期刊文献+
共找到9篇文章
< 1 >
每页显示 20 50 100
添加Triton X-100提高Streptococcus equisimilis FE-11发酵透明质酸产量和分子量的研究 被引量:1
1
作者 刘金龙 李志敏 +2 位作者 赵国群 孙锡友 任媛媛 《安徽化工》 CAS 2019年第2期30-33,40,共5页
考查了表面活性物质Triton X-100对Streptococcus equisimilis FE-11发酵透明质酸产量和分子量的影响。结果发现:向S.equisimilis FE-11培养体系中添加Triton X-100对透明质酸产量和分子量的影响效果与添加时机和剂量紧密相关,在发酵的... 考查了表面活性物质Triton X-100对Streptococcus equisimilis FE-11发酵透明质酸产量和分子量的影响。结果发现:向S.equisimilis FE-11培养体系中添加Triton X-100对透明质酸产量和分子量的影响效果与添加时机和剂量紧密相关,在发酵的第6小时添加Triton X-100至5 g/L可以使透明质酸产量和分子量同时达到最高水平。5 L发酵罐验证实验表明,应用该添加策略可使透明质酸产量和分子量分别提高至4.21 g/L和2.49 MDa。与不添加Triton X-100相比,分别提升了15.34%和29.02%。与此同时,S.equisimilis FE-11细胞膜结构中饱和脂肪酸/不饱和脂肪酸的比率从0.80降低至0.50,添加Triton X-100显著改变了菌体细胞膜结构,改善了细胞膜的流动性和通透性,促进了透明质酸产量和分子量的提升。 展开更多
关键词 STREPTOCOCCUS equisimilis fe-11 透明质酸 产量 分子量
在线阅读 下载PDF
冷轧变形量对Fe-11Cr-5Al-2Mo合金显微组织和力学性能的影响 被引量:1
2
作者 王馨敏 王玉容 +3 位作者 吴裕 潘钱付 姚力夫 徐祺 《核动力工程》 EI CAS CSCD 北大核心 2024年第S01期159-166,共8页
为掌握Fe-11Cr-5Al-2Mo合金冷变形规律,并为其包壳管材研制提供基础数据和理论依据。开展了不同冷轧变形量的Fe-11Cr-5Al-2Mo合金板材轧制实验,对冷轧后的板材在800℃下进行了1 h退火,并对冷轧板材及退火板材的显微组织演变进行了表征,... 为掌握Fe-11Cr-5Al-2Mo合金冷变形规律,并为其包壳管材研制提供基础数据和理论依据。开展了不同冷轧变形量的Fe-11Cr-5Al-2Mo合金板材轧制实验,对冷轧后的板材在800℃下进行了1 h退火,并对冷轧板材及退火板材的显微组织演变进行了表征,通过室温拉伸试验评价了Fe-11Cr-5Al-2Mo合金的强度和塑性。Fe-11Cr-5Al-2Mo合金板材的变形态组织随着冷轧变形量的增大而拉长,板材的强度随着冷轧变形量的增大而增大。800℃退火1 h后,50%冷轧变形量的板材获得了最细小、均匀的再结晶组织,并且具有良好的韧塑性配合。本文阐明了合金冷轧变形量-组织-性能之间的关系,为Fe-11Cr-5Al-2Mo合金管材冷轧变形量设计和退火工艺研究提供了参考。 展开更多
关键词 fe-11Cr-5Al-2Mo合金 冷轧变形 力学性能 显微组织
原文传递
高速火焰喷涂Fe-25Al/11SiC复合涂层性能研究
3
作者 孙志娟 徐润生 《焊接》 北大核心 2007年第12期50-53,共4页
用高速火焰喷涂方法制备出Fe-25Al/11SiC复合涂层,对涂层的结合强度、抗热震性及温度为650℃时的热腐蚀行为进行研究,并利用扫描电镜和X射线衍射仪(XRD)对腐蚀前后涂层的表面形貌和相组成进行分析。结果表明:Fe-25Al/11SiC复合涂层组织... 用高速火焰喷涂方法制备出Fe-25Al/11SiC复合涂层,对涂层的结合强度、抗热震性及温度为650℃时的热腐蚀行为进行研究,并利用扫描电镜和X射线衍射仪(XRD)对腐蚀前后涂层的表面形貌和相组成进行分析。结果表明:Fe-25Al/11SiC复合涂层组织致密,与基体结合状况良好,且以机械结合为主;该涂层具有较好的抗热震性能;经过150h热腐蚀后,Fe-25Al/11SiC复合涂层腐蚀增重约为基体20钢的1/3,抗热腐蚀性能优异;Fe-25Al/11SiC复合涂层发生的是第二类低温热腐蚀。 展开更多
关键词 高速火焰喷涂 fe-25Al/11SiC复合涂层 热腐蚀
在线阅读 下载PDF
Fe-27Mn-11Al-0.9C低密度钢变形开裂机理研究
4
作者 李振江 庞有超 +3 位作者 赵永琦 胡旭涛 齐会萍 杨雯 《塑性工程学报》 CAS CSCD 北大核心 2024年第12期229-236,共8页
通过Gleeble-3500热模拟实验机对Fe-27Mn-11Al-0.9C低密度钢进行不同温度(700~1200℃)的等温拉伸实验,研究了不同温度下实验钢的变形行为并观察了断裂后的微观组织。结果表明:在700~1200℃温度下进行等温拉伸实验,基体组织为奥氏体和铁... 通过Gleeble-3500热模拟实验机对Fe-27Mn-11Al-0.9C低密度钢进行不同温度(700~1200℃)的等温拉伸实验,研究了不同温度下实验钢的变形行为并观察了断裂后的微观组织。结果表明:在700~1200℃温度下进行等温拉伸实验,基体组织为奥氏体和铁素体两相,流变应力随着温度的升高而逐渐降低,700℃等温拉伸塑性最差,800℃等温拉伸塑性居中,900~1200℃等温拉伸时塑性都较好。变形温度不同,组织会有差别,进而导致拉伸断裂机制不同。700℃等温拉伸时,在奥氏体晶界处有κ-碳化物生成,断裂形式为典型的沿晶断裂。800℃等温拉伸时,晶界仍然有脆性的κ-碳化物析出,但该温度下变形时奥氏体能够发生塑性变形,导致800℃拉伸断裂为沿晶延性断裂。当拉伸温度为900~1200℃时,碳化物未析出,塑性显著增强,在奥氏体和铁素体的相界处发生断裂,为韧性断裂。 展开更多
关键词 fe-27Mn-11Al-0.9C 等温拉伸 微观组织 κ-碳化物 断裂机制
原文传递
Corrosion behavior of Ce-doped Ni-10Cu-11Fe-6Al(wt%) inert anode in molten CaCl_2 salt 被引量:1
5
作者 Mehdi Alzamani Kourosh Jafarzadeh Arash Fattah-alhosseini 《Journal of Rare Earths》 SCIE EI CAS CSCD 2019年第2期218-224,共7页
In this research the effect of cerium dopingon corrosion behavior of Ni-10 Cu-11 Fe-6 Al(wt%) alloy as a novel inert anode in titanium electrolytic production was investigated. The samples, including un-doped and Ce-d... In this research the effect of cerium dopingon corrosion behavior of Ni-10 Cu-11 Fe-6 Al(wt%) alloy as a novel inert anode in titanium electrolytic production was investigated. The samples, including un-doped and Ce-doped nickel-based alloys, were prepared using vacuum induction melting(VIM) process and then exposed to the electrolysis in molten calcium chloride at 900C at à1.6 V versus graphite reference electrode for different immersion time. The surface and cross-section of the samples were characterized using scanning electron microscopy(SEM), and their electrochemical behavior was investigated by electrochemical impedance spectroscopy(EIS). The results show that the un-doped samples have greater number of voids and porosities as compared to that of the 0.0064 wt% Ce-doped samples(as the optimum content of cerium in the alloy). Thus, the nickel-based alloy becomes less sensitive to the pitting by addition of cerium. The corrosion penetration depth reaches about 244 mm after 16 h of electrolysis in the un-doped sample, while was approximately 103 mm for the 0.0064 wt% Ce-doped sample, which is an indication that the corrosion penetration depth decreases by adding small amounts of Ce. 展开更多
关键词 Ni-10Cu-11fe-6Al Ce doping Corrosion behavior MOLTEN CACL2 SALT Nickel-based alloy Rare earths
原文传递
1∶12型Tb(Fe_(1-x)Co_x)_(11.3)Nb_(0.7)化合物的结构和磁性
6
作者 史俊锋 徐孝贞 +1 位作者 富泉 王建立 《中央民族大学学报(自然科学版)》 1999年第1期46-50,共5页
通过x射线衍射和磁性测量,研究了1∶12型稀土过渡族金属间化合物Tb(Fe1-xCox)11.3Nb0.7的结构和磁性,其中x=0.00、0.05、0.10、0.15、0.20和0.30.实验结果表明所有化合物均是四... 通过x射线衍射和磁性测量,研究了1∶12型稀土过渡族金属间化合物Tb(Fe1-xCox)11.3Nb0.7的结构和磁性,其中x=0.00、0.05、0.10、0.15、0.20和0.30.实验结果表明所有化合物均是四方ThMn12型结构.晶格常数a、c以及晶胞体积V随Co含量增加而减小;Co替代部分Fe后导致Tb(Fe1-xCox)11.3Nb0.7化合物的居里温度TC显著增加,而自旋重取向温度TSR单调降低。 展开更多
关键词 Tb(Fe1-xCox)11.3Nb0.7化合物 结构 磁性 稀土
在线阅读 下载PDF
新型接触线材料的研究 被引量:4
7
作者 姚再起 葛继平 +1 位作者 刘书华 李明生 《中国铁道科学》 EI CAS CSCD 北大核心 2004年第6期99-102,共4页
利用SEM,XRD,MTS,电阻率测试仪等试验手段,研究在300~750℃经2h时效处理,以及室温变形+中间热处理对Cu 11 5%Fe合金的组织、力学性能和导电性的影响。结果表明,Fe在Cu中的溶解度和析出粒子大小严重影响着Cu 11 5%Fe合金的性能,经过550... 利用SEM,XRD,MTS,电阻率测试仪等试验手段,研究在300~750℃经2h时效处理,以及室温变形+中间热处理对Cu 11 5%Fe合金的组织、力学性能和导电性的影响。结果表明,Fe在Cu中的溶解度和析出粒子大小严重影响着Cu 11 5%Fe合金的性能,经过550℃,2h时效处理可获得较好的导电性。合金经室温变形后,Fe相由铸态的树枝状变成薄片状纤维;随着形变量的增加,材料的强度提高。加入适当的中间热处理可以大大降低其电阻率,获得具有高强度高导电性的形变Cu 11 5%Fe原位复合材料。 展开更多
关键词 形变 原位 复合材料 Cu-11.5%Fe合金 时效处理 电阻率 强度
在线阅读 下载PDF
配合物[Fe_2(μ_2-OH)(tpmc)](ClO_4)_3·EtOH的合成及其晶体结构
8
作者 王宏图 刘波 《合成化学》 CAS CSCD 北大核心 2012年第6期724-727,共4页
以Fe(ClO4)2.6H2O和N,N',N'',N'''-四(2-吡啶甲基)-1,4,8,11-四氮杂环十四烷(tpmc)为原料,采用溶液界面扩散法,在二氯甲烷与乙醇两相溶剂的界面上制得Fe(Ⅱ)的双核配合物[Fe2(μ2-OH)(C34H44N8)](ClO4)3.EtOH(... 以Fe(ClO4)2.6H2O和N,N',N'',N'''-四(2-吡啶甲基)-1,4,8,11-四氮杂环十四烷(tpmc)为原料,采用溶液界面扩散法,在二氯甲烷与乙醇两相溶剂的界面上制得Fe(Ⅱ)的双核配合物[Fe2(μ2-OH)(C34H44N8)](ClO4)3.EtOH(1),其结构经X-射线单晶衍射表征。1属正交晶系,Pbcm空间群,晶胞参数a=11.652(2),b=17.505(4),c=22.256(5),α=β=γ=90°,V=453 9.7(16)3,Z=4,Dc=1.519 g.cm-3,μ=0.887 mm-1,F(000)=2 152,R1=0.058 3,ωR2=0.175 8。1中的Fe(Ⅱ)分别与外向型配体tpmc的十四元环上的两个氮原子,两个吡啶环上的氮原子和μ2-OH上的氧原子配位,形成一个畸变的三角双锥几何构型。连接两个Fe(Ⅱ)核中心的μ2-OH氧桥以及分子内和分子间的氢键缔合作用,增强了晶体结构的稳定性。 展开更多
关键词 N N' N'' N'''-四(2-吡啶甲基)-1 4 8 11-四氮杂环十四烷 Fe(Ⅱ) 双核配合物 μ2-OH氧桥 合成 晶体结构
在线阅读 下载PDF
新型钼系低温脱氢催化剂的催化机理、制备方法及其性能优化 被引量:1
9
作者 秦玉楠 《中国钼业》 2004年第4期24-29,共6页
在Mo-Fe-K-Ce金属氧化物体系中添加适量的ZnO,可使脱氢活性相(KFe11O17)的形成温度降低50℃以上,从而使得乙苯脱氢生成苯乙烯的反应温度下降了5~18℃。新研制的Mo-Fe-K-Ce-Zn系催化剂具有较佳的机械强度、耐水性能和稳定性,可以在工业... 在Mo-Fe-K-Ce金属氧化物体系中添加适量的ZnO,可使脱氢活性相(KFe11O17)的形成温度降低50℃以上,从而使得乙苯脱氢生成苯乙烯的反应温度下降了5~18℃。新研制的Mo-Fe-K-Ce-Zn系催化剂具有较佳的机械强度、耐水性能和稳定性,可以在工业装置上应用。 展开更多
关键词 新型钼系催化剂 脱氢活性相 乙苯脱氢 稳定性 性能评价
在线阅读 下载PDF
上一页 1 下一页 到第