The extraction and separation of zinc, manganese, cobalt and nickel from nickel laterite bacteria leach liquor were carried out using sodium salts of TOPS-99 and Cyanex 272 in kerosene. The unwanted metal ions were re...The extraction and separation of zinc, manganese, cobalt and nickel from nickel laterite bacteria leach liquor were carried out using sodium salts of TOPS-99 and Cyanex 272 in kerosene. The unwanted metal ions were removed by precipitation method and solvent extraction was used to extract/separate Zn, Mn, Co and Ni. The nickel laterite leach liquor which was obtained from bioleaching of chromite overburden samples contained 3.72 g/L Fe, 2.08 g/L Al, 0.44 g/L Ni, 0.02 g/L Co, 0.13 g/L Mn, 0.14 g/L Zn and 0.22 g/L Cr. From this leach liquor, 100% Fe, 96.98% Al and 70.42% Cr were removed by precipitation with Ca CO_3 at pH 4.4 followed by precipitation of remaining Al and Cr with 50% ammonia at p H 5.4. After precipitation, the extraction of Zn from the Fe, Al and Cr free leach liquor was carried out with 0.1 mol/L TOPS-99 followed by Mn extraction with 0.04 mol/L Na TOPS-99. The yields of Zn and Mn were 97.77% and 95.63%, respectively. After Mn extraction, cobalt was removed from the leach liquor using 0.0125 mol/L Na Cyanex 272 and finally nickel extraction was carried out using 0.12 mol/L Na TOPS-99 with 99.84% yield. The stripping of loaded organic(LO) phases were achieved with dilute H_2SO_4.展开更多
文摘The extraction and separation of zinc, manganese, cobalt and nickel from nickel laterite bacteria leach liquor were carried out using sodium salts of TOPS-99 and Cyanex 272 in kerosene. The unwanted metal ions were removed by precipitation method and solvent extraction was used to extract/separate Zn, Mn, Co and Ni. The nickel laterite leach liquor which was obtained from bioleaching of chromite overburden samples contained 3.72 g/L Fe, 2.08 g/L Al, 0.44 g/L Ni, 0.02 g/L Co, 0.13 g/L Mn, 0.14 g/L Zn and 0.22 g/L Cr. From this leach liquor, 100% Fe, 96.98% Al and 70.42% Cr were removed by precipitation with Ca CO_3 at pH 4.4 followed by precipitation of remaining Al and Cr with 50% ammonia at p H 5.4. After precipitation, the extraction of Zn from the Fe, Al and Cr free leach liquor was carried out with 0.1 mol/L TOPS-99 followed by Mn extraction with 0.04 mol/L Na TOPS-99. The yields of Zn and Mn were 97.77% and 95.63%, respectively. After Mn extraction, cobalt was removed from the leach liquor using 0.0125 mol/L Na Cyanex 272 and finally nickel extraction was carried out using 0.12 mol/L Na TOPS-99 with 99.84% yield. The stripping of loaded organic(LO) phases were achieved with dilute H_2SO_4.