Microstructural evolution of Al-20Si-5Fe alloy during rapid solidification and hot consolidation 被引量:2
1
作者 M.Rajabi M.Vahidi +1 位作者 a.simchi P.Davami 《Rare Metals》 SCIE EI CAS CSCD 2009年第6期639-645,共7页
Al-20Si-5Fe melt was rapidly solidified into particles and ribbons and then consolidated to near full density by hot pressing at 400℃/250 MPa/1 h. According to the eutectic-growth and dendritic-growth velocity models... Al-20Si-5Fe melt was rapidly solidified into particles and ribbons and then consolidated to near full density by hot pressing at 400℃/250 MPa/1 h. According to the eutectic-growth and dendritic-growth velocity models, the solidification front velocity and the amount of undercooling were estimated for the particles with different sizes. Values of 0.43-1.2 cm/s and 15-28 K were obtained. The secondary dendrite arm spacing revealed a cooling rate of 6 × 10^5 K/s for the particles with an average size of 20 μm. Solidification models for the ribbons yielded a cooling rate of 5 × 10^7 K/s. As a result of the higher cooling rate, the melt-spun ribbons exhibited considerable microstructural refinement and modification. The size of the primary silicon decreased from approximately 1μm to 30 nm while the formation of iron-containing intermetallic compounds was suppressed. Supersaturation of the aluminum matrix in an amount of-7 at.% Si was noticed from the XRD patterns During the hot consolidation process, coarsening of the primary silicon particles and precipitation of β-Al5FeSi phase were observed. Evaluation of the compressive strength and hardness of the alloy indicated an improvement in mechanical properties due to the microstructural modification. 展开更多
关键词 Al-Si-Fe alloy rapid solidification cooling rate microstructure mechanical properties
在线阅读 下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部