期刊文献+
共找到3篇文章
< 1 >
每页显示 20 50 100
Experimental investigations on wear properties of Palm kernel reinforced composites for brake pad applications
1
作者 Satish Pujari S.Srikiran 《Defence Technology(防务技术)》 SCIE EI CAS CSCD 2019年第3期295-299,共5页
The use of asbestos material is being avoided to manufacture the brake pads as it is harmful and toxic in nature. Further it leads to various health issues like asbestosis, mesothelioma and lung cancers. These brake p... The use of asbestos material is being avoided to manufacture the brake pads as it is harmful and toxic in nature. Further it leads to various health issues like asbestosis, mesothelioma and lung cancers. These brake pads can be replaced by natural fibers like Palm kernel (0-50%), Nile roses (0-15%) and Wheat (0-10%) with additives like aluminum oxide (5%-20%) and graphite powder (10%-35%). Phenolic resin of 35% is utilized as a binder. Particulated Nile roses are used to increase the friction coefficient and wheat powder is used to reduce the wear rate. Aluminum oxide and graphite are abrasive in nature. This helps to make brake pads with high friction co-efficient and less wear rate with low noise pollution. The wear of the proposed composites have been investigated at different speeds. Various tests like wear on pin-ondisc apparatus, hardness on the Rockwell hardness apparatus and oil absorption test have been conducted. Phenolic resin produces good bonding nature to fiber. Thus, Fibers found to have performed palatably among all commercial brake pads. The objective of the research indicates that Palm kernal shell could be a conceivable alternative for asbestos in friction coating materials. 展开更多
关键词 Friction materials palm kernel fiber NILE ROSE Wheat Brake pad WEAR TEST Hardness TEST Oil absorption TEST
在线阅读 下载PDF
酶法结合化学改性对油棕粕膳食纤维理化性质与降血糖活性的影响
2
作者 王楠 宋昕凌 +4 位作者 马彪 刘心语 张怡萱 郑亚军 王浩 《食品工业科技》 北大核心 2026年第5期43-50,共8页
本文探究酶法结合羧甲基化或乙酰化改性对油棕粕膳食纤维的化学组成、结构、理化性质与降血糖活性的影响。结果表明,两种复合改性均使油棕粕膳食纤维的微观结构变得疏松多孔;FT-IR光谱证实化学改性成功引入了羧甲基和乙酰基,且3400 cm-... 本文探究酶法结合羧甲基化或乙酰化改性对油棕粕膳食纤维的化学组成、结构、理化性质与降血糖活性的影响。结果表明,两种复合改性均使油棕粕膳食纤维的微观结构变得疏松多孔;FT-IR光谱证实化学改性成功引入了羧甲基和乙酰基,且3400 cm-1附近吸收峰的伸缩振动说明复合改性破坏了纤维中的氢键。经酶法结合羧甲基改性和酶法结合乙酰化改性处理后,油棕粕纤维的可溶性膳食纤维含量从4.00%显著增至16.14%和12.85%(P<0.05);持水力从2.06 g/g分别增至5.72 g/g和4.15 g/g;膨胀力从1.01 mL/g分别增至3.58 mL/g和2.46 mL/g;黏度从4.08 cP分别增至13.90 cP和7.71 cP;葡萄糖吸附能力从1.84μmol/g分别增至3.99μmol/g和4.53μmol/g;葡萄糖扩散抑制能力从16.32%分别增至38.18%和25.15%。此外,经酶法结合羧甲基处理的纤维,其α-淀粉酶抑制活性(19.41%)较未改性纤维提升了0.43倍,而酶法结合乙酰化处理的纤维该活性并未得到提高。综上所述,酶法结合羧甲基或乙酰化均可一定程度增强油棕粕膳食纤维的理化性质与降血糖活性,其中酶法结合羧甲基改性的效果最优,这有助于扩大其在食品工业生产中的应用。 展开更多
关键词 油棕粕膳食纤维 酶法改性 羧甲基化 乙酰化 理化性质 降血糖活性
在线阅读 下载PDF
利用棕榈丝纤维和棕榈仁粕栽培茶树菇配方试验 被引量:1
3
作者 陈新淇 刘叶高 《园艺与种苗》 CAS 2024年第1期26-27,39,共3页
[目的]研究能提高茶树菇产量的配方,丰富栽培茶树菇的原辅材料。[方法]利用棕榈丝纤维和棕榈仁粕混合配方栽培茶树菇,设3个不同配比,并以杂木屑配方作为对照,对比4个配方间产量的差异。[结果]棕榈丝纤维和棕榈仁粕可以显著提高茶树菇的... [目的]研究能提高茶树菇产量的配方,丰富栽培茶树菇的原辅材料。[方法]利用棕榈丝纤维和棕榈仁粕混合配方栽培茶树菇,设3个不同配比,并以杂木屑配方作为对照,对比4个配方间产量的差异。[结果]棕榈丝纤维和棕榈仁粕可以显著提高茶树菇的产量,其中添加棕榈配方的茶树菇平均单袋产量可达277.7 g,比杂木屑配方的产量(178.9 g)提高了55.2%左右。但是菌丝的生长速度随着加入棕榈原材料量的增加而减缓,特别是棕榈仁粕,当其量达一定值时,茶树菇菌丝生长缓慢甚至无法满袋,且无法正常出菇。[结论]在实际生产中,可在杂木屑配方中适当添加棕榈丝纤维或者棕榈仁粕,以提高茶树菇产量。 展开更多
关键词 茶树菇 棕榈丝纤维 棕榈仁粕 杂木屑 生物学效率
在线阅读 下载PDF
上一页 1 下一页 到第