The practical application of the lithium anode in lithium metal batteries(LMBs) has been hindered by the uncontrollable growth of lithium dendrite and the high volumetric change during cycling. Herein, the in situ for...The practical application of the lithium anode in lithium metal batteries(LMBs) has been hindered by the uncontrollable growth of lithium dendrite and the high volumetric change during cycling. Herein, the in situ formed three-dimensional(3D) lithium-boron(Li-B) alloy is suggested as an excellent alternative to the Li metal, in which the 3D Li B skeleton can mitigate the growth of Li dendrites and volumetric change. In this study, the Li-B alloy anodes with different B contents were manufactured by high-temperature melting. It was found that the boron content had a significant effect on the electrochemical performance of the Li-B alloy. The Li-B alloy with the least B content(10 wt%, 10LiB) demonstrated the lowest overpotential of 0.0852 V after 300 h and the lowest interface resistance. However, the full cell with 15LiB as the anode displayed the best cycling performance of 115 m Ah·g^(-1) after 100 cycles with a columbic efficiency greater than 97%. The obtained results suggest that the in situ formed three-dimensional Li-B alloy anode can be an excellent alternative to the Li anode via tuning B contents for next-generation high energy density LMBs.展开更多
A Li-B alloy has been prepared using a pretreated amorphous B powder and pure Li ingot as starting materials by continually slow addition of B powder and intensified stirring in the process of melting. The microstruct...A Li-B alloy has been prepared using a pretreated amorphous B powder and pure Li ingot as starting materials by continually slow addition of B powder and intensified stirring in the process of melting. The microstructure and the discharge characteristic of the materials have been investigated- Results show that the problem of temperature control in synthesis would be modified by means of continual addition of B powder, the Li7B6 would be more finely distributed in the metal Li by means of intensified stirring. The discharge characteristic of the Li-B alloy using amorphous B as starting materials is almost the same with that of using crystalline B.展开更多
Li-B alloy is expected to meet the expanding demands of energy storage,primarily driven by their high energydensity and structural stability.The fibrous porous skeleton can increase the electrochemical active area and...Li-B alloy is expected to meet the expanding demands of energy storage,primarily driven by their high energydensity and structural stability.The fibrous porous skeleton can increase the electrochemical active area and reduce thelocal current density,therefore diminishing the lithium dendrites.In this study,we prepared Li-B alloys with differentlithium contents and examined the impact of lithium content on the structure and electrochemical properties of Li-Balloys.With the increase of lithium content,the spacing between the skeleton of the Li-B alloys increases.The lithiumdeposition on the top of the skeleton decreases,leading to thinner SEI,and lower polarization.The Li-B alloy with thehighest lithium content(64 wt.%lithium content)in the symmetric battery exhibits the longest cycle time,lasting over140 h at 1 mA/cm^(2)and 0.5 mA·h/cm^(2),with a minimal overpotential of 0.08 V.When paired with LiNi_(0.5)Co_(0.2)Mn_(0.3)O_(2),thefull battery has the highest specific discharge capacity and the best rate capacity.展开更多
基金financially supported by the National Natural Science Foundation of China (Nos. U1904216 and51771236)the Science Fund for Distinguished Young Scholars of Hunan Province (No. 2018JJ1038)+1 种基金the Innovation-Driven Project of Central South University (No. 2020CX007)the State Key Laboratory of Powder Metallurgy, Central South University。
文摘The practical application of the lithium anode in lithium metal batteries(LMBs) has been hindered by the uncontrollable growth of lithium dendrite and the high volumetric change during cycling. Herein, the in situ formed three-dimensional(3D) lithium-boron(Li-B) alloy is suggested as an excellent alternative to the Li metal, in which the 3D Li B skeleton can mitigate the growth of Li dendrites and volumetric change. In this study, the Li-B alloy anodes with different B contents were manufactured by high-temperature melting. It was found that the boron content had a significant effect on the electrochemical performance of the Li-B alloy. The Li-B alloy with the least B content(10 wt%, 10LiB) demonstrated the lowest overpotential of 0.0852 V after 300 h and the lowest interface resistance. However, the full cell with 15LiB as the anode displayed the best cycling performance of 115 m Ah·g^(-1) after 100 cycles with a columbic efficiency greater than 97%. The obtained results suggest that the in situ formed three-dimensional Li-B alloy anode can be an excellent alternative to the Li anode via tuning B contents for next-generation high energy density LMBs.
基金State Ministry of Education Under contract No. 96053311.
文摘A Li-B alloy has been prepared using a pretreated amorphous B powder and pure Li ingot as starting materials by continually slow addition of B powder and intensified stirring in the process of melting. The microstructure and the discharge characteristic of the materials have been investigated- Results show that the problem of temperature control in synthesis would be modified by means of continual addition of B powder, the Li7B6 would be more finely distributed in the metal Li by means of intensified stirring. The discharge characteristic of the Li-B alloy using amorphous B as starting materials is almost the same with that of using crystalline B.
基金Project(2022JJ40591)supported by the Natural Science Foundation of Hunan Province,ChinaProject(kq2202094)supported by the Natural Science Foundation of Changsha,China。
文摘Li-B alloy is expected to meet the expanding demands of energy storage,primarily driven by their high energydensity and structural stability.The fibrous porous skeleton can increase the electrochemical active area and reduce thelocal current density,therefore diminishing the lithium dendrites.In this study,we prepared Li-B alloys with differentlithium contents and examined the impact of lithium content on the structure and electrochemical properties of Li-Balloys.With the increase of lithium content,the spacing between the skeleton of the Li-B alloys increases.The lithiumdeposition on the top of the skeleton decreases,leading to thinner SEI,and lower polarization.The Li-B alloy with thehighest lithium content(64 wt.%lithium content)in the symmetric battery exhibits the longest cycle time,lasting over140 h at 1 mA/cm^(2)and 0.5 mA·h/cm^(2),with a minimal overpotential of 0.08 V.When paired with LiNi_(0.5)Co_(0.2)Mn_(0.3)O_(2),thefull battery has the highest specific discharge capacity and the best rate capacity.