Fe-Al/Cr3C2 coatings were sprayed on low steel by high velocity arc spraying(HVAS) technology. The influences of oxides on erosion, corrosion and wear behavior for high velocity arc sprayed Fe-Al/Cr3C2 coatings were...Fe-Al/Cr3C2 coatings were sprayed on low steel by high velocity arc spraying(HVAS) technology. The influences of oxides on erosion, corrosion and wear behavior for high velocity arc sprayed Fe-Al/Cr3C2 coatings were studied. The results show that HVAS-sprayed Fe-Al/Cr3C2 coatings have good erosion, heat corrosion and wear resistance. The erosion resistance improves with the increase of the temperature. On one hand, the ferrous oxides are incompact, so they peel off the surface of the coatings easily during the high temperature erosion. On the other hand, compact Al2O3 films on the surface can protect the coatings.展开更多
New chiral C_2-symmetrical bis(oxazoline) compounds bearing one isobutyl-, secbutyl-, benzyl- or isopropyl-substituent at the 4-position have been prepared and characterized.
The kinetics of CO hydrogenation for the synthesis of C_2 oxygenates overRh-Mn-Li-Fe/SiO_2 was investigated. Kinetic parameters for the formation of ethanol, acetaldehyde,C'2 oxygenates, methanol and methane were ...The kinetics of CO hydrogenation for the synthesis of C_2 oxygenates overRh-Mn-Li-Fe/SiO_2 was investigated. Kinetic parameters for the formation of ethanol, acetaldehyde,C'2 oxygenates, methanol and methane were obtained. The activation energy. H_2 and CO dependenceorders for ethanol and acetaldehyde formation differed greatly, the large difference seemed to implythat they were formed through different intermediates.展开更多
文摘Fe-Al/Cr3C2 coatings were sprayed on low steel by high velocity arc spraying(HVAS) technology. The influences of oxides on erosion, corrosion and wear behavior for high velocity arc sprayed Fe-Al/Cr3C2 coatings were studied. The results show that HVAS-sprayed Fe-Al/Cr3C2 coatings have good erosion, heat corrosion and wear resistance. The erosion resistance improves with the increase of the temperature. On one hand, the ferrous oxides are incompact, so they peel off the surface of the coatings easily during the high temperature erosion. On the other hand, compact Al2O3 films on the surface can protect the coatings.
基金the Foundation for Academic Leader by the Education Department of Hunan province.
文摘New chiral C_2-symmetrical bis(oxazoline) compounds bearing one isobutyl-, secbutyl-, benzyl- or isopropyl-substituent at the 4-position have been prepared and characterized.
基金This work was financially by the Chinese Science and Technology Ministry (Grant No.G1999022404)
文摘The kinetics of CO hydrogenation for the synthesis of C_2 oxygenates overRh-Mn-Li-Fe/SiO_2 was investigated. Kinetic parameters for the formation of ethanol, acetaldehyde,C'2 oxygenates, methanol and methane were obtained. The activation energy. H_2 and CO dependenceorders for ethanol and acetaldehyde formation differed greatly, the large difference seemed to implythat they were formed through different intermediates.