每页显示 20 50 100
Preparation of a Fe_(3)O_(4)@SiO_(2)@Fe-MIL-101 for the Adsorption Removal of Fluoride in Zinc Sulfate Electrolyte
1
作者 LIAO Jia WANG Chunmei +4 位作者 LI Fei YANG Chengcheng GUO Xianyu TAN Wentao LI Hui 《吉首大学学报(自然科学版)》 2025年第3期46-61,共16页
To remove the fluoride in zinc sulfate electrolyte to an appropriate level,mitigate environmental fluoride pollution,and drive the development of the hydrometallurgy industry of zinc,a novel Fe_(3)O_(4)@SiO_(2)@Fe-MIL... To remove the fluoride in zinc sulfate electrolyte to an appropriate level,mitigate environmental fluoride pollution,and drive the development of the hydrometallurgy industry of zinc,a novel Fe_(3)O_(4)@SiO_(2)@Fe-MIL-101 magnetic composite material was successfully synthesized via the one-pot method.Preparation conditions were optimized and structural characterization of this material conducted using FTIR,SEM,EDS,XRD and Hysteresis analysis.The results show that this composite exhibits a more rapid fluoride adsorption dynamics and a higher fluoride adsorption capacity(18.34 mg/g)and its adsorption behavior fitted for the first order dynamic model and the Freundlich isotherm model.The adsorption of fluorine by this composite is mainly physical adsorption according to the mean adsorption energy(1.216 kJ/mol).The interfering ions co-existed in fluoride-containing solutions,like HCO_(3)^(-),NO^(-)and Cl^(-),have a significant effect on fluorine adsorption.This composite has also been proved with magnetism,higher adsorption selectivity and satisfactory reusability.When this composite is employed as an adsorbent for adsorption removing fluoride in zinc sulfate electrolyte,it exhibits higher pH-dependent behavior as well as high fluoride removal efficiency at pH 6.5. 展开更多
关键词 fe_(3)o_(4)@Sio_(2)@fe-MIL-101 composite FLUoRIDE REMoVAL ADSoRPTIoN zinc sulfate electrolyte
在线阅读 下载PDF
Fe/Mg改性γ-Al_(2)O_(3)复合吸附剂硒吸附性能研究
2
作者 谷梦瑶 郭士豪 +3 位作者 樊昊天 刘皓 陈娟 姚洪 《燃烧科学与技术》 北大核心 2025年第4期435-442,共8页
通过浸渍法制备不同摩尔比的Fe/γ-Al_(2)O_(3)复合吸附剂及Mg/Al/Fe三元复合吸附剂,并在固定床上进行硒吸附实验.探讨400~700℃下Fe/γ-Al_(2)O_(3)吸附剂的吸附性能及H_(2)O浓度对两种吸附剂硒吸附特性的影响.结果表明,在500℃、8%H_(... 通过浸渍法制备不同摩尔比的Fe/γ-Al_(2)O_(3)复合吸附剂及Mg/Al/Fe三元复合吸附剂,并在固定床上进行硒吸附实验.探讨400~700℃下Fe/γ-Al_(2)O_(3)吸附剂的吸附性能及H_(2)O浓度对两种吸附剂硒吸附特性的影响.结果表明,在500℃、8%H_(2)O条件下,Fe/Al摩尔比为1∶10的吸附剂表现出最佳硒吸附性能,吸附量为10.968 mg/g,而Mg/Al/Fe吸附剂在20%H_(2)O条件下硒吸附性能最佳,吸附量为9.7606 mg/g.XPS结果显示,烟气中的SeO2与Mg/Al/Fe吸附剂表面的晶格氧结合,提高吸附剂表面的氧缺陷,从而改善吸附性能. 展开更多
关键词 fe/γ-Al_(2)o_(3)复合吸附剂 吸附性能 H_(2)o
在线阅读 下载PDF
磁靶向纳米Fe_3O_4-TiO_2复合物的制备及其对肝癌细胞的光催化杀伤效应 被引量:6
3
作者 文雯 高晓亚 +4 位作者 宋志英 韩冬 王娟 朱美霞 张爱平 《物理化学学报》 SCIE CAS CSCD 北大核心 2012年第9期2221-2230,共10页
采用三种低温溶胶-凝胶法制备了具有不同Fe3O4掺杂量的磁靶向纳米Fe3O4-TiO2复合物,通过X射线衍射(XRD)、透射电镜(TEM)、傅里叶变换红外(FTIR)光谱、紫外-可见(UV-Vis)光谱、荧光光谱(FS)及磁性能分析等表征方法筛选出包覆均匀、分散... 采用三种低温溶胶-凝胶法制备了具有不同Fe3O4掺杂量的磁靶向纳米Fe3O4-TiO2复合物,通过X射线衍射(XRD)、透射电镜(TEM)、傅里叶变换红外(FTIR)光谱、紫外-可见(UV-Vis)光谱、荧光光谱(FS)及磁性能分析等表征方法筛选出包覆均匀、分散性好、磁性能优异及光催化活性较高的纳米Fe3O4-TiO2复合物.以四甲基偶氮唑蓝(MTT)法检测肝癌细胞(HepG2)的存活率,考察纳米Fe3O4-TiO2复合物在外磁场作用下对HepG2细胞的光催化杀伤效应.结果表明:采用方法三制备的5%(质量分数)Fe3O4-TiO2复合物具备核-壳结构,在混悬液中分散性较好,平均粒径约为50nm,具有较强的光催化活性和良好的磁响应性,同时将纳米TiO2的光响应范围拓宽至444nm;在外磁场作用下,紫外光和可见光激发纳米Fe3O4-TiO2复合物对HepG2细胞的杀伤效应差异不大,且均强于纳米TiO2;其杀伤效应在0-1.0T范围内随着外磁场强度的增大而增强. 展开更多
关键词 磁靶向 fe3o4-tio2纳米颗粒 HepG2细胞 光催化 杀伤效应
在线阅读 下载PDF
Ru-Cu/Fe_3O_4-TiO_2催化剂上甘油氢解制备1,2-丙二醇的研究 被引量:4
4
作者 李霞 胡玉方 +3 位作者 刘德蓉 冯建 熊伟 宋发益 《化学研究与应用》 CAS CSCD 北大核心 2016年第5期629-635,共7页
以生物柴油生产过程中副产的甘油为原料,通过催化氢解制备1,2-丙二醇是增长生物柴油产业链、提高其经济效益的有效途径.采用浸渍法制备了双金属磁性催化剂Ru-Cu/ Fe3 O4 -TiO2 ,利用X 射线衍射、X 射线光电子能谱、透射电子显微镜、N2 ... 以生物柴油生产过程中副产的甘油为原料,通过催化氢解制备1,2-丙二醇是增长生物柴油产业链、提高其经济效益的有效途径.采用浸渍法制备了双金属磁性催化剂Ru-Cu/ Fe3 O4 -TiO2 ,利用X 射线衍射、X 射线光电子能谱、透射电子显微镜、N2 吸附等方法对催化剂进行了表征,考察了Ru/ Cu 摩尔比、反应温度、H2 压力、反应时间和催化剂用量等因素对催化剂性能的影响.结果表明,Ru-Cu/ Fe3 O4 -TiO2 双金属催化剂具有很高的催化活性和良好的1,2-丙二醇选择性.Cu 的加入没有明显改变Ru 的化学环境,但有效地提高了1,2-丙二醇的选择性,同时Ru 可改善Cu 在钛铁复合载体上的分散性,从而获得了平均金属粒径在5-9 nm 左右的催化剂.在Ru/ Cu 摩尔比1 ∶1. 6、反应温度200 ℃、H2 压力4. 0 MPa、反应时间10 h 的条件下,甘油转化率和1,2-丙二醇的选择性分别高达96. 12% 和86. 77%.反应后产物与催化剂可有效实现磁性分离,为该过程的工业化应用奠定了基础. 展开更多
关键词 Ru-Cu双金属催化剂 fe3o4-tio2 甘油 氢解 1 2-丙二醇
在线阅读 下载PDF
酸处理制备高性能Co_(3)O_(4)催化剂及其催化分解N_(2)O污染研究
5
作者 万思彤 张琬悦 +2 位作者 杜媛婷 熊英 于海彪 《现代化工》 北大核心 2025年第5期125-130,共6页
Co_(3)O_(4)作为氧化亚氮(N_(2)O)催化分解反应中最有潜力的催化剂,面临着反应温度过高、抗杂质气体性能差等问题。在微观结构上对Co_(3)O_(4)催化剂进行设计,采用酸性环境对Co_(3)O_(4)表面进行适当刻蚀,制备富有缺陷的Co_(3)O_(4)催... Co_(3)O_(4)作为氧化亚氮(N_(2)O)催化分解反应中最有潜力的催化剂,面临着反应温度过高、抗杂质气体性能差等问题。在微观结构上对Co_(3)O_(4)催化剂进行设计,采用酸性环境对Co_(3)O_(4)表面进行适当刻蚀,制备富有缺陷的Co_(3)O_(4)催化剂以提高其催化分解N_(2)O的性能。结果表明,采用0.2 mol/L硝酸,在室温下对Co_(3)O_(4)处理1 h后所得到的0.2MCo_(3)O_(4)-N催化剂活性最佳。N_(2)O的完全催化分解温度由单纯Co_(3)O_(4)的475℃降低至0.2MCo_(3)O_(4)-N的400℃。经硝酸处理后,0.2MCo_(3)O_(4)-N表面产生大量缺陷位点,且比表面积也比未处理前增加1倍,具有一定的介孔结构,孔径约为5.6 nm。由于缺陷位的产生,催化剂表面的Co—O键被弱化。此外,所得催化剂具有很好的催化稳定性,在5%O_(2)和100μL/L NO杂质气体共存于反应气的条件下,该催化剂在400℃持续反应10 h后,催化性能几乎没有降低。 展开更多
关键词 催化分解N_(2)o 酸刻蚀 Co_(3)o_(4) 缺陷位点 杂质气体
原文传递
Si_(3)N_(4)/Si_(2)N_(2)O复相粉体对Al_(2)O_(3)-SiC-C浇注料性能的影响
6
作者 李有奇 何健 +2 位作者 陈俊峰 张嘉良 李正坤 《耐火材料》 北大核心 2025年第1期1-7,共7页
为了提高Al_(2)O_(3)-SiC-C浇注料的综合服役性能,采用化学燃烧法合成的微晶氮化硅/氮氧化硅(Si_(3)N_(4)/Si_(2)N_(2)O)复相粉体为添加物,以棕刚玉、板状刚玉、碳化硅、活性α-Al_(2)O_(3)微粉、SiO_(2)微粉、纯铝酸钙水泥、单质Si粉... 为了提高Al_(2)O_(3)-SiC-C浇注料的综合服役性能,采用化学燃烧法合成的微晶氮化硅/氮氧化硅(Si_(3)N_(4)/Si_(2)N_(2)O)复相粉体为添加物,以棕刚玉、板状刚玉、碳化硅、活性α-Al_(2)O_(3)微粉、SiO_(2)微粉、纯铝酸钙水泥、单质Si粉和球沥青为原料,制备了Al_(2)O_(3)-SiC-C浇注料。研究了复相粉体外加量(外加质量分数分别为0、1%、2%、3%和5%)对浇注料性能的影响,同时探究Si_(3)N_(4)/Si_(2)N_(2)O增强试样综合性能的作用机制。结果表明:1)Si_(3)N_(4)/Si_(2)N_(2)O复相粉可以显著改善Al_(2)O_(3)-SiC-C浇注料的力学性能、抗氧化性能和抗热震性;2)Si_(3)N_(4)/Si_(2)N_(2)O复相粉通过填充孔隙、促进烧结反应进行、生成晶须状物质等途径优化了浇注料的显微结构,提高了浇注料的综合性能;3)当Si_(3)N_(4)/Si_(2)N_(2)O复相粉外加量为3%(w)时,浇注料的性能最佳。 展开更多
关键词 Si_(3)N_(4)/Si_(2)N_(2)o复相粉 Al_(2)o_(3)-SiC-C浇注料 抗氧化性 抗热震性
在线阅读 下载PDF
Fe_3O_4-TiO_2复合材料的制备及光催化降解性能 被引量:2
7
作者 陈汝芬 张云 刘辉 《河北师范大学学报(自然科学版)》 CAS 北大核心 2014年第4期382-387,共6页
通过水热法制得Fe3O4八面体微米颗粒,以Fe3O4为载体,用溶胶-凝胶法将纳米TiO2负载于Fe3O4表面,制备Fe3O4-TiO2复合材料,并进行光催化降解甲基橙的研究.结果表明:用溶胶-凝胶法通过控制Fe3O4-TiO2的复合比,在Fe3O4表面能均匀负载一层TiO... 通过水热法制得Fe3O4八面体微米颗粒,以Fe3O4为载体,用溶胶-凝胶法将纳米TiO2负载于Fe3O4表面,制备Fe3O4-TiO2复合材料,并进行光催化降解甲基橙的研究.结果表明:用溶胶-凝胶法通过控制Fe3O4-TiO2的复合比,在Fe3O4表面能均匀负载一层TiO2纳米粒子;与纯Fe3O4和TiO2相比,Fe3O4-TiO2复合材料作为催化剂,对甲基橙的光催化降解性有明显的提高;样品的有机碳去除率较高,重复使用性较好. 展开更多
关键词 fe3o4-tio2 制备 甲基橙 光催化性
在线阅读 下载PDF
Fe基分子筛催化剂应用于NH_(3)选择性催化还原和N_(2)O直接催化分解反应的研究进展
8
作者 明淑君 李新楠 +4 位作者 庞磊 苏长罗 程春晖 杨小东 李涛 《低碳化学与化工》 北大核心 2025年第6期97-112,共16页
柴油车排放的氮氧化物(NO_(x))和氧化亚氮(N_(2)O)对人类健康和生态环境造成了显著危害。NH_(3)选择性催化还原(NH_(3)-SCR)技术是当前控制柴油车尾气中NO_(x)排放的有效方法之一,而N_(2)O的直接催化分解(简称“N_(2)O分解”)则被认为... 柴油车排放的氮氧化物(NO_(x))和氧化亚氮(N_(2)O)对人类健康和生态环境造成了显著危害。NH_(3)选择性催化还原(NH_(3)-SCR)技术是当前控制柴油车尾气中NO_(x)排放的有效方法之一,而N_(2)O的直接催化分解(简称“N_(2)O分解”)则被认为是减少N_(2)O排放的最具潜力的技术。这两种技术的核心均依赖于催化剂的开发与应用。Fe基分子筛催化剂在NH_(3)-SCR和N_(2)O分解反应中展现出了卓越的催化性能,为实现NO_(x)和N_(2)O的同步高效去除提供了一条有前途的路径。综述了Fe基分子筛催化剂在NH_(3)-SCR和N_(2)O分解反应中的催化机理,探讨了Fe基分子筛催化剂的制备方法、拓扑结构、助剂金属掺杂,以及反应环境中共存气体对其理化性质、NH_(3)-SCR活性和N_(2)O分解性能的影响。具体而言,Fe基分子筛催化剂的Fe物种形成与分布受到制备方法和分子筛拓扑结构的显著影响。助剂金属的引入不仅能够增大催化剂的酸性位点含量,还能改善Fe物种的分散性,从而优化其催化性能。此外,共存气体(如NO、O_(2)和H2O)对Fe基分子筛催化剂的N_(2)O分解活性产生不同程度的影响。最后,对Fe基分子筛催化剂的未来研究方向进行了展望,并对催化剂设计优化与性能提升提出了建议。 展开更多
关键词 fe基分子筛催化剂 NH_(3)-SCR N_(2)o直接催化分解 催化机理
在线阅读 下载PDF
热处理工艺对激光熔覆Ti-10V-2Al-3Fe合金粉末修复Ti-6Al-4V合金组织和性能的影响
9
作者 黄兆亮 魏翔宇 +4 位作者 王红顺 王艳 张峰 高俊杰 刘保侠 《机械工程材料》 北大核心 2025年第9期83-89,共7页
采用激光熔覆Ti-10V-2Al-3Fe合金粉末的方法对轧制态Ti-6Al-4V合金表面进行修复,分别进行650℃×2 h退火和750℃×2 h固溶+510℃×8 h时效处理,研究了热处理工艺对试样不同区域显微组织、硬度和拉伸性能的影响。结果表明:... 采用激光熔覆Ti-10V-2Al-3Fe合金粉末的方法对轧制态Ti-6Al-4V合金表面进行修复,分别进行650℃×2 h退火和750℃×2 h固溶+510℃×8 h时效处理,研究了热处理工艺对试样不同区域显微组织、硬度和拉伸性能的影响。结果表明:沉积态激光熔覆层组织由原始柱状β晶粒以及β晶粒内部的网篮状α相组成,热影响区组织为过饱和针状马氏体;退火后熔覆层的部分网篮组织长大,部分层片状α相转化为等轴α相,热影响区中马氏体减少,形成弥散的(α+β)相,原始组织为片状α相延伸晶粒和β晶界的基体中出现α等轴晶;与退火态相比,固溶时效态激光熔覆层部分网篮组织进一步长大,更多层片状α相转化为等轴α相,热影响区中马氏体进一步减少,基体中出现更多α等轴晶。退火和固溶时效处理降低了激光熔覆层的硬度,对基体和热影响区的总体硬度影响不大。退火处理后基体和激光熔覆层的抗拉强度和屈服强度降低,断后伸长率提高;固溶时效处理使得基体强度降低,断后伸长率提高,使得激光熔覆层强度和断后伸长率同步提高。经750℃×2 h固溶和500℃×8 h时效处理后试样的综合力学性能最好,基体和激光熔覆层的硬度分别为349,373 HV,抗拉强度分别为888,1003 MPa,断后伸长率分别为22.1%和20.9%。 展开更多
关键词 激光熔覆 Ti-10V-2Al-3fe合金熔覆层 热处理 TI-6AL-4V合金 显微组织 拉伸性能
在线阅读 下载PDF
La(OH)_(3)/Bi_(4)O_(5)Br_(2)@O-MoS_(2)材料的制备及其光催化还原六价铬的研究
10
作者 刘宇轩 胡蓉仪 刘志华 《环境化学》 北大核心 2025年第10期3717-3730,共14页
通过机械搅拌法原位在O-MoS_(2)上合成可见光驱动的La(OH)_(3)/Bi_(4)O_(5)Br_(2)@O-MoS_(2)光催化剂,使用XRD、XPS、SEM、TEM和UV-Vis DRS等手段进行表征,研究了材料的光电化学性能和处理Cr(Ⅵ)的性能和机理.结果表明,光催化反应30 min... 通过机械搅拌法原位在O-MoS_(2)上合成可见光驱动的La(OH)_(3)/Bi_(4)O_(5)Br_(2)@O-MoS_(2)光催化剂,使用XRD、XPS、SEM、TEM和UV-Vis DRS等手段进行表征,研究了材料的光电化学性能和处理Cr(Ⅵ)的性能和机理.结果表明,光催化反应30 min后,La(OH)_(3)/Bi_(4)O_(5)Br_(2)@O-MoS_(2)(9%)对Cr(Ⅵ)的还原率为85.44%,还原速率(0.06423 min^(−1))远高于Bi_(4)O_(5)Br_(2)(0.02455 min^(−1))和La(OH)_(3)/Bi_(4)O_(5)Br_(2)(0.04334 min^(−1)).根据自由基捕获实验,证明e^(−)是参与Cr(Ⅵ)还原过程的主要活性物质.此外,中性和弱碱性的条件更有利于该材料对六价铬的还原,表明制备的新型La(OH)_(3)/Bi_(4)O_(5)Br_(2)@O-MoS_(2)材料具有良好的实际应用价值. 展开更多
关键词 La(oH)_(3)/Bi_(4)o_(5)Br_(2)@o-MoS_(2) Cr (Ⅵ) 可见光催化.
原文传递
Synthesis and Characterization of Fe3O4 Nanoparticles by Sol-Gel Method Using Water as a Solvent
11
作者 Ahmad Mustafa Usman Ali +4 位作者 Mukarama   Ali Iqbal Maria Qayyum Inam Ul Haq Fakhar Islam 《Advances in Nanoparticles》 2025年第1期1-11,共11页
Ferromagnetic Fe3O4 nanoparticles were synthesized using water as the solvent through the sol-gel method, which was selected for its cost-effectiveness, simplicity, and eco-friendly nature. The synthesized nanoparticl... Ferromagnetic Fe3O4 nanoparticles were synthesized using water as the solvent through the sol-gel method, which was selected for its cost-effectiveness, simplicity, and eco-friendly nature. The synthesized nanoparticles were characterized using a variety of techniques, including Fourier Transform Infrared (FTIR) spectroscopy, X-ray powder diffraction (XRD), Scanning Electron Microscopy (SEM), Thermogravimetric Analysis (TGA), and Vibrating Sample Magnetometer (VSM). These characterizations confirmed the successful formation of Fe3O4 nanoparticles. The FTIR spectra identified characteristic peaks corresponding to the functional groups present, and XRD analysis, using Scherer’s equation, determined an average crystalline size of 1.2 nm for the Fe3O4 nanoparticles. TGA results demonstrated the thermal stability of the nanoparticles, SEM imaging revealed distinct honeycomb-like structures for the nanoparticles synthesized with water as the solvent, while the VSM analysis was used to determine the magnetic behavior of the nanoparticles. 展开更多
关键词 fe3o4 Nanoparticles Sol-Gel Synthesis Honeycomb Structures FTIR XRD SEM TGA VSM
在线阅读 下载PDF
Understanding the interatomic electron transfer effect on boosting electrocatalytic water splitting over Nd-Co_(3)O_(4)nanosheets self-supporting electrode
12
作者 Chenliang Zhou Cheng-Zong Yuan +4 位作者 Fengyang Jing Cong-Hui Li Hongrui Zhao Yuting Sun Wenjing Yuan 《Journal of Energy Chemistry》 2025年第7期142-150,共9页
Regulating the orbital spin-electron filling of metal centers via interatomic electron transfer in transition metal oxides is one promising approach to enhancing their electrocatalytic oxygen evolution reaction(OER)pe... Regulating the orbital spin-electron filling of metal centers via interatomic electron transfer in transition metal oxides is one promising approach to enhancing their electrocatalytic oxygen evolution reaction(OER)performances,while it is still a challenge due to lacking of efficient strategy and deep understanding.In this work,a facile strategy containing electrochemical deposition and annealing in air atmosphere has been proposed to introduce monodispersed neodymium(Nd)atoms into spinel Co_(3)O_(4)nanosheets to trigger the electron transfer.Accordingly,the as-prepared Nd doped Co_(3)O_(4)nanosheets(Nd/Co_(3)O_(4))on nickel foam or carbon cloth showed greatly enhanced OER performances,with low overpotential of 284 and 396 mV at 10 m A cm^(-2),small Tafel slope of 95 and 119 mV dec^(-1)in 1.0 M KOH and 0.5 M H_(2)SO_(4),respectively.The experimental and density function theory results coherently indicate that the charge transfer in the Nd-O-Co asymmetric configuration not only enhances the conductivity of Co_(3)O_(4),but also regulates the filling degree of egorbitals of Co,leading to higher spin states,optimized adsorption ability,and accelerated H_(2)O dissociation process,thus achieving boosted OER activity. 展开更多
关键词 Charge transfer E_(g)orbitals filling Nd doped Co_(3)o_(4) H_(2)o dissociation oxygen evolution reaction
在线阅读 下载PDF
Fe_3O_4-TiO_2·nH_2O·Al吸附剂去除水中氟离子 被引量:8
13
作者 蒋步青 李继香 +4 位作者 邱长泉 何淑英 康长安 轩军旗 潘文灏 《环境工程学报》 CAS CSCD 北大核心 2016年第5期2259-2264,共6页
以实验室制备的Fe_3O_4-TiO_2·n H_2O·Al吸附剂处理模拟和实际含氟废水,探讨了吸附剂用量、体系p H、吸附温度和吸附时间等因素对F-吸附效果的影响。结果表明:在初始F-浓度16.1 mg/L,起始p H 8.0,吸附剂投加量5 g/L,室温(... 以实验室制备的Fe_3O_4-TiO_2·n H_2O·Al吸附剂处理模拟和实际含氟废水,探讨了吸附剂用量、体系p H、吸附温度和吸附时间等因素对F-吸附效果的影响。结果表明:在初始F-浓度16.1 mg/L,起始p H 8.0,吸附剂投加量5 g/L,室温(约25℃)下吸附15 min时,模拟和实际废水的出水F-均可达到〈10 mg/L的《电镀污染物排放标准》和《污水综合排放标准》,且吸附剂的容量都在1.6 mg/g左右,显示Fe_3O_4-TiO_2·n H_2O·Al具有一定的实际应用价值。含氟水溶液初始p H对Fe_3O_4-TiO_2·n H_2O·Al吸附F-性能影响较大。在p H介于3.0~5.0时,吸附容量较大,过高或过低都会导致吸附容量降低。Fe_3O_4-TiO_2·n H_2O·Al吸附F-的过程为放热反应,升温不利于F-的吸附。该吸附剂吸附F-的过程为化学吸附,符合准二级动力学模型,等温线拟合接近Freundlich吸附等温线。 展开更多
关键词 fe3o4-tio2·nH2o·Al 除氟 准二级动力学模型 Freundlich吸附等温线
原文传递
BiOI/g-C_(3)N_(4)/NH_(2)-MIL-53(Fe)三元异质结光催化剂的合成与性能研究 被引量:1
14
作者 何林 吴敏 《化工时刊》 CAS 2024年第3期15-22,共8页
半导体光催化技术是解决能源危机和环境污染的有效手段。作者采用一步溶剂热法制备了Bi OI/g-C_(3)N_(4)/NH_(2)-MIL-53(Fe)三元异质结催化剂。以X射线衍射、扫描电子显微镜等表征方法对样品进行分析,以双酚S为目标污染物考察了催化剂... 半导体光催化技术是解决能源危机和环境污染的有效手段。作者采用一步溶剂热法制备了Bi OI/g-C_(3)N_(4)/NH_(2)-MIL-53(Fe)三元异质结催化剂。以X射线衍射、扫描电子显微镜等表征方法对样品进行分析,以双酚S为目标污染物考察了催化剂的光催化性能,以自由基捕获实验得出·OH、h^(+)和·O_(2)^(-)在降解过程中均发挥强氧化作用,并基于催化剂光芬顿性能研究以及半导体能带结构,提出其催化光芬顿反应的可能的机理。 展开更多
关键词 Bi oI g-C_(3)N_(4) NH_(2)-MIL-53(fe) 光芬顿法
在线阅读 下载PDF
纳米Fe_3O_4-TiO_2靶向光动力疗法对肝癌细胞的杀伤效应(英文)
15
作者 王玲 文雯 +5 位作者 李莎 付正卿 仝月菊 王娟 韩冬 张爱平 《无机化学学报》 SCIE CAS CSCD 北大核心 2016年第3期393-404,共12页
光动力疗法(PDT)作为一种迅速发展的传统替代疗法,在抗癌治疗中显示出巨大的潜力。为增强靶向性和提高光催化杀伤效率,本研究设计了一种新型光敏剂Fe_3O_4-Ti O_2磁性纳米粒。在不同外磁场下,考察其在可见光和紫外光激发下对肝癌细胞的... 光动力疗法(PDT)作为一种迅速发展的传统替代疗法,在抗癌治疗中显示出巨大的潜力。为增强靶向性和提高光催化杀伤效率,本研究设计了一种新型光敏剂Fe_3O_4-Ti O_2磁性纳米粒。在不同外磁场下,考察其在可见光和紫外光激发下对肝癌细胞的杀伤效应。同时利用流式细胞术检测纳米Fe_3O_4-Ti O_2对肝癌细胞凋亡率、细胞周期和线粒体膜电位的影响。根据纳米Fe_3O_4-Ti O_2和肝癌细胞的作用方式探讨其抗癌机制。结果表明,可见光激发纳米Fe_3O_4-Ti O_2可以杀伤癌细胞,且其杀伤效率与紫外光激发下无明显差别。此外,Fe_3O_4-Ti O_2比Ti O_2具有更高的细胞摄取率,从而使其具有更高的选择性和光催化杀伤效率。其作用机制是光催化纳米Fe_3O_4-Ti O_2产生活性氧ROS抑制癌细胞,然后通过阻滞细胞周期G_0/G_1期,降低线粒体膜电位,线粒体去极化,最终诱导细胞凋亡。 展开更多
关键词 光动力疗法 fe3o4-tio2纳米粒 光催化 机制 肝癌细胞
在线阅读 下载PDF
固体超强酸SO_4^(2-)/Fe_2O_3-TiO_2催化合成癸二酸二乙酯的研究 被引量:12
16
作者 董壮龙 郭俊胜 《精细石油化工》 CAS CSCD 北大核心 2003年第1期23-25,共3页
研究了用固体超强酸SO2 -4/Fe2 O3 TiO2 为催化剂 ,由癸二酸和乙醇反应合成癸二酸二乙酯的最佳工艺条件。结果表明 ,当n(醇 )∶n(酸 ) =4 .0∶1,催化剂用量为酸质量的 5 % ,反应时间为 3.5h ,酯的产率可达96 %。该工艺产率高 ,反应时间... 研究了用固体超强酸SO2 -4/Fe2 O3 TiO2 为催化剂 ,由癸二酸和乙醇反应合成癸二酸二乙酯的最佳工艺条件。结果表明 ,当n(醇 )∶n(酸 ) =4 .0∶1,催化剂用量为酸质量的 5 % ,反应时间为 3.5h ,酯的产率可达96 %。该工艺产率高 ,反应时间短 ,无腐蚀无污染 ,催化剂可回收、活化、重复使用 10次。 展开更多
关键词 催化合成 癸二酸二乙酯 研究 固体超强酸催化剂 So4^2-/fe2o3-tio2 催化酯化
在线阅读 下载PDF
Fe_(3)O_(4)/Cu_(2)O的制备及其类芬顿性能研究
17
作者 葛伊柠 姜承志 +1 位作者 刘彦祺 王新颢 《沈阳理工大学学报》 CAS 2024年第4期57-62,69,共7页
为提高Fe_(3)O_(4)在类芬顿反应体系中对污染物的去除效果,基于类芬顿催化氧化技术,制备了Fe_(3)O_(4)/Cu_(2)O复合材料作为非均相类芬顿催化剂,与H_(2)O_(2)共同构成以亚甲基蓝模拟废水为目标物的类芬顿催化氧化体系。对比分析不同实... 为提高Fe_(3)O_(4)在类芬顿反应体系中对污染物的去除效果,基于类芬顿催化氧化技术,制备了Fe_(3)O_(4)/Cu_(2)O复合材料作为非均相类芬顿催化剂,与H_(2)O_(2)共同构成以亚甲基蓝模拟废水为目标物的类芬顿催化氧化体系。对比分析不同实验条件下Fe_(3)O_(4)/Cu_(2)O复合材料的类芬顿活性,并通过X射线衍射仪、扫描电子显微镜等对材料进行表征。实验结果表明:当Fe_(3)O_(4)与CuCl_(2)·2H_(2)O的复合配比(质量比)为2∶1时制备Fe_(3)O_(4)/Cu_(2)O,且其投加量为40 mg、H_(2)O_(2)用量为0.5 mL时,对浓度为6 mg/L的废水溶液中亚甲基蓝的去除率达到84.27%,类芬顿活性较好;类芬顿反应中起主要活性作用的是·OH。 展开更多
关键词 fe_(3)o_(4)/Cu_(2)o 类芬顿 H_(2)o_(2) 亚甲基蓝
在线阅读 下载PDF
Fe_3O_4@SiO_2-TiO_2磁性介孔复合材料光催化降解亚甲基蓝的性能研究 被引量:6
18
作者 谢焕玲 贺卫 +2 位作者 陈格 全学军 杨桔材 《内蒙古工业大学学报(自然科学版)》 2014年第1期25-31,共7页
染料废水处理是水污染治理中非常重要内容之一,针对染料废水带有极高的色度、可生化性差和含"三致"物等特点。本文采用水热法制备复合材料用于染料废水处理。通过XRD、TEM、SBET等表征手段证实制备材料为核-壳Fe3O4@SiO2-TiO... 染料废水处理是水污染治理中非常重要内容之一,针对染料废水带有极高的色度、可生化性差和含"三致"物等特点。本文采用水热法制备复合材料用于染料废水处理。通过XRD、TEM、SBET等表征手段证实制备材料为核-壳Fe3O4@SiO2-TiO2复合材料。将此材料用于染料废水处理,选用亚甲基蓝(Methylene Blue,简称MB)作为染料废水典型目标物,测定催化剂Ti:Si摩尔比、催化剂用量、染料溶液pH值和催化剂重复利用对染料废水降解效果影响。研究结果表明,染料废水浓度为14mg/L,双氧水用量为2mL,催化剂用量为2g/L,脱色90min时,溶液脱色率能达到98.6%。催化剂重复使用4次,其脱色效果仍然保持在90%左右。由此可见,用此方法制备的核-壳材料是比较有效且实用的一种染料废水处理非均相Fenton催化剂。 展开更多
关键词 fe3o4@Sio2-tio2 水热合成法 亚甲基蓝 染料废水处理 脱色率
在线阅读 下载PDF
复合固体酸SO_4^(2-)/Fe_2O_3-TiO_2催化合成环己酮缩乙二醇 被引量:1
19
作者 胡逢恺 《化工时刊》 CAS 2008年第5期37-39,共3页
以复合固体酸SO42-/Fe2O3-TiO2为多相催化剂,通过环己酮和乙二醇反应合成了环己酮缩乙二醇。探讨SO42-/Fe2O3-TiO2对缩酮反应的催化活性,较系统地研究了酮醇物质的量比,催化剂用量,反应时间诸因素对产品收率的影响。实验表明:SO42-/Fe2O... 以复合固体酸SO42-/Fe2O3-TiO2为多相催化剂,通过环己酮和乙二醇反应合成了环己酮缩乙二醇。探讨SO42-/Fe2O3-TiO2对缩酮反应的催化活性,较系统地研究了酮醇物质的量比,催化剂用量,反应时间诸因素对产品收率的影响。实验表明:SO42-/Fe2O3-TiO2是合成环己酮缩乙二醇的良好催化剂,在酮醇物质的量比为1∶1.5,催化剂用量为反应物料总质量的2%,带水剂选用环己烷,反应时间1.5 h的条件下,环己酮缩乙二醇的收率可达92.7%。 展开更多
关键词 复合固体酸 So4^2-/fe2o3-tio2 环己酮缩乙二醇 催化合成
在线阅读 下载PDF
Fe_3O_4/Ce^(3+)-TiO_2复合光催化材料的制备及其光催化性能研究 被引量:2
20
作者 王凡非 冯启明 +2 位作者 王维清 黄阳 夏维清 《功能材料》 EI CAS CSCD 北大核心 2014年第17期17099-17103,共5页
采用溶胶-凝胶法,以钛酸四丁酯、硝酸铈为主要原料,无水乙醇为溶剂,冰醋酸为抑制剂,浓硝酸为催化剂制得稳定的Ce3+掺杂TiO2溶胶,其凝胶经不同温度煅烧3 h后制得Ce3+掺杂量不同的TiO2粉体。用XRD对TiO2进行了测试对比分析,以紫外光为光源... 采用溶胶-凝胶法,以钛酸四丁酯、硝酸铈为主要原料,无水乙醇为溶剂,冰醋酸为抑制剂,浓硝酸为催化剂制得稳定的Ce3+掺杂TiO2溶胶,其凝胶经不同温度煅烧3 h后制得Ce3+掺杂量不同的TiO2粉体。用XRD对TiO2进行了测试对比分析,以紫外光为光源,亚甲基蓝溶液为模拟有机染料废水,研究了TiO2的光催化性能。用化学共沉淀法制备了具有强磁性的纳米Fe3O4水基磁流体,再与Ce3+掺杂TiO2进行复合,制备了Fe3O4负载量不同的磁性Ce3+掺杂TiO2,研究了其对亚甲基蓝的光催化降解效果、磁分离回收率的影响。结果表明,TiO2凝胶热处理温度、Ce3+掺量、TiO2晶型及Fe3O4负载量对亚甲基蓝的光催化活性均有影响。掺Ce3+量为1%,热处理温度650℃的Ce3+掺杂TiO2粉体光催化活性最高。Fe3O4负载量为10%的Fe3O4/Ce3+-TiO2对亚甲基蓝的降解率8 h时达到90.3%,磁分离回收率达96.8%。 展开更多
关键词 纳米fe3o4 磁性Ce3+掺杂Tio2 亚甲基蓝 光催化活性 磁分离回收率
在线阅读 下载PDF