期刊文献+
共找到261篇文章
< 1 2 14 >
每页显示 20 50 100
Effects of current density on preparation and performance of Al/conductive coating/α-PbO_2-Ce O_2-TiO_2/β-Pb O_2-MnO_2-WC-ZrO_2 composite electrode materials 被引量:1
1
作者 杨海涛 陈步明 +5 位作者 郭忠诚 刘焕荣 张永春 黄惠 徐瑞东 付仁春 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2014年第10期3394-3404,共11页
Al/conductive coating/α-Pb O2-Ce O2-Ti O2/β-PbO 2-MnO 2-WC-Zr O2 composite electrode material was prepared on Al/conductive coating/α-PbO 2-Ce O2-Ti O2 substrate by electrochemical oxidation co-deposition technique... Al/conductive coating/α-Pb O2-Ce O2-Ti O2/β-PbO 2-MnO 2-WC-Zr O2 composite electrode material was prepared on Al/conductive coating/α-PbO 2-Ce O2-Ti O2 substrate by electrochemical oxidation co-deposition technique. The effects of current density on the chemical composition, electrocatalytic activity, and stability of the composite anode material were investigated by energy dispersive X-ray spectroscopy(EDXS), anode polarization curves, quasi-stationary polarization(Tafel) curves, electrochemical impedance spectroscopy(EIS), scanning electron microscopy(SEM), and X-ray diffraction(XRD). Results reveal that the composite electrode obtained at 1 A/dm2 possesses the lowest overpotential(0.610 V at 500 A/m2) for oxygen evolution, the best electrocatalytic activity, the longest service life(360 h at 40 °C in 150 g/L H2SO4 solution under 2 A/cm2), and the lowest cell voltage(2.75 V at 500 A/m2). Furthermore, with increasing current density, the coating exhibits grain growth and the decrease of content of Mn O2. Only a slight effect on crystalline structure is observed. 展开更多
关键词 composite electrode material A1 substrate β-pbo2-mno2-wc-zro2 electrochemical co-deposition current density
在线阅读 下载PDF
β-PbO_2电极中加入纳米级TiO_2的性能研究 被引量:18
2
作者 蔡天晓 鞠鹤 +2 位作者 武宏让 康新婷 张玉萍 《稀有金属材料与工程》 SCIE EI CAS CSCD 北大核心 2003年第7期558-560,共3页
通过对传统电沉积β-PbO2工艺技术的改进(在镀液中加入纳米级TiO2),使镀层β-PbO2的脆性大大降低,从而使其可在温度为90℃的H2SO4介质中使用,镀层不会从基材剥落,而是自然损耗。
关键词 β-pbo2电极 电催化 TIO2 纳米
在线阅读 下载PDF
δ-MnO_2氧化降解苯酚的机理研究 被引量:15
3
作者 徐建 张莹 +2 位作者 李蕾 郭昌胜 张远 《环境科学学报》 CAS CSCD 北大核心 2013年第4期1010-1016,共7页
δ-MnO2以水羟锰矿和水钠锰矿的形式普遍存在于陆地和海洋环境中,是酚类等有机污染物发生非生物转化的重要氧化剂.本文研究了实验室制备的δ-MnO2悬浮液对苯酚的去除作用,同时讨论了pH、二氧化锰投加量、离子强度、共存金属离子和腐殖... δ-MnO2以水羟锰矿和水钠锰矿的形式普遍存在于陆地和海洋环境中,是酚类等有机污染物发生非生物转化的重要氧化剂.本文研究了实验室制备的δ-MnO2悬浮液对苯酚的去除作用,同时讨论了pH、二氧化锰投加量、离子强度、共存金属离子和腐殖酸等不同影响因素对苯酚去除效率的影响.结果表明,苯酚氧化降解的最佳pH和δ-MnO2投加量分别为3.62和0.13mg·L-1.溶液中共存的Na+和Mn2+会对苯酚氧化降解产生抑制作用,而Mg2+和Ca2+对反应过程没有明显的影响.溶液中共存的腐殖酸也对苯酚的降解过程产生了抑制作用,随着腐殖酸的浓度由1mg·L-1增加到5mg·L-1,苯酚的去除率从96.9%降为78.9%.GC-MS分析发现,对苯二酚为该过程的主要中间产物,同时给出了苯酚在δ-MnO2存在时的可能降解机制. 展开更多
关键词 Δ-mno2 苯酚 氧化降解 机理
原文传递
Ti/α-PbO_2/β-PbO_2电极电化学降解2-氯酚(英文) 被引量:12
4
作者 张钱丽 郭新艳 +2 位作者 曹晓丹 王东田 魏杰 《催化学报》 SCIE EI CAS CSCD 北大核心 2015年第7期975-981,共7页
采用电化学沉积法在Ti基底上制备了复合电极Ti/α-PbO 2/β-PbO 2,扫描电镜结果表明电极呈现由β-PbO 2小晶体组成的菜花状微观形貌.所制电极在电化学降解环境污染物2-氯酚时表现出较高的电催化效率、较好的电极稳定性和较长的电极寿命... 采用电化学沉积法在Ti基底上制备了复合电极Ti/α-PbO 2/β-PbO 2,扫描电镜结果表明电极呈现由β-PbO 2小晶体组成的菜花状微观形貌.所制电极在电化学降解环境污染物2-氯酚时表现出较高的电催化效率、较好的电极稳定性和较长的电极寿命.用正交实验优化了电化学降解2-氯酚的实验条件.在最优的实验条件(2-氯酚初始浓度50 mg/L,电解质0.1 mol/L Na2SO4,温度35 oC,阳极电流密度20 mA/cm2)下电化学降解180 min后,2-氯酚的去除率达100%.动力学结果表明,Ti/α-PbO 2/β-Pb O2电极上2-氯酚的电化学氧化符合准一级动力学过程. 展开更多
关键词 电化学降解 2-氯酚 β-Pb O2电极 α-pbo 2中间层 动力学
在线阅读 下载PDF
水热法合成δ-MnO_2及其对重金属Pb^(2+)的吸附作用 被引量:12
5
作者 朱丽珺 张金池 +2 位作者 宰德欣 柴家觉 王忺 《安全与环境学报》 CAS CSCD 2007年第4期20-23,共4页
用水热法合成δ-MnO2,研究其对重金属Pb2+的吸附性能,以及溶液的pH值、盐浓度对吸附效果的影响,并与无定型二氧化锰对比。研究结果表明水热法可以成功合成δ-MnO2,且具有颗粒微小,无杂质等优点。δ-MnO2对Pb2+的等温吸附结果用多种等温... 用水热法合成δ-MnO2,研究其对重金属Pb2+的吸附性能,以及溶液的pH值、盐浓度对吸附效果的影响,并与无定型二氧化锰对比。研究结果表明水热法可以成功合成δ-MnO2,且具有颗粒微小,无杂质等优点。δ-MnO2对Pb2+的等温吸附结果用多种等温吸附式拟合,结果显示Temkin方程的拟合效果最好。相同条件下,δ-MnO2对Pb2+的吸附量远大于无定型二氧化锰。同一种吸附剂,对Pb2+吸附率随着溶液pH值的增大而增大,随着盐浓度的增加先增加后稳定再减少。 展开更多
关键词 环境化学 水热法 Δ-mno2 PB^2+ 吸附 二氧化锰
在线阅读 下载PDF
xAu/α-MnO_2催化剂的结构及催化氧化VOCs气体性能 被引量:14
6
作者 叶青 霍飞飞 +2 位作者 王海平 王娟 王道 《高等学校化学学报》 SCIE EI CAS CSCD 北大核心 2013年第5期1187-1194,共8页
以NaOH为沉淀剂,采用沉积-沉淀法制备了α-MnO2负载Au催化剂xAu/α-MnO2(x=1.0%~7.0%,质量分数),利用X射线衍射(XRD)、N2吸附-脱附、H2程序升温还原(H2-TPR)、透射电子显微镜(TEM)和X射线光电子能谱(XPS)等技术对所得样品进行了表征,... 以NaOH为沉淀剂,采用沉积-沉淀法制备了α-MnO2负载Au催化剂xAu/α-MnO2(x=1.0%~7.0%,质量分数),利用X射线衍射(XRD)、N2吸附-脱附、H2程序升温还原(H2-TPR)、透射电子显微镜(TEM)和X射线光电子能谱(XPS)等技术对所得样品进行了表征,并对其催化氧化挥发性有机化合物(VOCs,苯和甲苯)的性能进行了研究.XRD结果表明,负载Au对α-MnO2载体结构影响不大,但对其晶粒大小和比表面积略有影响.随着Au含量的增加,α-MnO2结晶度增强,颗粒增大,Au粒径明显增大.XPS结果表明,随着Au负载量的增加,xAu/α-MnO2的晶格氧(O2-),Mn4+和Au3+的浓度增加.H2-TPR结果表明,由于贵金属的溢氢作用,Au明显提升了xAu/α-MnO2的还原能力,其中3%Au/α-MnO2的还原能力最强.负载Au明显影响xAu/α-MnO2的催化性能,xAu/α-MnO2的催化性能与Au的颗粒分散性、低温还原性能及表面氧物种密切相关,其中3%Au/α-MnO2显示出最佳活性,其催化氧化苯和甲苯的T100分别为280和250℃. 展开更多
关键词 AU α-mno2催化剂 还原性能 协同作用 甲苯 催化氧化
在线阅读 下载PDF
γ-MnO_2对Tl(Ⅰ)的吸附性能 被引量:13
7
作者 邓红梅 王耀龙 +2 位作者 吴宏海 刘涛 陈永亨 《环境科学研究》 EI CAS CSSCI CSCD 北大核心 2015年第1期103-109,共7页
通过静态批处理吸附试验,研究了γ-MnO2对Tl(Ⅰ)(铊)的吸附性能,考察了溶液的pH、离子强度、γ-MnO2投加量、接触时间、初始ρ〔Tl(Ⅰ)〕和温度等因素对吸附的影响.结果表明:在pH为2-3的酸性溶液中,γ-MnO2对Tl(Ⅰ)的吸附容量... 通过静态批处理吸附试验,研究了γ-MnO2对Tl(Ⅰ)(铊)的吸附性能,考察了溶液的pH、离子强度、γ-MnO2投加量、接触时间、初始ρ〔Tl(Ⅰ)〕和温度等因素对吸附的影响.结果表明:在pH为2-3的酸性溶液中,γ-MnO2对Tl(Ⅰ)的吸附容量随着pH的增大而减小;当pH为4-6时,吸附容量随pH的增加而迅速增大;而当pH〉6时,吸附达到平衡.γ-MnO2对Tl(Ⅰ)的吸附量随着离子强度的降低、γ-MnO2投加量的减小而增大.γ-MnO2对Tl(Ⅰ)的吸附在15min内达到平衡,并满足准二级动力学方程.在温度为288、303、318K的条件下,初始ρ〔Tl(Ⅰ)〕为10-1000mg/L时,最大饱和吸附量分别为53.04、49.05、45.03mg/g,符合Freundlich吸附等温方程.γ-MnO2对Tl(Ⅰ)的吸附过程是自发的放热过程.脱附研究表明,γ-MnO2表面的吸附行为属离子交换,并受离子强度影响.试验证明,γ-MnO2是一种极具潜力的Tl(Ⅰ)吸附剂. 展开更多
关键词 Tl(铊) γ-mno2 动力学 等温线 热力学
在线阅读 下载PDF
CaO-SiO_2-Al_2O_3-MnO系低熔点区域控制 被引量:19
8
作者 金利玲 王海涛 +1 位作者 许中波 王福明 《北京科技大学学报》 EI CAS CSCD 北大核心 2007年第6期574-577,共4页
通过热力学计算软件FactSage计算分析了CaO-SiO2-Al2O3-MnO四元系夹杂物低熔点区域的控制范围.从控制夹杂物成分的角度,指出随着Al2O3含量和CaO含量的增加,夹杂物低熔点区域大小都是先增大后减小;随着SiO2含量和MnO含量的增加,夹杂物低... 通过热力学计算软件FactSage计算分析了CaO-SiO2-Al2O3-MnO四元系夹杂物低熔点区域的控制范围.从控制夹杂物成分的角度,指出随着Al2O3含量和CaO含量的增加,夹杂物低熔点区域大小都是先增大后减小;随着SiO2含量和MnO含量的增加,夹杂物低熔点区域增大.为了得到低熔点夹杂物,应控制SiO2-Al2O3-CaO-MnO系中Al2O3质量分数为20%左右,CaO质量分数在25%~30%之间;同时控制CaO/SiO2比值为0.8~1,SiO2质量分数应为30%左右. 展开更多
关键词 炼钢 CaO—SiO2-Al2O3-mno 热力学计算 夹杂物 成分控制
在线阅读 下载PDF
β-PbO_2电极的改性制备及其性能 被引量:23
9
作者 蔡天晓 鞠鹤 武宏让 《表面技术》 EI CAS CSCD 北大核心 2002年第5期22-23,共2页
通过对传统电沉积 β PbO2 工艺技术的改进 (在镀液中加入纳米级TiO2 ) ,使镀层 β PbO2 ,的脆性大大降低 ,从而使其在温度为 90℃的H2 SO4 介质中使用 ,镀层不会与基材剥落 ,而是自然损耗。
关键词 β-pbo2电极 改性 制备 性能 电催化
在线阅读 下载PDF
Influence of nano-CeO_2 on coating structure and properties of electrodeposited Al/α-PbO_2/β-PbO_2 被引量:4
10
作者 陈阵 余强 +2 位作者 廖登辉 郭忠诚 武剑 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2013年第5期1382-1389,共8页
Al/α-PbO2/β-PbO2 composite electrodes doped with rare earth oxide (CeO2) were prepared by anodic oxidation method investigate the influence of nano-CeO2 dopants on the properties of Al/α-PbO2/β-PbO2-CeO2 electro... Al/α-PbO2/β-PbO2 composite electrodes doped with rare earth oxide (CeO2) were prepared by anodic oxidation method investigate the influence of nano-CeO2 dopants on the properties of Al/α-PbO2/β-PbO2-CeO2 electrodes and the impact of α-PbO2 as the intermediate layer. The results show that using α-PbO2 as the intermediate layer will benefit the crystallization of β-PbO2 and β-PbO2 is more suitable as the surface layer than α-PbO2. CeO2 dopants change the crystallite size and crystal structure, enhance the catalytic activity, and even change the deposition mechanism of PbO2. The doping of CeO2 in the PbO2 electrodes can enhance the electro-catalytic activity, which is helpful for oxygen evolution, and therefore reduce the cell voltage. 展开更多
关键词 rare earth CEO2 composite electrode material α-pbo2 β-pbo2 cell voltage inert anode
在线阅读 下载PDF
Ti/α-PbO_2/β-PbO_2电极电催化氧化处理苯酚废水 被引量:12
11
作者 王鸿辉 杨卫华 +1 位作者 黄龙 黄婷婷 《华侨大学学报(自然科学版)》 CAS 北大核心 2008年第2期263-266,共4页
采用电催化氧化法,以自制Ti/α-PbO2/β-PbO2电极为阳极,在室温条件下对苯酚模拟废水进行降解研究,探讨电流密度、电极间距、pH值及苯酚初始质量浓度对苯酚降解效率的影响规律.结果表明,在电流密度为600 A.m-2,电极间距为1.0 cm,pH值为3... 采用电催化氧化法,以自制Ti/α-PbO2/β-PbO2电极为阳极,在室温条件下对苯酚模拟废水进行降解研究,探讨电流密度、电极间距、pH值及苯酚初始质量浓度对苯酚降解效率的影响规律.结果表明,在电流密度为600 A.m-2,电极间距为1.0 cm,pH值为3,苯酚初始质量浓度为100 mg.L-1的条件下,苯酚降解效率达92%以上.紫外光谱等实验结果表明,苯酚在氧化降解过程中会产生苯醌等中间产物,苯酚及其中间产物最终被矿化为CO2和H2O. 展开更多
关键词 电催化氧化 Ti/α-pbo2/β-pbo2电极 苯酚 降解
在线阅读 下载PDF
β-PbO_2纳米棒及Pb_3O_4纳米晶的制备与表征 被引量:22
12
作者 庄京 邓兆祥 +1 位作者 梁家和 李亚栋 《高等学校化学学报》 SCIE EI CAS CSCD 北大核心 2002年第7期1223-1226,共4页
利用 Na Cl O在碱性溶液中与 Pb(Ac) 2 进行氧化反应直接合成出直径为 1 0~ 2 0 nm、长度为 40 0 nm、长径比达 2 0以上的纯相 β-Pb O2 纳米棒 .对所得 β-Pb O2 在 42 0℃下进行热解 ,得到晶粒尺寸为 2 0 nm左右的 Pb3O4 .对液相氧... 利用 Na Cl O在碱性溶液中与 Pb(Ac) 2 进行氧化反应直接合成出直径为 1 0~ 2 0 nm、长度为 40 0 nm、长径比达 2 0以上的纯相 β-Pb O2 纳米棒 .对所得 β-Pb O2 在 42 0℃下进行热解 ,得到晶粒尺寸为 2 0 nm左右的 Pb3O4 .对液相氧化反应的温度、时间、氧化剂浓度、p H等因素的影响进行了详细研究 ,获得了最佳合成反应条件 .所得产物利用粉末 X射线衍射和透射电子显微镜分析进行了表征 . 展开更多
关键词 制备 表征 纳米棒 纳米晶 β-pbo2 Pb3O4 β-二氧化铅 四氧化三铅
在线阅读 下载PDF
δ-MnO_2对TiO_2光催化降解甲基橙的抑制作用 被引量:6
13
作者 李顺军 马子川 +1 位作者 丁克强 刘敬泽 《高等学校化学学报》 SCIE EI CAS CSCD 北大核心 2007年第12期2338-2342,共5页
采用动力学方法研究了在水悬浮液中δ-MnO2颗粒物对P-25 TiO2光催化降解甲基橙活性的影响,并利用紫外-可见漫反射光谱(DRS)和光致发光光谱(PL)对受δ-MnO2污染前后的TiO2样品进行了表征.动力学研究结果表明,在3种不同初始pH值条件下,δ-... 采用动力学方法研究了在水悬浮液中δ-MnO2颗粒物对P-25 TiO2光催化降解甲基橙活性的影响,并利用紫外-可见漫反射光谱(DRS)和光致发光光谱(PL)对受δ-MnO2污染前后的TiO2样品进行了表征.动力学研究结果表明,在3种不同初始pH值条件下,δ-MnO2对TiO2光催化剂都具有明显的致毒效应,共存δ-MnO2的浓度越大,致毒效应越明显.表征结果表明,由于δ-MnO2与TiO2之间的界面接触,使得TiO2吸收带边蓝移,紫外光区的吸收强度降低,光致发光信号(PL)明显减弱.因此,δ-MnO2导致TiO2的禁带宽度增大,光利用率降低,并且是光生电子与空穴的复合中心. 展开更多
关键词 TIO2 Δ-mno2 失活 光催化 甲基橙
在线阅读 下载PDF
α-MnO_2负载纳米Au催化剂低温催化氧化CO和苯的性能 被引量:11
14
作者 叶青 霍飞飞 +3 位作者 闫立娜 王娟 程水源 康天放 《物理化学学报》 SCIE CAS CSCD 北大核心 2011年第12期2872-2880,共9页
以尿素为沉淀剂用沉积-沉淀法制备了α-MnO2负载Au催化剂xAu/α-MnO2(x=0-7(对应的Au负载量(质量分数)分别为0-7%)),使用X射线粉末衍射(XRD)、N2-吸附/脱附、透射电镜(TEM)、X射线光电子能谱(XPS)和H2-程序升温还原(H2-TPR)等技术对所... 以尿素为沉淀剂用沉积-沉淀法制备了α-MnO2负载Au催化剂xAu/α-MnO2(x=0-7(对应的Au负载量(质量分数)分别为0-7%)),使用X射线粉末衍射(XRD)、N2-吸附/脱附、透射电镜(TEM)、X射线光电子能谱(XPS)和H2-程序升温还原(H2-TPR)等技术对所制样品进行了表征,并测定其对CO和苯的催化氧化性能.XRD结果表明,负载Au对α-MnO2载体结构影响不大,随Au含量的增加,Au颗粒明显增大.N2-吸附/脱附和TEM结果表明,Au的加入对xAu/α-MnO2的比表面积、孔容和孔径等结构性能影响较小,表明Au分布在α-MnO2载体表面,未阻塞其孔道.XPS结果表明,随着Au负载量的增加,xAu/α-MnO2中的O2-/(O22-或O-)、Mn4+/Mn3+和Au3+/Au0的摩尔比在增加,表明其晶格氧、Mn4+和Au3+的浓度在增加.由于贵金属的溢氢作用,Au明显促进xAu/α-MnO2氧化还原能力,其中3Au/α-MnO2具有最高的氧化还原性.负载Au明显影响xAu/α-MnO2样品的催化活性,xAu/α-MnO2的催化性能与Au的分散性、氧化还原性能及表面氧物种的种类密切相关,其中3Au/α-MnO2显示出最佳活性,其催化氧化CO的T90=80°C,苯的T90=200°C. 展开更多
关键词 α-mno2负载Au催化剂 低温还原性 相互作用 CO氧化 苯催化燃烧
在线阅读 下载PDF
δ-MnO_2的制备与性能 被引量:9
15
作者 张启卫 钟建生 +2 位作者 黄行康 黄河宁 杨勇 《应用化学》 CAS CSCD 北大核心 2005年第8期908-911,共4页
用过二硫酸铵((NH4)2S2O8)氧化Mn(Ⅱ)盐制备δ-MnO2. 比较了反应过程中Mn2+与OH-的摩尔比、反应温度、(NH4)2S2O8用量等因素对MnO2晶型的影响. 用X射线衍射(XRD)、红外光谱(IR)分析了制得的δ-MnO2的结构. 测试了样品的热性能和循环伏... 用过二硫酸铵((NH4)2S2O8)氧化Mn(Ⅱ)盐制备δ-MnO2. 比较了反应过程中Mn2+与OH-的摩尔比、反应温度、(NH4)2S2O8用量等因素对MnO2晶型的影响. 用X射线衍射(XRD)、红外光谱(IR)分析了制得的δ-MnO2的结构. 测试了样品的热性能和循环伏安、恒电流充放电性能. 结果表明所制备的δ-MnO2具有良好的层状结构,热稳定性能较好,放电容量较高(约160 mA·h/g,2.0~4.5 V). 展开更多
关键词 Δ-mno2 制备 性能
在线阅读 下载PDF
纳米Ag_2O_2-PbO_2化学修饰电极对大肠杆菌细胞膜壁和DNA损伤的研究 被引量:6
16
作者 顾静 张文 +3 位作者 唐辉 金利通 左翼 吴自荣 《高等学校化学学报》 SCIE EI CAS CSCD 北大核心 2005年第12期2214-2217,共4页
制备了一种新型纳米Ag2O2-PbO2修饰电极,在选定的正电位下,电极表面产生羟基自由基(.OH).通过测定产生的脂质过氧化物和漏出蛋白质的量来研究羟基自由基对大肠杆菌细胞膜壁损伤的情况,并运用电泳和DNA测序的方法对大肠杆菌质粒DNA的损... 制备了一种新型纳米Ag2O2-PbO2修饰电极,在选定的正电位下,电极表面产生羟基自由基(.OH).通过测定产生的脂质过氧化物和漏出蛋白质的量来研究羟基自由基对大肠杆菌细胞膜壁损伤的情况,并运用电泳和DNA测序的方法对大肠杆菌质粒DNA的损伤及其对序列变化进行了研究. 展开更多
关键词 纳米Ag2O2-pbo2修饰电极 大肠杆菌 DNA损伤
在线阅读 下载PDF
Ti/SnO_2+Sb_2O_3/β-PbO_2阳极电化学氧化异噻唑啉酮 被引量:8
17
作者 韩卫清 周刚 +2 位作者 王连军 孙秀云 李健生 《过程工程学报》 EI CAS CSCD 北大核心 2006年第4期566-570,共5页
采用提拉法和电沉积法制作Ti/SnO2+Sb2O3/β-PbO2阳极,通过SEM扫描、XRD分析和极化曲线测定表征具有良好结构和催化性能.利用该电极氧化异噻唑啉酮水溶液,研究运行参数(电化学氧化时间、电流密度和水溶液pH值)的变化对异噻唑啉酮和化学... 采用提拉法和电沉积法制作Ti/SnO2+Sb2O3/β-PbO2阳极,通过SEM扫描、XRD分析和极化曲线测定表征具有良好结构和催化性能.利用该电极氧化异噻唑啉酮水溶液,研究运行参数(电化学氧化时间、电流密度和水溶液pH值)的变化对异噻唑啉酮和化学耗氧量(ChemicalOxygenDemand,CODcr)降解效果的影响,降解过程符合一级动力学方程.在异噻唑啉酮水溶液初始浓度200mg/L、电流密度15mA/cm2、电化学氧化180min时,异噻唑啉酮、CODcr去除率可分别达到98%和43%.通过紫外光谱图分析了异噻唑啉酮氧化过程为先开环,再生成低分子有机酸,最后矿化为CO2和H2O. 展开更多
关键词 异噻唑啉酮 电化学氧化 钛基β-氧化铅阳极(Ti/SnO2+Sb2O3/β-pbo2) 化学耗氧量
在线阅读 下载PDF
超级电容器用Ti/TiO_2-MnO纳米管阵列电极的制备及电化学性能 被引量:7
18
作者 黄有国 郑锋华 +2 位作者 任孟德 李庆余 王红强 《无机材料学报》 SCIE EI CAS CSCD 北大核心 2013年第11期1228-1232,共5页
通过阳极氧化-浸渍-退火的方式获得Ti/TiO2-MnO复合电极。通过XRD测定样品的晶相结构, 通过SEM观察样品的显微形貌。结果表明, Ti/TiO2纳米管阵列孔径分布在60~95 nm, 纳米管长度在350~820 nm。常温下阳极氧化获得的TiO2为无定形结构, ... 通过阳极氧化-浸渍-退火的方式获得Ti/TiO2-MnO复合电极。通过XRD测定样品的晶相结构, 通过SEM观察样品的显微形貌。结果表明, Ti/TiO2纳米管阵列孔径分布在60~95 nm, 纳米管长度在350~820 nm。常温下阳极氧化获得的TiO2为无定形结构, 500℃热处理后, TiO2变为锐钛矿(Anatase)。样品在MnSO4溶液中浸渍并500℃热处理后, 只有MnO相产生。组装扣式模拟超级电容器并测试其循环伏安曲线。CV曲线存在一对氧化还原峰, 对应H+在纳米管中的嵌入/脱出过程。H+在纳米管中传输过程为扩散控制。TiO2由无定形转变为Anatase晶形和在其中沉积MnO后, CV响应电流降低。 展开更多
关键词 阳极氧化 TI TiO2-mno纳米管阵列 超级电容器 电化学性能
在线阅读 下载PDF
钒在FeO-SiO_2-MnO渣系与铁液间的分配行为 被引量:5
19
作者 董进明 赵飞 +2 位作者 张延玲 仇圣桃 干勇 《钢铁》 CAS CSCD 北大核心 2011年第7期14-20,共7页
在实验室条件下,系统研究了1380℃下,钒在FeO—SiO2一MnO渣系与铁液间的分配行为。结果表明:钒的提取率、钒在渣一金两相的分配比、渣的钒容量随渣中SiO2的质量分数升高而降低。在SiO2的质量分数较低时,以上参数随MnO质量分数的增... 在实验室条件下,系统研究了1380℃下,钒在FeO—SiO2一MnO渣系与铁液间的分配行为。结果表明:钒的提取率、钒在渣一金两相的分配比、渣的钒容量随渣中SiO2的质量分数升高而降低。在SiO2的质量分数较低时,以上参数随MnO质量分数的增加而升高。而在SiO2的质量分数较高(〉20%)时,随MnO质量分数的增加呈现先升高后降低的趋势。FeO-SiO2一MnO三元渣系中,siO2的质量分数为10%~20%、MnO的质量分数为13%~5%时,以上参数达到最大值,且该区域对应着FeO-SiO2一MnO渣系熔点最低的区域。V2O3在FeO-SiO2一MnO渣系中活度系数的数量级为10^-6~10^-7。 展开更多
关键词 FeO-SiO2-mno 渣系 分配行为
原文传递
银含量和β-PbO_2镀层对Al/Pb-Ag合金性能的影响(英文) 被引量:6
20
作者 周向阳 王帅 +5 位作者 马驰原 龙波 王辉 杨娟 郭忠诚 陈步明 《稀有金属材料与工程》 SCIE EI CAS CSCD 北大核心 2018年第7期1999-2004,共6页
采用循环伏安曲线(CV)、阳极极化曲线、电化学阻抗曲线(EIS)和腐蚀速率测试研究了不同银含量和镀层的Al/Pb-Ag阳极的阳极行为和反应动力学;用X射线衍射仪和扫描电镜观察了阳极氧化膜层的组分和表面形貌。结果表明,电镀β-PbO_2和高含量... 采用循环伏安曲线(CV)、阳极极化曲线、电化学阻抗曲线(EIS)和腐蚀速率测试研究了不同银含量和镀层的Al/Pb-Ag阳极的阳极行为和反应动力学;用X射线衍射仪和扫描电镜观察了阳极氧化膜层的组分和表面形貌。结果表明,电镀β-PbO_2和高含量的银都能提高阳极的析氧活性、电催化活性以及耐腐蚀性。Al/Pb-0.75%Ag镀β-PbO_2具有最低的析氧过电位,其次是Al/Pb-0.3%Ag镀β-PbO_2,再其次是Al/Pb-0.75%Ag,最后是Al/Pb-0.3%Ag。然而,与镀β-PbO_2相比,高含量的银更能有助于提高阳极的耐腐蚀性。此外,4种阳极层的物相是α-PbO_2、β-PbO_2、Pb和PbO。 展开更多
关键词 Al/Pb-Ag合金 β-pbo2 析氧活性 电积锌
原文传递
上一页 1 2 14 下一页 到第
使用帮助 返回顶部