electrospun PET/TiO2 Composite Photoanode Layer for Dye-Sensitized Solar Cells, DSSCs, and Its Photovoltaic Performances
6
作者 Hajer Gallah Frej Mighri +3 位作者 Abdellah Ajji Jayita Bandyopadhyay Nouceir Ahmed Ben Ghorbel Judith Castillo-Rodriguez 《Materials Sciences and Applications》 2024年第11期481-503,共23页
Flexible polymer-based dye-sensitized solar cells (DSSCs) offer promising potential for lightweight, cost-effective and versatile photovoltaic applications. However, the critical challenge in their widespread applicat... Flexible polymer-based dye-sensitized solar cells (DSSCs) offer promising potential for lightweight, cost-effective and versatile photovoltaic applications. However, the critical challenge in their widespread applications is the weak thermal stability of most polymeric substrates, which can only withstand a maximum temperature processing of 150˚C. In this study, a facile and low-cost strategy is proposed to develop at low temperature DSSC flexible photoanode based on a polymeric matrix. Highly porous nanocomposites fibrous mats composed of polyethylene terephthalate (PET) and titanium dioxide (TiO2) nanobars were prepared through an electrospinning process using different configurations (uniaxial electrospinning, coaxial electrospinning, and electrospray-assisted electrospinning). These techniques enabled precise control of the microstructure and the positioning of TiO2 within the composite nanofibers. Therefore, the as-produced photoanodes were loaded with N719 dye and tested in DSSC prototype using iodide-triiodide electrolyte and platinum (Pt) coated counter electrode. The results show that incorporating TiO2 on the fiber surface through the electrospray-assisted electrospinning enhanced the performance of the nanofiber composite, leading to improved dye loading capacity, electron transfer efficiency and photovoltaic performance. 展开更多
关键词 Electrospinning ELECTROSPRAYING Coaxial Electrospinning Nanocomposites Nanofibers Flexible DSSCs PHOTOANODE tio2
在线阅读 下载PDF
One-Pot Green Synthesis of 1, 4-Dihydropyridine Derivatives Using Polyindole TiO2 Nanocatalyst by Solvent Free Method
7
作者 Deepak Babasaheb Phasage Sanjay K. Sharma +1 位作者 Balram Tripathi Sonia Chahar Srivastava 《Open Journal of Composite Materials》 2024年第3期109-123,共15页
This study used a Polyindole in combination with TiO2 nanocatalyst as an efficient heterogeneous catalyst to carry out a multi-component Hantzsch reaction involving different aromatic aldehydes with methyl acetoacetat... This study used a Polyindole in combination with TiO2 nanocatalyst as an efficient heterogeneous catalyst to carry out a multi-component Hantzsch reaction involving different aromatic aldehydes with methyl acetoacetate, and aqueous ammonium to create 1,4-dihydropyridine derivatives under solvent free condition at ambient temperature. A broad range of aldehydes and methyl acetoacetates, ranging from heteroaromatic to polyaromatic one, with high level of functional group tolerance can be used to provide the desired products possessing relevant medicinal moiety in high yields. This technology has prospective advantages over current protocols, including the utilization of a cheap, stable, recyclable, and safe catalyst, quicker reaction times with higher yields and simple product isolation. 展开更多
关键词 tio2 NANOCATALYST Green Synthesis Surface Morphology
在线阅读 下载PDF
载银纳米二氧化钛改性对木材常见菌种抑菌性能研究
8
作者 张倩 吕蕾 +2 位作者 周亚菲 时兰翠 张晔 《林业科技》 2025年第2期70-74,共5页
针对木材易受真菌侵蚀导致劣化的问题,本研究以载银纳米二氧化钛为环保型防腐剂,系统评价其对木材常见腐朽菌种黑曲霉、桔青霉、白腐菌和密粘褶菌的抑菌性能。通过牛津杯抑菌圈试验分析不同浓度改性剂的抑菌效果,结合扫描电镜和傅立叶... 针对木材易受真菌侵蚀导致劣化的问题,本研究以载银纳米二氧化钛为环保型防腐剂,系统评价其对木材常见腐朽菌种黑曲霉、桔青霉、白腐菌和密粘褶菌的抑菌性能。通过牛津杯抑菌圈试验分析不同浓度改性剂的抑菌效果,结合扫描电镜和傅立叶红外光谱表征材料特性,并探讨其抑菌机理。结果表明:载银纳米二氧化钛浓度与抑菌效果呈正相关,浓度为0.1%时综合抑菌性能最优,对密粘褶菌、白腐菌和黑曲霉的抑菌率均达85%以上,且抑菌圈直径最大(27.13 mm);0.2%浓度虽实现完全抑制,但抑菌效率趋于饱和。 展开更多
关键词 纳米二氧化钛 纳米银 木材保护 抗菌性能
在线阅读 下载PDF
Fe^3+掺杂TiO2光催化纤维材料的制备及表征 被引量:26
9
作者 苏碧桃 孙佳星 +3 位作者 胡常林 张小红 费鹏 雷自强 《物理化学学报》 SCIE CAS CSCD 北大核心 2009年第8期1561-1566,共6页
以棉花纤维为模板制备了一系列Fe3+掺杂的、具有中空纤维结构的TiO2光催化材料(Fe3+/TiO2),利用热重分析(TG)、扫描电子显微镜(SEM)、X射线衍射(XRD)、zeta电位、红外光谱(IR)和紫外-可见光谱(UV-Vis)等技术对其形貌、晶体结构及表面结... 以棉花纤维为模板制备了一系列Fe3+掺杂的、具有中空纤维结构的TiO2光催化材料(Fe3+/TiO2),利用热重分析(TG)、扫描电子显微镜(SEM)、X射线衍射(XRD)、zeta电位、红外光谱(IR)和紫外-可见光谱(UV-Vis)等技术对其形貌、晶体结构及表面结构、光吸收特性等进行了表征.以亚甲基蓝(MB)溶液的脱色降解为模型反应,考察了不同Fe3+掺杂量的样品在太阳光下的光催化性能.结果表明,用模板法制备的Fe3+/TiO2中空纤维结构材料表面存在大量纳米微粒(平均尺寸约12nm);Fe3+可能均匀分散于锐钛矿结构的TiO2中,部分取代Ti4+的晶格位置,既拓宽了TiO2的光谱响应范围,又形成了TiO2晶体结构的缺陷,使其表面带负电荷.在太阳光条件下,该纤维结构材料较纯TiO2对MB溶液具有更好的光催化脱色降解效果,且Fe3+的掺入量显著影响该纤维材料的催化性能;当Fe3+掺杂量为0.15%(w),在500℃焙烧2h所得中空纤维材料的催化性能最好,2h即可使MB溶液的脱色降解率达93%;重复使用5次仍可使MB溶液的脱色降解率保持在90%以上,且该催化剂材料易于离心分离去除.因此,以该模板合成法,通过Fe3+的掺杂有望使TiO2成为一种低或无能耗、高活性的绿色环保型催化材料. 展开更多
关键词 光催化 tio2 Fe3+掺杂 棉花纤维 模板法 制备 表征
在线阅读 下载PDF
温湿度和光强对水泥基材料负载纳米TiO2光催化氧化氮氧化物的影响 被引量:40
10
作者 钱春香 赵联芳 +2 位作者 付大放 李丽 王瑞兴 《环境科学学报》 CAS CSCD 北大核心 2005年第5期623-630,共8页
研究了路面水泥基材料负载纳米TiO2 光催化氧化汽车尾气中氮氧化物过程中湿度、温度和光强对催化反应的影响.试验和分析结果表明,光催化氧化效率随湿度增加而急剧下降;当NO2 浓度较低时,光辐照强度对光催化氧化效率的影响不显著;NO2 浓... 研究了路面水泥基材料负载纳米TiO2 光催化氧化汽车尾气中氮氧化物过程中湿度、温度和光强对催化反应的影响.试验和分析结果表明,光催化氧化效率随湿度增加而急剧下降;当NO2 浓度较低时,光辐照强度对光催化氧化效率的影响不显著;NO2 浓度较高时,随着光辐照强度的增强,光催化氧化效率呈现出上升趋势,在太阳光的照射下或在室内较弱紫外光照射下都具有良好的光催化氧化作用.在0~2 5℃的温度范围内,光催化氧化效率随温度升高而提高,而在2 展开更多
关键词 温度 湿度 光强 水泥基材料 纳米tio2 光催化 NO2
在线阅读 下载PDF
石墨烯/纳米TiO2复合材料的制备及其光催化性能 被引量:44
11
作者 周琪 钟永辉 +3 位作者 陈星 王岩 刘平 吴玉程 《复合材料学报》 EI CAS CSCD 北大核心 2014年第2期255-262,共8页
以氧化石墨烯(GO)和钛酸四丁酯(Ti(OBu)4)作为初始反应物,采用乙醇溶剂热法合成了石墨烯/纳米TiO2复合材料,并利用XRD、FE-SEM、TEM、RAMAN和XPS等手段对石墨烯/纳米TiO2复合材料的晶体结构、形貌及元素形态等性质进行了表征,同时将复... 以氧化石墨烯(GO)和钛酸四丁酯(Ti(OBu)4)作为初始反应物,采用乙醇溶剂热法合成了石墨烯/纳米TiO2复合材料,并利用XRD、FE-SEM、TEM、RAMAN和XPS等手段对石墨烯/纳米TiO2复合材料的晶体结构、形貌及元素形态等性质进行了表征,同时将复合材料应用于光催化降解甲基橙溶液,进行光催化性能评价。结果表明:Ti(OBu)4在乙醇溶剂中通过化学静电引力吸附到GO表面,经过溶剂热反应,GO被还原成石墨烯的同时,石墨烯的表面负载生长锐钛矿TiO2颗粒。随着溶剂热反应时间的延长,GO表面的活性基团减少,还原更加彻底,同时TiO2晶粒有一定的增大趋势;与纯TiO2相比,石墨烯/纳米TiO2复合材料光催化活性明显提高,石墨烯含量对复合材料的光催化活性有直接的影响。 展开更多
关键词 tio2 石墨烯 溶剂热法 复合材料 光催化
原文传递
V2O5-WO3/TiO2烟气脱硝催化剂的载体选择 被引量:49
12
作者 朱崇兵 金保升 +2 位作者 仲兆平 李锋 翟俊霞 《中国电机工程学报》 EI CSCD 北大核心 2008年第11期41-47,共7页
在选择性催化还原试验台上对4种不同TiO2为载体制备的催化剂的脱硝性能进行测试,采用BET、X射线衍射、傅里叶转换红外光谱、扫描电镜-能谱分析、X射线荧光分析和热重分析等技术进行微观表征,并与商业催化剂进行对比。以硫酸法制备的纳... 在选择性催化还原试验台上对4种不同TiO2为载体制备的催化剂的脱硝性能进行测试,采用BET、X射线衍射、傅里叶转换红外光谱、扫描电镜-能谱分析、X射线荧光分析和热重分析等技术进行微观表征,并与商业催化剂进行对比。以硫酸法制备的纳米级锐钛型TiO2适合作为选择性催化还原催化剂载体,制备的催化剂脱硝效率高,温度窗口宽,选择性好,其中硫酸盐质量分数为8%~10%时最为有利;以氯化法制备纳米TiO2过程中,生成了V3Ti6O17的聚合物导致NO脱除率较低,因此不适合作为催化剂载体。以工业级TiO2为载体制备的催化剂氨氮比为1.0时,在355~420℃的温度范围内NO脱除率为80%~85%,但由于成本很低,因此可以用于脱硝要求不高的场合。由钛酸丁酯溶胶法制备TiO2为载体制备的SCR催化剂性能不及硫酸法制备的纳米级锐钛型TiO2制备的催化剂,且操作复杂,技术难度大,不适宜推广。 展开更多
关键词 V2O5-WO3/tio2 催化剂载体 选择性催化还原 烟气脱硝 纳米级锐钛型tio2
在线阅读 下载PDF
稀土金属掺杂对锐钛矿型TiO2光催化活性影响的理论和实验研究 被引量:43
13
作者 刘月 余林 +3 位作者 魏志钢 潘湛昌 邹燕娣 谢英豪 《高等学校化学学报》 SCIE EI CAS CSCD 北大核心 2013年第2期434-440,共7页
从理论和实验两方面探讨稀土金属掺杂对锐钛矿型TiO2光催化活性的影响.理论上采用基于密度泛函理论(DFT)的第一性原理,对稀土掺杂TiO2前后的几何结构、能带结构、态密度及电子结构进行了系统的研究.结果表明,Y,La,Gd,Lu,Ce,Eu,Yb和Tb掺... 从理论和实验两方面探讨稀土金属掺杂对锐钛矿型TiO2光催化活性的影响.理论上采用基于密度泛函理论(DFT)的第一性原理,对稀土掺杂TiO2前后的几何结构、能带结构、态密度及电子结构进行了系统的研究.结果表明,Y,La,Gd,Lu,Ce,Eu,Yb和Tb掺杂有助于TiO2光催化活性的提高;而对于Pr,Nd,Pm,Sm,Dy,Ho,Er和Tm掺杂,由于在价带顶和导带底之间形成了较多的可能成为光生电子和空穴的复合中心的杂质能级,故此类稀土的掺杂浓度需要控制在较小的范围内.另一方面,采用溶胶-凝胶法制备了9种稀土金属(RE=Y,Ce,Pr,Sm,Gd,Dy,Ho,Er,Yb)掺杂的TiO2粉体,运用X射线衍射(XRD)和紫外-可见光谱法(UV-Vis)分别表征其晶体结构和光学吸收性质.结果表明,掺杂前后的TiO2均为锐钛矿相,且Ho,Pr,Ce,Sm,Y,Yb和Gd掺杂使TiO2在可见光区的吸收有不同程度的提高.理论预测与实验结果基本一致,且理论研究结果与周期表中稀土元素外层电子轨道排布规律一致,从而揭示了稀土元素掺杂的本质规律,指明了适量的稀土掺杂有利于TiO2光催化活性的提高. 展开更多
关键词 稀土掺杂tio2 锐钛矿相 密度泛函理论 能带结构
在线阅读 下载PDF
Au掺杂方式对锐钛矿TiO2光催化性能的影响 被引量:19
14
作者 卢晗锋 周瑛 +2 位作者 徐柏庆 陈银飞 刘化章 《物理化学学报》 SCIE CAS CSCD 北大核心 2008年第3期459-464,共6页
结合超临界乙醇干燥技术,采用沉积-沉淀(DP)和共沉淀(CP)法分别制备了具有单一锐钛矿晶相的Au/TiO2和Au(0.2%,原子分数)-TiO2光催化剂,通过XRD、BET、TEM、XPS和Raman手段表征样品中Au的掺杂形态,以光催化降解甲基橙为模型反应考察了样... 结合超临界乙醇干燥技术,采用沉积-沉淀(DP)和共沉淀(CP)法分别制备了具有单一锐钛矿晶相的Au/TiO2和Au(0.2%,原子分数)-TiO2光催化剂,通过XRD、BET、TEM、XPS和Raman手段表征样品中Au的掺杂形态,以光催化降解甲基橙为模型反应考察了样品的光催化活性.结果表明,DP法制备的Au/TiO2在110℃干燥处理后,表面存在的Au3+能有效地促进锐钛矿TiO2光催化性能,其一级反应速率常数比纯锐钛矿TiO2提高了3.2倍,比商用光催化剂Degussa-P25提高了4.1倍,而当Au3+被还原为Au0后光催化活性下降.用CP法制备的Au-TiO2并没有较大地提高锐钛矿TiO2光催化性能,在焙烧温度达到800℃时,Au向表面迁移聚集,造成锐钛矿TiO2晶格氧空位和缺陷位增加,使光催化活性下降. 展开更多
关键词 掺杂 氧化态 锐钛矿tio2 甲基橙 光催化
在线阅读 下载PDF
K2O对V2O5-WO3/TiO2催化剂的中毒作用 被引量:32
15
作者 朱崇兵 金保升 +3 位作者 仲兆平 李锋 陈玲霞 翟俊霞 《东南大学学报(自然科学版)》 EI CAS CSCD 北大核心 2008年第1期101-105,共5页
实验室制备了V2O5-WO3/TiO2的脱硝催化剂,采用模拟中毒法,在此催化剂上负载碱金属氧化物K2O,通过BET,XRD,SEM等方法对微观结构进行表征.在SCR活性试验台上研究不同含量K2O对催化剂脱硝活性,N2O生成率和SO2氧化率的影响.结果发现:K2O对... 实验室制备了V2O5-WO3/TiO2的脱硝催化剂,采用模拟中毒法,在此催化剂上负载碱金属氧化物K2O,通过BET,XRD,SEM等方法对微观结构进行表征.在SCR活性试验台上研究不同含量K2O对催化剂脱硝活性,N2O生成率和SO2氧化率的影响.结果发现:K2O对于催化剂的毒性较强,随着添加量的增大,NO脱除率急剧下降,SO2的氧化率大大提高;较大含量的K2O(nK/nV=1,摩尔比)使催化剂比表面积有所减少,催化剂颗粒发生轻微团聚,微观结构变化不大,但NO的脱除率小于50%(380℃),N2O的生成率和SO2的氧化率均增加;K2O通过与V2O5的活性酸性位结合,使催化剂中有效活性位数量大为降低,导致脱硝活性下降. 展开更多
关键词 中毒 K2O V2O5-WO3/tio2催化剂 SCR 脱硝
在线阅读 下载PDF
高分散TiO2/SBA-15的制备及光催化性能 被引量:24
16
作者 张书翠 姜东 +2 位作者 唐涛 李君华 徐耀 《物理化学学报》 SCIE CAS CSCD 北大核心 2010年第5期1330-1336,共7页
提出了一种制备高分散TiO2/SBA-15光催化剂的新方法.以钛酸四正丁酯(TB)和羧基改性的SBA-15(COOH/SBA-15)为原料,利用COOH/SBA-15表面上高分散的羧基与TB的配合作用将TB锚定,经过溶剂热及焙烧处理制得TiO2/SBA-15光催化剂.采用粉末X射... 提出了一种制备高分散TiO2/SBA-15光催化剂的新方法.以钛酸四正丁酯(TB)和羧基改性的SBA-15(COOH/SBA-15)为原料,利用COOH/SBA-15表面上高分散的羧基与TB的配合作用将TB锚定,经过溶剂热及焙烧处理制得TiO2/SBA-15光催化剂.采用粉末X射线衍射(XRD),N2吸脱附,傅里叶变换红外光谱(FT-IR),透射电镜(TEM)等对所得催化剂进行了表征.结果表明:所得TiO2/SBA-15光催化剂为高结晶度的锐钛矿晶型,TiO2均匀地分散在SBA-15表面,TiO2/SBA-15光催化剂保持较好的介孔特征结构,具有较大比表面积.以降解罗丹明B(RhB)为探针反应,考察了所得TiO2/SBA-15光催化剂的光催化性能.与后处理浸渍法制备的光催化剂相比,本文制备的TiO2/SBA-15光催化剂表现出了更加优越的光催化性能. 展开更多
关键词 光催化 羧基改性 tio2 SBA-15 溶剂热
在线阅读 下载PDF
纳米TiO2/聚乳酸复合材料的制备和表征 被引量:26
17
作者 庄韦 张建华 +3 位作者 刘靖 张强 胡柏星 沈健 《复合材料学报》 EI CAS CSCD 北大核心 2008年第3期8-11,共4页
采用原位聚合的方法制备了有机化处理过的纳米TiO2粒子质量分数分别为1 wt%、3 wt%、5 wt%和10 wt%的4种纳米TiO2/聚乳酸复合材料。SEM结果表明,当纳米TiO2粒子质量分数较低时,纳米TiO2在聚乳酸基体中呈现均匀稳定分散,而质量分数较高... 采用原位聚合的方法制备了有机化处理过的纳米TiO2粒子质量分数分别为1 wt%、3 wt%、5 wt%和10 wt%的4种纳米TiO2/聚乳酸复合材料。SEM结果表明,当纳米TiO2粒子质量分数较低时,纳米TiO2在聚乳酸基体中呈现均匀稳定分散,而质量分数较高时则发生团聚。通过力学和热学等性能测试发现复合材料的最大热分解温度、玻璃化转变温度和力学性能相对于聚乳酸有较大幅度提高,其中纳米TiO2的质量分数为3 wt%时改善效果最明显,其最大热分解温度、玻璃化转变温度分别比聚乳酸提高了25.3℃和4.9℃,拉伸强度、断裂伸长率和弹性模量分别提高了83.6%、6.73%和129.4%。 展开更多
关键词 聚乳酸 纳米tio2 复合材料 原位聚合
在线阅读 下载PDF
溶剂热法制备TiO2/g-C3N4及其光催化性能 被引量:18
18
作者 董海军 陈爱平 +2 位作者 何洪波 吕慧 李春忠 《华东理工大学学报(自然科学版)》 CAS CSCD 北大核心 2013年第5期536-541,共6页
采用溶剂热法合成了可见光响应的TiO_2/g-C_3N_4复合光催化剂,并对TiO_2/g-C_3N_4进行质子化处理。通过X射线衍射(XRD)、氮气吸附-脱附BET法、扫描电子显微镜(SEM)、透射电子显微镜(TEM)、傅里叶红外光谱(FT-IR)、紫外-可见漫反射(UV-vi... 采用溶剂热法合成了可见光响应的TiO_2/g-C_3N_4复合光催化剂,并对TiO_2/g-C_3N_4进行质子化处理。通过X射线衍射(XRD)、氮气吸附-脱附BET法、扫描电子显微镜(SEM)、透射电子显微镜(TEM)、傅里叶红外光谱(FT-IR)、紫外-可见漫反射(UV-vis DRS)和荧光光谱(PL)等方法对样品进行了表征,并以甲基橙(MO)光催化降解为模型反应,考察了可见光下制备的样品的光催化性能。结果表明,多孔TiO_2纳米晶与g-C_3N_4形成具有"芝麻饼"形貌的复合结构;TiO_2/g-C_3N_4复合光催化剂的光吸收带边扩展到465 nm,较TiO_2出现明显红移;TiO_2与g-C_3N_4能带匹配耦合,有效地抑制了电子与空穴的复合;质子化处理过程能够提高可见光区吸收强度和电子的传导能力,增强了TiO_2的光催化活性。 展开更多
关键词 tio2纳米晶 tio2 g—C3N4 g-C3N4 可见光响应 质子化处理 光催化
在线阅读 下载PDF
粒径可控球形TiO2的制备 被引量:17
19
作者 扈玫珑 白晨光 +2 位作者 徐盛明 徐刚 梁栋 《物理化学学报》 SCIE CAS CSCD 北大核心 2008年第12期2287-2292,共6页
在正丙醇与水的混合溶剂体系中以Ti(SO4)2为前驱物制备得到了粒径分布窄,分散性好的球形TiO2.对表面活性剂种类及用量,反应物浓度及焙烧温度和时间等影响因素进行了研究,结果表明,在正丙醇与水的体积比为1∶1的条件下,以聚乙烯吡咯烷酮(... 在正丙醇与水的混合溶剂体系中以Ti(SO4)2为前驱物制备得到了粒径分布窄,分散性好的球形TiO2.对表面活性剂种类及用量,反应物浓度及焙烧温度和时间等影响因素进行了研究,结果表明,在正丙醇与水的体积比为1∶1的条件下,以聚乙烯吡咯烷酮(PVP)为表面活性剂,温度为70-90℃时可制得粒径分布窄、分散性好的高质量的球形TiO2颗粒.通过TG-DSC、SEM、XRD等分析表明,颗粒粒度大小及粒径分布受表面活性剂浓度和反应前驱物浓度影响大;物相间的转化主要由焙烧温度和时间来决定.并引入LaMer模型对颗粒形核、长大的过程进行理论说明. 展开更多
关键词 球形tio2 粒径分布 分散性 物相转化 LaMer模型
在线阅读 下载PDF
有序介孔材料H6P2W18O62/TiO2(Brij-76)的制备与微波增强光催化降解一氯苯 被引量:23
20
作者 李莉 马禹 +2 位作者 曹艳珍 计远 郭伊荇 《物理化学学报》 SCIE CAS CSCD 北大核心 2009年第7期1461-1466,共6页
采用非离子表面活性剂C18H37(OCH2CH2)10OH(Brij-76)作为模板剂,在以杂多酸H6P2W18O62对TiO2掺杂改性基础上,通过模板-溶胶-凝胶-程序升温溶剂热一步法在较低温度下制备了有序复合介孔材料H6P2W18O62/TiO2(Brij-76).通过傅立叶变换红外(... 采用非离子表面活性剂C18H37(OCH2CH2)10OH(Brij-76)作为模板剂,在以杂多酸H6P2W18O62对TiO2掺杂改性基础上,通过模板-溶胶-凝胶-程序升温溶剂热一步法在较低温度下制备了有序复合介孔材料H6P2W18O62/TiO2(Brij-76).通过傅立叶变换红外(FT-IR)光谱,X射线衍射(XRD),扫描电子显微镜(SEM),能量色散X射线(EDX),N2吸附-脱附测定和NH3程序升温脱附(NH3-TPD)等手段对其进行了表征.结果表明,以非离子表面活性剂Brij-76为模板剂制得的复合材料H6P2W18O62/TiO2(Brij-76)平均孔径约为3.31nm,BET比表面积为99.78m2·g-1.与TiO2相比,其孔径有序性大幅度提高,粒子的聚集度降低,表面酸性显著增加.微波增强光催化性能研究结果显示,H6P2W18O62/TiO2(Brij-76)在微波作用下催化活性更高,可有效地降解一氯苯溶液. 展开更多
关键词 光催化 H6P2W18O62/tio2 C18H37(OCH2CH2)10OH 溶胶-凝胶法 微波 一氯苯
在线阅读 下载PDF