Effects of CeO_2 doping on the structure and properties of PSN-PZN-PMS-PZT piezoelectric ceramics 被引量:3
1
作者 SUN Qingchi LU Cuimin ZHOU Hua 《Rare Metals》 SCIE EI CAS CSCD 2005年第3期235-239,共5页
Quinary system piezoelectric ceramics PSN-PZN-PMS-PZT were prepared by using a two-step method. The effects of CeO2 doping on piezoelectric and dielectric properties of the system were investigated at morphotropic pha... Quinary system piezoelectric ceramics PSN-PZN-PMS-PZT were prepared by using a two-step method. The effects of CeO2 doping on piezoelectric and dielectric properties of the system were investigated at morphotropic phase boundary (MPB). The results reveal that the relative dielectric constant ε33^T|ε0, the Curie temperature To, the piezoelectric constant d33, the mechanical quality factor Qm, and the electromechanical coupling coefficient Kp are changed with the increase of CeO2 content. On the other hand, the effects of CeO2 doping on the dielectric properties of PSN-PZN-PMS-PZT piezoelectric ceramics at high electric field are consistent with the change at weak electric field. The values of dielectric constant and dielectric loss are enhanced with the increasing of electric field. 展开更多
关键词 piezoelectric ceramics piezoelectric and dielectric properties CeO2 doping morphotropic phase boundary (MPB)
在线阅读 下载PDF
水热合成技术的研究和应用──Ⅵ.钛酸钙电子陶瓷晶体粉末的制备研究 被引量:4
2
作者 胡嗣强 黎少华 《化工冶金》 CSCD 北大核心 1995年第1期42-46,共5页
采用水热法合成CaTiO3电子陶瓷晶体粉末,以Ca(OH)2和Ti(OH)2为水热合成前驱物,制备前驱物的原料选用Ca(NO3)2或CaO及TiCl4,水热体系的KOH浓度为0.1~1.6mol/L,水热温度为150~2000℃,时间20~60min.实验结果表明在各自... 采用水热法合成CaTiO3电子陶瓷晶体粉末,以Ca(OH)2和Ti(OH)2为水热合成前驱物,制备前驱物的原料选用Ca(NO3)2或CaO及TiCl4,水热体系的KOH浓度为0.1~1.6mol/L,水热温度为150~2000℃,时间20~60min.实验结果表明在各自实验范围均能有效合成CaTiO3,推荐合成条件为175℃、30min、水热体系KOH浓度0.2mol/L.文中对合成机理进行了初步讨论. 展开更多
关键词 钛酸钙 水热反应 电子陶瓷
全文增补中