淬冷法制备LiNi0.5Co0.5O2正极材料及其性能表征
1
作者 林和成 王琼 《电源技术》 CAS 北大核心 2019年第7期1110-1112,共3页
采用1 000℃煅烧并在液氮中淬冷的方法制备LiNi(0.5)Co(0.5)O2正极材料,在2.50~4.50 V范围内,以0.1 C (28m A/g)放电,其初始比容量可达到255.0 m Ah/g,为理论值的93%,并且具有高放电容量循环性能;在大倍率条件下,仍有175.6 m Ah/g (5 C)... 采用1 000℃煅烧并在液氮中淬冷的方法制备LiNi(0.5)Co(0.5)O2正极材料,在2.50~4.50 V范围内,以0.1 C (28m A/g)放电,其初始比容量可达到255.0 m Ah/g,为理论值的93%,并且具有高放电容量循环性能;在大倍率条件下,仍有175.6 m Ah/g (5 C)和145.4 m Ah/g (10 C)的初始放电比容量。采用循环伏安(CV)、交流阻抗谱(EIS)、X射线衍射(XRD)等测试技术进行测试,结果表明高温淬冷处理方法有利于提高LiNi(0.5)Co(0.5)O2正极材料的晶胞体积与晶体的层间距,降低材料接触与迁移电阻,改善其电化学性能。 展开更多
关键词 淬冷法 lini0.5co0.5o2 正极材料
在线阅读 下载PDF
In3+掺杂提升钠离子电池铁锰基层状氧化物正极稳定性
2
作者 李鹏志 盛子墨 +1 位作者 范哲 袁涛 《有色金属材料与工程》 2025年第1期48-56,共9页
O3型NaFe0.5Mn0.5O2由于成本低廉,是一种极具商业潜力的钠离子电池层状正极材料,但其循环稳定性不佳是商业化面临的主要挑战之一。在Na+脱嵌过程中,Mn^(3+)的强烈Jahn-Teller效应引起的不可逆相变和过渡金属(transition metal,TM)离子... O3型NaFe0.5Mn0.5O2由于成本低廉,是一种极具商业潜力的钠离子电池层状正极材料,但其循环稳定性不佳是商业化面临的主要挑战之一。在Na+脱嵌过程中,Mn^(3+)的强烈Jahn-Teller效应引起的不可逆相变和过渡金属(transition metal,TM)离子迁移是容量衰减的主要原因。采用电化学惰性离子In^(3+)取代Mn^(3+)的研究发现:In^(3+)掺杂通过调节TM离子的价态来抑制Jahn-Teller效应,从而增强结构稳定性;有效增强了TM―TM以及TM―O的键能,缩小了TM离子层间距,降低了TM离子迁移的可能性;减小了正极材料颗粒的粒径,缩短了Na+的传输距离,提高了离子的扩散能力。改性后的NaFe_(0.5)Mn_(0.5-x)In_(x)O_(2)样品在电压为2.0~4.0 V时表现出了更好的倍率性能和循环稳定性,可提供111.4 mA·h/g的可逆比容量。经过200圈循环后,其容量保持率从25.78%提升至93.62%。 展开更多
关键词 钠离子电池 层状正极 O3型NaFe_(0.5)Mn_(0.5)O_(2) JAHN-TELLER效应 In^(3+)掺杂
在线阅读 下载PDF
Ce^(4+)掺杂量对LiNi_(0.5)Mn_(1.5)O_(4)电化学性能的影响
3
作者 董怡辰 王振波 刘建 《蓄电池》 2025年第4期151-158,168,共9页
采用共沉淀法将Ce^(4+)掺杂到正极材料LiNi_(0.5)Mn_(1.5)O_(4)中改进材料缺陷以平稳提升其电化学性能。Ce^(4+)掺杂进入正极材料表面层的八面体空间点位,不改变LiNi_(0.5)Mn_(1.5)O_(4)材料的结构形态。Ce^(4+)掺杂使晶胞的晶格参数增... 采用共沉淀法将Ce^(4+)掺杂到正极材料LiNi_(0.5)Mn_(1.5)O_(4)中改进材料缺陷以平稳提升其电化学性能。Ce^(4+)掺杂进入正极材料表面层的八面体空间点位,不改变LiNi_(0.5)Mn_(1.5)O_(4)材料的结构形态。Ce^(4+)掺杂使晶胞的晶格参数增大,从而扩充Li^(+)扩散通道,便于Li^(+)在充放电过程中的扩散。通过电化学测试分析掺杂改性后的LiNi_(0.5)Mn_(1.5-x)Ce_(x)O_(4)材料的电化学性能,将测试结果与空白相LiNi_(0.5)Mn_(1.5)O_(4)正极材料的电化学性能进行比较。LiNi_(0.5)Mn_(1.495)Ce_(0.005)O_(4)具有更好的电化学性能,在1C放电倍率下首次放电比容量为126.43 mA·h·g^(-1),1C循环200次后的放电比容量为121.20 mA·h·g^(-1),容量保持率高达95.86%,在20C大倍率放电下放电比容量为104.10 mA·h·g^(-1)。 展开更多
关键词 LiNi_(0.5)Mn_(1.5)O_(4) 共沉淀法 锂离子电池 Ce^(4+) 掺杂 Ce_(2)(SO_(4))_(3)·4H_(2)O 晶胞 传荷阻抗 放电比容量
在线阅读 下载PDF
Bi掺杂O3型NaNi_(0.5)Mn_(0.5)O_(2)钠离子电池层状正极材料的制备与储钠性能 被引量:7
4
作者 仇健 盛子墨 +1 位作者 马乾乾 袁涛 《有色金属材料与工程》 CAS 2024年第1期16-25,共10页
O3型NaNi_(0.5)Mn_(0.5)O_(2)拥有高理论比容量且易于制备,是商业钠离子(Na+)电池的首选正极材料之一,但其循环稳定性仍面临挑战。利用Bi对NaNi_(0.5)Mn_(0.5)O_(2)进行改性。研究发现,Bi的引入可以在晶粒生长过程中通过调节表面能实现... O3型NaNi_(0.5)Mn_(0.5)O_(2)拥有高理论比容量且易于制备,是商业钠离子(Na+)电池的首选正极材料之一,但其循环稳定性仍面临挑战。利用Bi对NaNi_(0.5)Mn_(0.5)O_(2)进行改性。研究发现,Bi的引入可以在晶粒生长过程中通过调节表面能实现晶粒细化,并且Bi的掺杂增加了层状正极材料的晶胞参数,为Na+提供了宽的扩散通道,提高了Na+的扩散能力,优化了Na^(+)在脱嵌过程中的可逆性。改性后的NaNi_(0.495)Mn_(0.5)Bi_(0.005)O_(2)实现了在2.0~4.0 V的电势区间内0.2 C倍率下的可逆容量为138.1 mAh/g,在5 C倍率下循环100圈后容量保持率可以达到97%。 展开更多
关键词 钠离子电池 层状氧化物正极 O3-NaNi_(0.5)Mn_(0.5)O_(2) Bi掺杂
在线阅读 下载PDF
Co(CO_(3))_(0.5)(OH)·0.11H_(2)O/WO_(3)纳米材料制备及H_(2)S气敏性能
5
作者 桂阳海 吴锦涛 +2 位作者 田宽 郭会师 张心华 《复合材料学报》 EI CAS CSCD 北大核心 2024年第2期816-826,共11页
近年来,H_(2)S作为哮喘和慢阻肺的新型生物标志物对人体健康监测具有重要意义,因此人们对低功耗、高选择性、低检出限和高稳定性H_(2)S传感器的研究显得十分迫切。通过两步原位生长的方式合成了Co(CO_(3))_(0.5)(OH)·0.11H_(2)O/WO... 近年来,H_(2)S作为哮喘和慢阻肺的新型生物标志物对人体健康监测具有重要意义,因此人们对低功耗、高选择性、低检出限和高稳定性H_(2)S传感器的研究显得十分迫切。通过两步原位生长的方式合成了Co(CO_(3))_(0.5)(OH)·0.11H_(2)O/WO_(3)纳米材料。以原位水热法合成的WO_(3)纳米片为基底,通过调控水浴反应时间,在WO_(3)纳米片上原位生长了不同的Co(CO_(3))_(0.5)(OH)·0.11H_(2)O/WO_(3)纳米材料。利用FE-SEM、FTIR、XRD和TG等方法对复合材料进行表征和气敏性能测试。结果表明:反应20 min所制得的Co(CO_(3))_(0.5)(OH)·0.11H_(2)O/WO_(3)复合材料具有最优异的气敏性能,在最佳工作温度(90℃)下对浓度为50×10^(−6)H_(2)S气体的响应值高达109,响应和恢复时间分别为130 s和182 s,对H_(2)S气体表现出优异的选择性。该复合材料在低浓度H_(2)S(3×10^(−6))氛围中,仍具有良好的响应恢复曲线。在一个月内进行的3次重复测试中,表现出较好的重复性和长期稳定性。Co(CO_(3))_(0.5)(OH)·0.11H_(2)O/WO_(3)气敏材料的原位制备及气敏性能研究为气敏传感器器件的制备提供了新思路,为气敏材料的多样性提供了新途径。在环境检测和智能医疗方面有着潜在的应用价值。 展开更多
关键词 纳米材料 WO_(3) Co(CO_(3))_(0.5)(OH)·0.11H_(2)O H_(2)S 复合材料 原位 气敏
原文传递
LiNi_(0.5)Co_(0.5)O_2的制备及其电化学性能 被引量:4
6
作者 彭文杰 李新海 +2 位作者 王云燕 王志兴 郭华军 《中南大学学报(自然科学版)》 EI CAS CSCD 北大核心 2004年第3期390-395,共6页
分别以碳酸盐和氢氧化物为原料,合成了LiNi0.5Co0.5O2。研究结果表明:用氢氧化物为原料,在氧气气氛中,适当提高合成温度和延长反应时间均有利于LiNi0.5Co0.5O2晶格结构的完整;在740℃和氧气气氛下,以氢氧化物为原料反应15h可以合成结构... 分别以碳酸盐和氢氧化物为原料,合成了LiNi0.5Co0.5O2。研究结果表明:用氢氧化物为原料,在氧气气氛中,适当提高合成温度和延长反应时间均有利于LiNi0.5Co0.5O2晶格结构的完整;在740℃和氧气气氛下,以氢氧化物为原料反应15h可以合成结构理想的LiNi0.5Co0.5O2;LiNi0.5Co0.5O2的初始放电容量与LiCoO2的初始放电容量相当,达到141.3mA·h/g,以LiNi0.5Co0.5O2为正极的电极系统具有稳定的电压输出和良好的循环性能,经200次循环后放电容量保持率为82%,可作为LiCoO2的廉价替代物。 展开更多
关键词 锂离子电池 正极材料 lini0.5co0.5o2 电化学性能
在线阅读 下载PDF
柠檬酸溶胶-凝胶燃烧法制备LiNi_(0.5)Co_(0.5)O_2 被引量:5
7
作者 张爱波 刘建睿 +1 位作者 李岚 黄卫东 《精细化工》 EI CAS CSCD 北大核心 2006年第5期421-423,442,共4页
用柠檬酸溶胶-凝胶燃烧法制备了锂离子电池正极材料L iN i0.5Co0.5O2,并对材料进行了热分析、红外分析及X射线衍射分析。研究结果表明,L iN i0.5Co0.5O2干凝胶在空气中自蔓延燃烧,燃烧产物再于800℃烧结10 h,可避免因缺氧而导致杂相L i2... 用柠檬酸溶胶-凝胶燃烧法制备了锂离子电池正极材料L iN i0.5Co0.5O2,并对材料进行了热分析、红外分析及X射线衍射分析。研究结果表明,L iN i0.5Co0.5O2干凝胶在空气中自蔓延燃烧,燃烧产物再于800℃烧结10 h,可避免因缺氧而导致杂相L i2CO3、L i2N i8O10的产生,产物晶型完整。 展开更多
关键词 柠檬酸 溶胶-凝胶法 自蔓延燃烧 lini0.5co0.5o2
在线阅读 下载PDF
合成条件对LiNi_(0.5)Co_(0.5)O_2结构和性能的影响 被引量:4
8
作者 杨书廷 岳红云 +2 位作者 尹艳红 杨伟光 杨金鑫 《电池》 CAS CSCD 北大核心 2006年第4期252-254,共3页
以聚丙烯酰胺(PAM)为模板剂,用微波加热法合成了锂离子电池层状正极材料LiNi0.5Co0.5O2。通过SEM、激光粒度分析和XRD等技术,研究了PAM和微波处理对材料的形貌、粒度和晶相结构的影响。结果表明:PAM可以有效地控制材料的形貌及... 以聚丙烯酰胺(PAM)为模板剂,用微波加热法合成了锂离子电池层状正极材料LiNi0.5Co0.5O2。通过SEM、激光粒度分析和XRD等技术,研究了PAM和微波处理对材料的形貌、粒度和晶相结构的影响。结果表明:PAM可以有效地控制材料的形貌及粒度。充放电测试表明:在3.0-4.3V电压范围内,充放电倍率为0.2C,PAM用量为原材料总质量的2%时,材料的放电比容量达154mAh/g;除首次循环外,前10次循环的充放电效率平均在98.5%以上。 展开更多
关键词 锂离子电池 正极材料 lini0.5co0.5o2 晶相结构
在线阅读 下载PDF
锂离子电池正极材料LiNi_(0.5)Co_(0.5)O_2的制备及性能 被引量:6
9
作者 蔡振平 刘人敏 +1 位作者 吴国良 金维华 《电池》 CAS CSCD 北大核心 2002年第z1期58-60,共3页
LiNixCo1-xO2(0≤x≤1)系是一种很有希望的新型的锂离子电池电极材料。以Li2CO3,NiO,Co3O4为原料,经过造粒的预处理,固相反应合成了锂离子电池正极材料LiNi0.5Co0.5O2。研究了不同的合成条件对产物结构、性能的影响。结果表明,反应温... LiNixCo1-xO2(0≤x≤1)系是一种很有希望的新型的锂离子电池电极材料。以Li2CO3,NiO,Co3O4为原料,经过造粒的预处理,固相反应合成了锂离子电池正极材料LiNi0.5Co0.5O2。研究了不同的合成条件对产物结构、性能的影响。结果表明,反应温度、时间、Li/(Ni+Co)摩尔比等因素对产物的结构、电性能有一定的为响。XRD分析表明合成的产物LiNi0.5Co0.5O2结晶良好,具有规整的α-NaFeO2层状结构的。充放电测试表明在优化条件下合成的LiNi0.5Co0.5O2首次充电容量为170.1mAh/g,放电容量为157.4mAh/g,20次循环后保持初始容量的92%,循环稳定性良好。以MCMB为阳极材料,合成产物为阴极材料,组装成18650型锂离子电池,性能与LiCoO2相当。 展开更多
关键词 锂离子电池 正极材料 lini0.5co0.5o2
在线阅读 下载PDF
微波-固相复合加热技术合成LiNi_(0·5)Co_(0·5)O_2及其性能研究 被引量:3
10
作者 杨书廷 岳红云 +3 位作者 尹艳红 杨金鑫 杨伟光 王辉 《高等学校化学学报》 SCIE EI CAS CSCD 北大核心 2006年第11期2017-2021,共5页
用高分子分散及微波-固相复合加热技术合成了层状锂离子电池正极材料L iN i0.5Co0.5O2.采用循环伏安、充放电循环、扫描电子显微镜(SEM)以及X射线粉末衍射(XRD)等测试技术,研究了煅烧条件对材料微观形貌、相结构以及电化学性能的影响规... 用高分子分散及微波-固相复合加热技术合成了层状锂离子电池正极材料L iN i0.5Co0.5O2.采用循环伏安、充放电循环、扫描电子显微镜(SEM)以及X射线粉末衍射(XRD)等测试技术,研究了煅烧条件对材料微观形貌、相结构以及电化学性能的影响规律.研究结果表明:在750℃煅烧4 h即可得到形状为类球形的纯相层状L iN i0.5Co0.5O2正极材料,该材料的最大放电容量达到154 mA.h/g,循环10周后放电容量仍保持在148 mA.h/g以上. 展开更多
关键词 锂离子电池 层状正极材料 微波-固相烧结法 lini0.5co0.5o2
在线阅读 下载PDF
钴掺杂镍酸锂的密度泛函计算及电化学性能 被引量:3
11
作者 顾大明 谢颖 +1 位作者 史鹏飞 付宏刚 《无机化学学报》 SCIE CAS CSCD 北大核心 2006年第4期696-700,共5页
LiNiO2 and LiNi0.5Co0.5O2 cathodes for lithium-ion batteries were synthesized with co-precipitation method and their electrochemical property was characterized by Galvanostatic cycling. Meanwhile, plane-wave pseudopot... LiNiO2 and LiNi0.5Co0.5O2 cathodes for lithium-ion batteries were synthesized with co-precipitation method and their electrochemical property was characterized by Galvanostatic cycling. Meanwhile, plane-wave pseudopotential method base on density functional theory was used to calculate average cell voltage and the electronic structure of LiNiO2 and LiNi0.5Co0.5O2. The experimental and computational results showed that the average voltage of the cell decreased as Li-ion intercalated to the host cathode (discharge); The potential of LixNi0.5Co0.5O2 was higher than that of LixNiO2 (when 0.25≤x≤0.5). The calculations also indicated that the distortion of the NiO6 octahedron in LixNiO2 was decreased by Co-doped. During the Li-ion intercalates to the host cathode, the micro-structures of NiO6 and CoO6 in the LixNi0.5Co0.5O2 were mutually stabilized, the Jahn-Teller effect was weakened and the electrochemical properties of the materials were enhanced. 展开更多
关键词 lini0.5co0.5o2 正极材料 密度泛函理论 电子结构
在线阅读 下载PDF
蒸发干燥法制备LiNi_(0.5)Mn_(1.5)O_(4)正极材料
12
作者 董怡辰 王振波 《蓄电池》 CAS 2024年第4期151-155,共5页
以LiNO_(3)、Ni(NO_(3))_(2)·6H_(2)O和Mn(CH_(3)COO)_(2)·4H_(2)O为原料,采用蒸发干燥法制备锂电池用LiNi_(0.5)Mn_(1.5)O_(4)正极材料。将原料在玛瑙研钵中研磨后置于100℃水浴盆中。待固体物料溶解后,在混合物中加入的无... 以LiNO_(3)、Ni(NO_(3))_(2)·6H_(2)O和Mn(CH_(3)COO)_(2)·4H_(2)O为原料,采用蒸发干燥法制备锂电池用LiNi_(0.5)Mn_(1.5)O_(4)正极材料。将原料在玛瑙研钵中研磨后置于100℃水浴盆中。待固体物料溶解后,在混合物中加入的无水乙醇和浓度为15.0 mol·L^(-1)的氨水,伴随机械搅拌。将混合物置于120℃的真空干燥室中,干燥2 h(始终在真空氛围中)以获得前驱体。把前驱体放在400℃空气中煅烧4 h,分解硝酸盐和醋酸盐,接着在不同温度的氧气中煅烧6 h,合成LiNi_(0.5)Mn_(1.5)O_(4)材料。将合成的LiNi_(0.5)Mn_(1.5)O_(4)材料放在600℃氧气氛围中退火氧化2 h,再冷却至室温。通过电化学测试得到,在烧结温度800℃,烧结时间6 h的条件下合成的LiNi_(0.5)Mn_(1.5)O_(4)正极材料具有较高的锂插层容量和良好的循环稳定性。 展开更多
关键词 LiNO_(3) Ni(NO_(3))_(2)·6H_(2)O Mn(CH_(3)COO)_(2)·4H_(2)O LiNi_(0.5)Mn_(1.5)O_(4) 锂电池 正极材料 插层容量 蒸发干燥法
在线阅读 下载PDF
层状化合物LiNi_(0.5)Co_(0.5)O_2材料的模板法合成及性能
13
作者 杨书廷 岳红云 +2 位作者 尹艳红 杨金鑫 杨伟光 《电源技术》 CAS CSCD 北大核心 2006年第11期904-907,共4页
以聚丙烯酰胺(PAM)为模板剂用微波-固相复合加热技术合成了层状锂离子蓄电池正极材料LiNi0.5Co0.5O2,并与直接高温固相法合成的该材料进行比较。通过扫描电子显微镜(SEM)、激光粒度分析和X-射线粉末衍射(XRD)分析等技术对材料的微观形... 以聚丙烯酰胺(PAM)为模板剂用微波-固相复合加热技术合成了层状锂离子蓄电池正极材料LiNi0.5Co0.5O2,并与直接高温固相法合成的该材料进行比较。通过扫描电子显微镜(SEM)、激光粒度分析和X-射线粉末衍射(XRD)分析等技术对材料的微观形貌、粒度分布和相结构进行了表征。恒电流充放电循环测试表明:在3.0~4.3V电压范围内充放电倍率为0.2C时,采用微波法合成的材料放电比容量高达154mAh/g,且有良好的循环性能。同时,计时电量和电化学交流阻抗测试表明前者有较小的内阻,且在循环过程中Li+有较强的扩散能力。 展开更多
关键词 锂离子蓄电池 正极材料 lini0.5co0.5o2 交流阻抗
在线阅读 下载PDF
锂离子电池正极材料LiCo0.5Ni0.5O2的颗粒生长研究
14
作者 文衍宣 郑绵平 +1 位作者 童张法 粟海锋 《材料导报》 EI CAS CSCD 北大核心 2005年第F05期269-270,283,共3页
用高温固相反应合成了性能优良的LiCo0.5Ni0.5O2,并研究了合成过程中LiCo0.5Ni0.5O2的颗粒生长过程。LiCo0.5Ni0.5O2的粒径随预热温度、锂用量、焙烧温度和时间的增加而增加,不同合成条件下材料的粒径与生长时间呈对数线性关系。
关键词 锂离子电池 正极材料 lini0.5co0.5o2
在线阅读 下载PDF
LiNi_(0.5)Co_(0.5)O_2体系的结构稳定化作用和独立充放电机理
15
作者 顾大明 张鼎 付宏刚 《无机化学学报》 SCIE CAS CSCD 北大核心 2007年第5期765-770,共6页
为了解释锂离子二次电池正极材料LiNi_(0.5)Co_(0.5)O_2具有的优良充放电循环性能和高比容量特征,采用基于密度泛函理论(DFT)的第一性原理计算方法对LiNi_(0.5)Co_(0.5)O_2和LiNiO_2的相关特性进行了研究。结果表明LiNi_(0.5)Co_(0.5)O_... 为了解释锂离子二次电池正极材料LiNi_(0.5)Co_(0.5)O_2具有的优良充放电循环性能和高比容量特征,采用基于密度泛函理论(DFT)的第一性原理计算方法对LiNi_(0.5)Co_(0.5)O_2和LiNiO_2的相关特性进行了研究。结果表明LiNi_(0.5)Co_(0.5)O_2的结构稳定性优于LiNiO2的原因在于充放电过程中体系中Ni、Co离子交替存在的价电子构型t_(2g)~6e_g^0。依据LiNi_(0.5)Co_(0.5)O_2体系中Ni离子和Co离子相互独立的电极反应提出了适用于LiNixCo_1-xO_2(0≤x≤1)体系的独立充放电机理(0.2C、3.0 ̄4.2VvsLi+/Li),并得到实验的证实。 展开更多
关键词 正极材料 lini0.5co0.5o2 密度泛函理论 独立充放电机理
在线阅读 下载PDF
草酸盐共沉淀法制备锂离子电池正极材料LiNi0.5Mn0.5O2及其电化学性能 被引量:17
16
作者 卢华权 吴锋 +3 位作者 苏岳锋 李宁 陈实 包丽颖 《物理化学学报》 SCIE CAS CSCD 北大核心 2010年第1期51-56,共6页
使用草酸盐共沉淀法合成了LiNi0.5Mn0.5O2,并研究了共沉淀时的pH条件对终产物的结构、形貌及电化学性能的影响.采用X射线衍射(XRD)和扫描电镜(SEM)表征了在pH值为4.0、5.5、7.0和8.5时得到的共沉淀和终产物LiNi0.5Mn0.5O2的结构和形貌.... 使用草酸盐共沉淀法合成了LiNi0.5Mn0.5O2,并研究了共沉淀时的pH条件对终产物的结构、形貌及电化学性能的影响.采用X射线衍射(XRD)和扫描电镜(SEM)表征了在pH值为4.0、5.5、7.0和8.5时得到的共沉淀和终产物LiNi0.5Mn0.5O2的结构和形貌.使用充放电实验研究了不同pH条件下得到的LiNi0.5Mn0.5O2的电化学性能.结果表明,pH为7.0时,合成的材料颗粒更小、分布最均匀,材料具有良好的层状特征,且材料中锂镍的混排程度最小.电化学测试结果印证了pH为7.0时合成的材料具有更好的电化学性能,在0.1C的倍率下,材料的首次放电比容量达到了185 mAh.g-1,在循环20周后,放电比容量仍然保持在160 mAh.g-1.X射线光电子能谱(XPS)测试结果表明,pH为7.0时合成的LiNi0.5Mn0.5O2中Ni为+2价,Mn为+4价. 展开更多
关键词 锂离子电池 正极材料 草酸盐共沉淀 LINI0.5MN0.5O2 电化学性能
在线阅读 下载PDF
锂离子电池正极材料LiNi_(0.5)Mn_(0.5)O_2的循环性能 被引量:14
17
作者 肖劲 曾雷英 +2 位作者 彭忠东 赵浩 胡国荣 《中国有色金属学报》 EI CAS CSCD 北大核心 2006年第8期1439-1444,共6页
采用共沉淀法可以制备出首次放电容量高达210mA·h/g的LiNi0.5Mn0.5O2材料(2.8~4.5V,电流密度30mA/g),但材料循环性能受制备过程中的处理工艺影响很大,处理不严格将导致材料循环性能严重下降。围绕材料的循环性问题,对... 采用共沉淀法可以制备出首次放电容量高达210mA·h/g的LiNi0.5Mn0.5O2材料(2.8~4.5V,电流密度30mA/g),但材料循环性能受制备过程中的处理工艺影响很大,处理不严格将导致材料循环性能严重下降。围绕材料的循环性问题,对其机理进行了分析并在此基础上对制备工艺进行了进一步改善:分别从配锂方式,烧结过程中的升降温速率以及烧结的保温制度进行了系统研究。结果表明:采用改进配锂方式,缓慢升温速率(2℃/min),高低温结合的烧结制度和快速风冷工艺所制备的材料首次放电容量达到188mA·h/g,30个循环后仍保持在174mA·h/g,循环效率有了明显的提高。 展开更多
关键词 LINI0.5MN0.5O2 锂离子电池 正极材料 循环性能
在线阅读 下载PDF
Co/Ce0.5Zr0.5O2催化剂的制备及甲烷部分氧化制合成气 被引量:16
18
作者 余长林 胡久彪 +2 位作者 翁维正 周晓春 陈喜蓉 《燃料化学学报》 EI CAS CSCD 北大核心 2012年第4期418-423,共6页
利用共沉淀法制备了具有介孔结构的Ce0.5Zr0.5O2固溶体载体,然后浸渍不同质量分数(10%、20%、30%)的活性组分钴,制备了系列Co/Ce0.5Zr0.5O2催化剂。利用N2物理吸附(BET)、X射线粉末衍射(XRD)、H2-程序升温还原(H2-TPR)、扫描电子显微镜(... 利用共沉淀法制备了具有介孔结构的Ce0.5Zr0.5O2固溶体载体,然后浸渍不同质量分数(10%、20%、30%)的活性组分钴,制备了系列Co/Ce0.5Zr0.5O2催化剂。利用N2物理吸附(BET)、X射线粉末衍射(XRD)、H2-程序升温还原(H2-TPR)、扫描电子显微镜(SEM)、透射电子显微镜(TEM)、程序升温氧化(TPO)和热重(TG)等手段对制备和反应后的催化剂进行了表征,研究了它们对甲烷部分氧化制合成气反应的催化性能。研究结果表明,铈锆固溶体负载的钴比较容易被还原,该系列催化剂具有较高的活性和对H2及CO的选择性,且随Co含量的增加,催化剂的活性和对H2和CO的选择性得到提高的同时,也增强了催化剂的抗积炭性能。 展开更多
关键词 Ce0.5Zr0.5O2固溶体 甲烷部分氧化 合成气
在线阅读 下载PDF
CuO在Ce_(0.5)Zr_(0.5)O_2上的分散状态及其CO氧化性能的研究 被引量:5
19
作者 蒋晓原 周仁贤 +2 位作者 陈煜 楼莉萍 郑小明 《浙江大学学报(理学版)》 CAS CSCD 2001年第6期653-658,共6页
以硝酸铈和硝酸锆为原料 ,采用共沉淀法制备了不同摩尔比 (0 ,0 .1,0 .2~ 0 .9,1.0 )的Cem Zr1-m O2 样品 .并以 Ce0 .5Zr0 .5O2 为载体 ,采用浸渍法负载不同含量的 Cu O,在色谱流动法上考察其对CO的氧化活性 .并用 XRD,TPR和 BET等技... 以硝酸铈和硝酸锆为原料 ,采用共沉淀法制备了不同摩尔比 (0 ,0 .1,0 .2~ 0 .9,1.0 )的Cem Zr1-m O2 样品 .并以 Ce0 .5Zr0 .5O2 为载体 ,采用浸渍法负载不同含量的 Cu O,在色谱流动法上考察其对CO的氧化活性 .并用 XRD,TPR和 BET等技术对 Cu O/ Ce0 .5Zr0 .5O2 各样品进行了表征 .结果表明 ,当Cu O负载量为 5 .0 %时 ,其 CO的氧化活性最高 .XRD测定表明其氧化活性的高低与铜物种在 Ce0 .5Zr0 .5O2 上的分散状态有关 .TPR结果亦显示活性的高低与 Ce0 .5Zr0 .5O2 上分散较好的铜物种的 α还原峰及分散较差的γ还原峰的峰温及形状有关 . 展开更多
关键词 Ce-mZr1-mO2复合氧化物 CuO/ Ce0.5Zr0.5O2催化剂 分散状态 CO氧化活性
在线阅读 下载PDF
流变相法制备LiNi_(0.5)Mn_(1.5)O_4锂离子电池正极材料及其电化学性质 被引量:14
20
作者 何则强 熊利芝 +3 位作者 吴显明 刘文萍 陈上 黄可龙 《无机化学学报》 SCIE CAS CSCD 北大核心 2007年第5期875-878,共4页
随着人们生活水平的提高.对锂离子电池的性能要求越来越高。为此,需要研究电压更高、电池容量更大的正、负极材料。过渡金属阳离子取代的尖晶石型锂锰氧化物LiMXMn2-xO4(M=Ni,Co,Fe,Cu)由于具有4.5V以上的高电压充放电平台和更... 随着人们生活水平的提高.对锂离子电池的性能要求越来越高。为此,需要研究电压更高、电池容量更大的正、负极材料。过渡金属阳离子取代的尖晶石型锂锰氧化物LiMXMn2-xO4(M=Ni,Co,Fe,Cu)由于具有4.5V以上的高电压充放电平台和更高的能量密度.受到人们的广泛关注。在这些5V级正极材料中,LiNi0.5Mn1.5O4因其高容量、高电压(4.7V)和良好的循环性能而倍受瞩目。 展开更多
关键词 锂离子电池 LiNi0.5Mn15O4 正极材料 流变相法
在线阅读 下载PDF