RESEARCH ON CYLINDRICAL BOX TYPE WINDOWS USED TO TRANSMIT HIGH POWER CW 被引量:1
1
作者 LinFumin DingYaogen +1 位作者 ShenBin XuShouxi 《Journal of Electronics(China)》 2004年第5期392-400,共9页
The formula for calculating the threshold of average transmitting power of cylindrical TE11 mode window is revised by accurate deduction and a practical method for calculating the temperature increment of the dielectr... The formula for calculating the threshold of average transmitting power of cylindrical TE11 mode window is revised by accurate deduction and a practical method for calculating the temperature increment of the dielectric disk in cylindrical box type window is given. Meanwhile,a typical cylindrical box type window is calculated and used as an example to discuss the power capacity, the special harmfulness and elimination of ghost mode resonance when the window is used to transmit high power Continuous Wave(CW). 展开更多
关键词 High power Continuous Wave(CW) microwave window Dielectric disk in window RF loss Power capacity Ghost mode
在线阅读 下载PDF
Interfacial Structure and Mechanical Properties of Diamond/Copper Joint Brazed by Ag-Cu-In-Ti Low-Temperature Brazing Filler 被引量:2
2
作者 Pan Yufan Liang Jiabin +10 位作者 Nie Jialong Liu Xin Sun Huawei Chang Yunfeng Li Huaxin Lu Chuanyang Xu Dong Wang Xingxing Yang Yang Yang Jianguo He Yanming 《稀有金属材料与工程》 北大核心 2025年第2期301-310,共10页
Ag-Cu-In-Ti low-temperature filler was used to braze the diamond and copper,and the effects of brazing temperature and soaking time on the microstructure and mechanical properties of the joints were investigated.In ad... Ag-Cu-In-Ti low-temperature filler was used to braze the diamond and copper,and the effects of brazing temperature and soaking time on the microstructure and mechanical properties of the joints were investigated.In addition,the joint formation mechanism was discussed,and the correlation between joint microstructure and mechanical performance was established.Results show that adding appropriate amount of In into the filler can significantly reduce the filler melting point and enhance the wettability of filler on diamond.When the brazing temperature is 750°C and the soaking time is 10 min,a uniformly dense braze seam with excellent metallurgical bonding can be obtained,and its average joint shear strength reaches 322 MPa.The lower brazing temperature can mitigate the risk of diamond graphitization and also reduce the residual stresses during joining. 展开更多
关键词 diamond microwave window vacuum brazing Ag-Cu-In-Ti microstructure mechanical properties