The microstructure and anti-corrosion behavior of Mg–Mn alloys by magnesium scrap have been investigated in this study.The results show that the size of the Fe-rich particles in magnesium scrap decreases but the quan...The microstructure and anti-corrosion behavior of Mg–Mn alloys by magnesium scrap have been investigated in this study.The results show that the size of the Fe-rich particles in magnesium scrap decreases but the quantity increases with the Mn addition.Although the presence of Mn-containing Fe-rich particles with unique symbiotic structure can eff ectively weaken the micro-galvanic corrosion,the presence of more free Fe(Fe-rich particles)does not necessarily lead to severe corrosion of the alloy.The corrosion susceptibility of Mg–Mn–Fe alloy primarily depends on the solubility of iron in the Mg matrix,while it can be significantly reduced by suitable Mn addition.Besides,the tolerance limit of the Fe impurity can be expressed as Femax=0.0083 Mn(relative to the iron solubility).Only when the Fe/Mn ratio is below 0.0083 can the alloy have excellent corrosion resistance,with the corrosion rate changing in the scope of 0.38±0.09 to 0.54±0.15 mg/cm^(2) day and icorr from 3 to 9×10^(–4) A/cm^(2).展开更多
The iron and manganese absorption properties of several filter media were studied. Four plain filter media and six surface-modified media were examined. The surface modification was performed using potassium permangan...The iron and manganese absorption properties of several filter media were studied. Four plain filter media and six surface-modified media were examined. The surface modification was performed using potassium permanganate as a surface treatment. The surface-modified manganese sand was found to be most efficient at removing iron and manganese from water. The metal concentrations in filtered effluent were between 0.01 and 0.04 mg/L, which is far lower than the standard for recycle water. A concen-tration of 5% KMnO4 was found to be most effective as surface modifier. The surface of the manganese sand modified by 5% KMnO4 was examined and found to be covered with a dense membrane of some compound. The membrane had the advantages of uniform texture, large surface area and physical and chemical stability. It was effective at removing iron and manganese from mine water.展开更多
With the laser remelting of cast alloys combined with non-equilibrium liquidus projection thermodynamic calculations,a high-strength and heat-resistant Al-3Fe-2Mn alloy was designed.Incorporating Mn atoms into the met...With the laser remelting of cast alloys combined with non-equilibrium liquidus projection thermodynamic calculations,a high-strength and heat-resistant Al-3Fe-2Mn alloy was designed.Incorporating Mn atoms into the metastable nanoscale Al_(6)Fe phase,occupying some lattice sites,enhances its thermal stability.Additionally,during rapid solidification of laser powder bed fusion(L-PBF),the solubility of Fe and Mn elements in the aluminum alloy increases significantly,forming a supersaturated solid solution with improved strength.This alloy demonstrates excellent processability,achieving a relative density of over 99%,and tensile strengths of 295 MPa at 200℃ and 230 MPa at 300℃.The Al-3Fe-2Mn alloy holds great potential for wide applications due to its high strength at high temperature.展开更多
基金financially supported by the National Key Research and Development Program of China(No.2016YFB0301100)the Fundamental Research Funds for the Central Universities(No.2018CDJDCD0001)the Key Nature Science Foundation of Chongqing(No cstc2017jcyjBX0040)。
文摘The microstructure and anti-corrosion behavior of Mg–Mn alloys by magnesium scrap have been investigated in this study.The results show that the size of the Fe-rich particles in magnesium scrap decreases but the quantity increases with the Mn addition.Although the presence of Mn-containing Fe-rich particles with unique symbiotic structure can eff ectively weaken the micro-galvanic corrosion,the presence of more free Fe(Fe-rich particles)does not necessarily lead to severe corrosion of the alloy.The corrosion susceptibility of Mg–Mn–Fe alloy primarily depends on the solubility of iron in the Mg matrix,while it can be significantly reduced by suitable Mn addition.Besides,the tolerance limit of the Fe impurity can be expressed as Femax=0.0083 Mn(relative to the iron solubility).Only when the Fe/Mn ratio is below 0.0083 can the alloy have excellent corrosion resistance,with the corrosion rate changing in the scope of 0.38±0.09 to 0.54±0.15 mg/cm^(2) day and icorr from 3 to 9×10^(–4) A/cm^(2).
基金provided by the National Hi-tech Research and Development Program of China (No.2008AA06z305)the National Natural Science Foundation of China (No.50678172)the Science and Technology Research Program of the Ministry of Education of China (No.107022)
文摘The iron and manganese absorption properties of several filter media were studied. Four plain filter media and six surface-modified media were examined. The surface modification was performed using potassium permanganate as a surface treatment. The surface-modified manganese sand was found to be most efficient at removing iron and manganese from water. The metal concentrations in filtered effluent were between 0.01 and 0.04 mg/L, which is far lower than the standard for recycle water. A concen-tration of 5% KMnO4 was found to be most effective as surface modifier. The surface of the manganese sand modified by 5% KMnO4 was examined and found to be covered with a dense membrane of some compound. The membrane had the advantages of uniform texture, large surface area and physical and chemical stability. It was effective at removing iron and manganese from mine water.
基金supported by the National Natural Science Foundation of China(No.U21B2073)the Science and Technology Project of the Science and Technology Department of Hubei Province,China(No.2022EHB020)。
文摘With the laser remelting of cast alloys combined with non-equilibrium liquidus projection thermodynamic calculations,a high-strength and heat-resistant Al-3Fe-2Mn alloy was designed.Incorporating Mn atoms into the metastable nanoscale Al_(6)Fe phase,occupying some lattice sites,enhances its thermal stability.Additionally,during rapid solidification of laser powder bed fusion(L-PBF),the solubility of Fe and Mn elements in the aluminum alloy increases significantly,forming a supersaturated solid solution with improved strength.This alloy demonstrates excellent processability,achieving a relative density of over 99%,and tensile strengths of 295 MPa at 200℃ and 230 MPa at 300℃.The Al-3Fe-2Mn alloy holds great potential for wide applications due to its high strength at high temperature.