Based on the analysis and processing on relative empirical formula and data, C-values in Larson-Miller (P) expression, P= T(C + Igt), have determined for pearlitic heat resistant steel 12Cr1MoV and 15CrMo(20.62 and 20...Based on the analysis and processing on relative empirical formula and data, C-values in Larson-Miller (P) expression, P= T(C + Igt), have determined for pearlitic heat resistant steel 12Cr1MoV and 15CrMo(20.62 and 20.30). The simulation experiments of high temperature aging, heated from 1.5 to 873 hours, have been designed and performed for its verification. And in combination with published information and the present nearly quantitative works, it has further been verified that both the degradations of microstructures and mechanical properties show a good accuracy and practicability using the Larson-Miller parameter with the present determined C-values. Finally, the effects of carbon content on C-value are analyzed by the empirical electron theory of solids and molecules (EET).展开更多
The observations of dislocations, substructures and other microstructural details were conducted mainly by means of transmission electron microscope (TEM) and scanning electron microscope (SEM) for 12CrlMoV pearlitic ...The observations of dislocations, substructures and other microstructural details were conducted mainly by means of transmission electron microscope (TEM) and scanning electron microscope (SEM) for 12CrlMoV pearlitic heat-resistant steel. It is shown that during the high temperature long-term aging, the disordered and jumbled phase-transformed dislocations caused by normalized cooling are recovered and rearranged into cell substructures, and then the dislocation density is reduced gradually. Finally a low density linear dislocation configuration and a stabler dislocation network are formed and ferritic grains grow considerably.展开更多
文摘Based on the analysis and processing on relative empirical formula and data, C-values in Larson-Miller (P) expression, P= T(C + Igt), have determined for pearlitic heat resistant steel 12Cr1MoV and 15CrMo(20.62 and 20.30). The simulation experiments of high temperature aging, heated from 1.5 to 873 hours, have been designed and performed for its verification. And in combination with published information and the present nearly quantitative works, it has further been verified that both the degradations of microstructures and mechanical properties show a good accuracy and practicability using the Larson-Miller parameter with the present determined C-values. Finally, the effects of carbon content on C-value are analyzed by the empirical electron theory of solids and molecules (EET).
基金supported by the Natural Science Foundation of Gansu Province(No.ZS001-A22-046-C).
文摘The observations of dislocations, substructures and other microstructural details were conducted mainly by means of transmission electron microscope (TEM) and scanning electron microscope (SEM) for 12CrlMoV pearlitic heat-resistant steel. It is shown that during the high temperature long-term aging, the disordered and jumbled phase-transformed dislocations caused by normalized cooling are recovered and rearranged into cell substructures, and then the dislocation density is reduced gradually. Finally a low density linear dislocation configuration and a stabler dislocation network are formed and ferritic grains grow considerably.